CN103360875A - 可复涂耐久型防涂鸦抗粘贴涂料及其制备方法 - Google Patents

可复涂耐久型防涂鸦抗粘贴涂料及其制备方法 Download PDF

Info

Publication number
CN103360875A
CN103360875A CN2013103420664A CN201310342066A CN103360875A CN 103360875 A CN103360875 A CN 103360875A CN 2013103420664 A CN2013103420664 A CN 2013103420664A CN 201310342066 A CN201310342066 A CN 201310342066A CN 103360875 A CN103360875 A CN 103360875A
Authority
CN
China
Prior art keywords
parts
agent
trade mark
capacity
butyl acetate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013103420664A
Other languages
English (en)
Inventor
吕壮志
洪宇
张其亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU HAIYAO CHEMICAL CO., LTD.
Original Assignee
CHANGZHOU SPECIAL PAINT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGZHOU SPECIAL PAINT Co Ltd filed Critical CHANGZHOU SPECIAL PAINT Co Ltd
Priority to CN2013103420664A priority Critical patent/CN103360875A/zh
Publication of CN103360875A publication Critical patent/CN103360875A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种可复涂耐久型防涂鸦抗粘贴涂料及其制备方法。其组成成份及重量份数为氟改性硅树脂60-70份、流平剂0.5-2份、非离子型活性剂0.2-1份、金红石型钛白粉25-30份、消泡剂0.2-1份、表面张力平衡剂1-3份、纳米SiO2 0.5-3份、分散剂0.2-1、固化剂0-13份、醋酸乙酯3-5份、醋酸丁酯7-10份;所述氟改性硅树脂的原料组成及质量份数为氟碳树脂70-75份、聚二甲氧基硅烷13-16份、偶联剂0.5-1份、反应促进剂0.3-0.4份、醋酸丁酯8-10份。本发明的涂料在保持较好抗粘贴效果的同时,耐久性大大提高,而且重涂无障碍,方便返修。

Description

可复涂耐久型防涂鸦抗粘贴涂料及其制备方法
技术领域
本发明涉及一种用于各种表面涂覆的涂料,具体是一种可复涂耐久型防涂鸦抗粘贴涂料及其制备方法。
背景技术
现有的防涂鸦涂料主要有三种类型:A抗粘贴型;B防涂鸦型;C抗粘贴并防涂鸦型。目前市场上主要存在的以A、C型为主,而且多以C型命名。现有此类涂料多以氟碳漆为主,通过添加适量硅类流平以及低表面张力的助剂以提高接触角为目的,最终形成荷叶效应,但其实际效果不并不满意,而且成本较高,不利于市场的推广应用。其主要问题还要归结于本身表面张力降低后的可复涂性以及最终表面纳米层并未与主体树脂形成有效的共价结构,导致涂层耐久性不佳,往往较短时间就失去效果,继而带来返修等一系列问题。
发明内容
本发明所要解决的技术问题是,提供一种具有抗粘贴效果,并且耐久性和复涂性好的可复涂耐久型防涂鸦抗粘贴涂料及其制备方法。
本发明的可复涂耐久型防涂鸦抗粘贴涂料的组成成份及重量份数为氟改性硅树脂60-70份、流平剂0.5-2份、非离子型活性剂0.2-1份、金红石型钛白粉25-30份、消泡剂0.2-1份、表面张力平衡剂1-3份、纳米SiO20.5-3份、分散剂0.2-1、固化剂0-13份、醋酸乙酯3-5份、醋酸丁酯7-10份;所述氟改性硅树脂的原料组成及质量份数为氟碳树脂70-75份、聚二甲氧基硅烷13-16份、偶联剂0.5-1份、反应促进剂0.3-0.4份、醋酸丁酯8-10份。
所述流平剂牌号为DE-2050、非离子型活性剂牌号为3M4432、金红石型钛白粉牌号为R902、消泡剂牌号为BYK067、表面张力平衡剂牌号为H20SDS、分散剂牌号为BYK-110、固化剂牌号为拜耳3792、;所述偶联剂牌号为KH570、反应促进剂牌号为3M4430。
上述可复涂耐久型防涂鸦抗粘贴涂料的其制备方法依次包括以下步骤:
a.预制氟改性硅树脂,取足量氟碳树脂加热升温至42-46℃,滴加足量的聚二甲氧基硅烷,保温45-50分钟后滴加足量偶联剂,升温至50-55℃,保温4-5小时保持搅拌状态,添加足量的反应促进剂,搅拌10-15分钟,降温至42-46℃,保温1.5-2小时,冷却添加足量的醋酸丁酯搅拌均匀,待用;
b.制备涂料,将氟改性硅树脂、金红石型钛白粉、醋酸丁酯、分散剂进行足量物理混合,经研磨分散至18-20微米,在搅拌的状态下添加剩余的流平剂、非离子型活性剂、消泡剂、表面张力平衡剂、纳米SiO2、固化剂、醋酸乙酯,完成后继续搅拌25-30分钟,制得成品。
本发明针对现产品的可复涂性及耐久性方面的不足,调整漆分子结构以及表面官能团的分布情况,结合硅类短键高能的特点,选用能够与之形成非镶嵌型的永久涂层,同时选择性的保留部分活性基团来解决可复涂的问题;实验证明,其在保持较好抗粘贴效果的同时,耐久性大大提高,而且重涂无障碍,方便返修。
附图说明
图1是本发明实施例获得的产品实际使用后涂覆表面接触角随干燥时间的变化曲线图。
具体实施方式
本发明实施例如下:
1、预制氟改性硅树脂,取足量氟碳树脂75份,加热升温至45℃,滴加聚二甲氧基硅烷15份,60分钟内添加完成,保温45分钟,滴加偶联剂(KH570)1份,升温致50度保温4小时保持搅拌状态,添加反应促进剂(3M4430)0.4份。低速搅拌15分钟,降温致45度,保温2小时,冷却添加9份醋酸丁酯搅拌均匀待用。
2、制备涂料,将氟改性硅树脂65份、金红石型钛白粉(R902)25份、醋酸丁酯(试剂级)7份、分散剂(BYK-110)0.2份进行物理混合,经研磨分散至20微米,在搅拌的状态下添加流平剂(DE-2050)1份、非离子型活性剂(3M4432)0.5份、消泡剂(BYK067)0.2份、表面张力平衡剂(H20SDS)3份、纳米SiO20.5份、固化剂(拜耳3792)10份、醋酸乙酯(试剂级)3份,完成后继续搅拌25-30分钟,制得成品。
将上述实施例获得的产品进行涂覆试验,并检测性能,结果如下:
(1)接触角随干燥时间的变化曲线,如图1所示。
(2)其他性能检测数据见下表:
Figure BDA00003630423300031
Figure BDA00003630423300041

Claims (3)

1.一种可复涂耐久型防涂鸦抗粘贴涂料,其特征是:其组成成份及重量份数为氟改性硅树脂60-70份、流平剂0.5-2份、非离子型活性剂0.2-1份、金红石型钛白粉25-30份、消泡剂0.2-1份、表面张力平衡剂1-3份、纳米SiO2 0.5-3份、分散剂0.2-1、固化剂0-13份、醋酸乙酯3-5份、醋酸丁酯7-10份;所述氟改性硅树脂的原料组成及质量份数为氟碳树脂70-75份、聚二甲氧基硅烷13-16份、偶联剂0.5-1份、反应促进剂0.3-0.4份、醋酸丁酯8-10份。
2.根据权利要求1所述的可复涂耐久型防涂鸦抗粘贴涂料,其特征是:所述流平剂牌号为DE-2050、非离子型活性剂牌号为3M4432、金红石型钛白粉牌号为R902、消泡剂牌号为BYK067、表面张力平衡剂牌号为H20SDS、分散剂牌号为BYK-110、固化剂牌号为拜耳3792、;所述偶联剂牌号为KH570、反应促进剂牌号为3M4430。
3.一种权利要求1或3的可复涂耐久型防涂鸦抗粘贴涂料的制备方法,其特征是:依次包括以下步骤,
a. 预制氟改性硅树脂,取足量氟碳树脂加热升温至42-46℃,滴加足量的聚二甲氧基硅烷,保温45-50分钟后滴加足量偶联剂,升温至50-55℃,保温4-5小时保持搅拌状态,添加足量的反应促进剂,搅拌10-15分钟,降温至42-46℃,保温1.5-2小时,冷却添加足量的醋酸丁酯搅拌均匀,待用;
b.制备涂料,将氟改性硅树脂、金红石型钛白粉、醋酸丁酯、分散剂进行足量物理混合,经研磨分散至18-20微米,在搅拌的状态下添加剩余的流平剂、非离子型活性剂、消泡剂、表面张力平衡剂、纳米SiO2、固化剂、醋酸乙酯,完成后继续搅拌25-30分钟,制得成品。
CN2013103420664A 2013-08-07 2013-08-07 可复涂耐久型防涂鸦抗粘贴涂料及其制备方法 Pending CN103360875A (zh)