CN103509203B - 一种增强的聚丙烯发泡珠粒的制备方法 - Google Patents
一种增强的聚丙烯发泡珠粒的制备方法 Download PDFInfo
- Publication number
- CN103509203B CN103509203B CN201310439081.0A CN201310439081A CN103509203B CN 103509203 B CN103509203 B CN 103509203B CN 201310439081 A CN201310439081 A CN 201310439081A CN 103509203 B CN103509203 B CN 103509203B
- Authority
- CN
- China
- Prior art keywords
- polypropylene
- crystallization
- auxiliary agent
- foaming beads
- enhancing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (6)