- CN103271513A CN103271513A CN2013101288990A CN201310128899A CN103271513A CN 103271513 A CN103271513 A CN 103271513A CN 2013101288990 A CN2013101288990 A CN 2013101288990A CN 201310128899 A CN201310128899 A CN 201310128899A CN 103271513 A CN103271513 A CN 103271513A
- Authority
- CN
- China
- Prior art keywords
- shoe
- footwear
- big end
- joint place
- shoe bottom
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Footwear And Its Accessory, Manufacturing Method And Apparatuses (AREA)
Abstract
本发明公开了一种鞋大底、鞋帮底部和贴合处的喷胶方法,包括以下步骤:第一步、鞋大底、鞋帮底部和贴合处刷处理剂进行处理;第二步、喷热溶胶粉,通过喷粉机将热溶胶粉喷在已经刷有处理剂的鞋大底、鞋帮底部和贴合处上;第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。本发明的喷胶方法具有将热溶胶粉回收利用的特点,并且能控制热熔胶的使用量,大大减少了胶料成本。
Description
技术领域
本发明涉及制鞋领域,特别涉及一种鞋大底、鞋帮底部和贴合处的喷胶方法。
背景技术
目前,制鞋生产的工序中,鞋大底、鞋帮底部和贴合处的喷胶处理是必不可少的,现在有的鞋大底、鞋帮底部和贴合处的喷胶是采用喷胶机将胶水喷洒在鞋大底、鞋帮底部和贴合处上。但喷胶量的多少无法控制,导致胶水大量浪费,并且加长了胶水溶化时间,大大降低了生产效率。
发明内容
本发明的目的是针对现有技术的上述缺陷,提供一种鞋大底、鞋帮底部和贴合处的喷胶方法。
为解决现有技术的上述缺陷,本发明要解决的技术方案是:一种鞋大底、鞋帮底部和贴合处的喷胶方法,包括以下步骤:
第一步、鞋大底、鞋帮底部和贴合处刷处理剂进行处理;
第二步、喷热溶胶粉,通过喷粉机将热溶胶粉喷在已经刷有处理剂的鞋大底、鞋帮底部和贴合处上;
第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;
第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;
第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。
作为本发明鞋大底、鞋帮底部和贴合处的喷胶方法的一种改进,所述处理剂为粘着剂。鞋大底、鞋帮底部和贴合处的处理采用粘着剂处理,当鞋大底、鞋帮底部和贴合处使用喷粉机喷热溶胶粉时,更容易吸附在鞋大底上。
作为本发明鞋大底、鞋帮底部和贴合处的喷胶方法的一种改进,所述烘箱温度在以下范围选择:60℃-100℃。
本发明的优点是:本发明采用喷粉机将粉状的热溶胶喷洒在刷有粘着剂的鞋大底、鞋帮底部和贴合处上,多余的热溶胶粉通过喷粉机的回收装置进行回收利用,热溶胶粉经过烘箱加热后成胶状,便可进行贴合。本发明的喷胶方法具有将热溶胶粉回收利用的特点,并且能控制热熔胶的使用量,大大减少了胶料成本。
具体实施方式
实施例一:一种鞋大底、鞋帮底部和贴合处的喷胶方法,包括以下步骤:
第一步、鞋大底、鞋帮底部和贴合处刷处理剂,将需要喷胶的鞋大底、鞋帮底部和贴合处进行处理;处理剂采用粘着剂;鞋大底、鞋帮底部和贴合处的处理采用粘着剂处理,当鞋大底、鞋帮底部和贴合处使用喷粉机喷热溶胶粉时,更容易吸附;
第二步、喷热溶胶粉,通过喷粉机将热溶胶粉喷在已经刷有粘着剂的鞋大底上;
第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;
第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;烘箱温度控制在60℃;
第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。
实施例二:一种鞋大底、鞋帮底部和贴合处的喷胶方法,包括以下步骤:
第一步、鞋大底、鞋帮底部和贴合处刷处理剂,将需要喷胶的鞋大底、鞋帮底部和贴合处进行处理;处理剂采用粘着剂;鞋大底、鞋帮底部和贴合处的处理采用粘着剂处理,当鞋大底、鞋帮底部和贴合处使用喷粉机喷热溶胶粉时,更容易吸附;
第二步、喷热溶胶粉,通过喷粉机将热溶胶粉喷在已经刷有粘着剂的鞋大底、鞋帮底部和贴合处上;
第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;
第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;烘箱温度控制在80℃;
第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。
实施例三:一种鞋大底、鞋帮底部和贴合处的喷胶方法,包括以下步骤:
第一步、鞋大底、鞋帮底部和贴合处刷处理剂,将需要喷胶的鞋大底、鞋帮底部和贴合处进行处理;处理剂采用粘着剂;当鞋大底、鞋帮底部和贴合处使用喷粉机喷热溶胶粉时,更容易吸附;
第二步、喷热溶胶粉,通过喷粉机将热溶胶粉喷在已经刷有粘着剂的鞋大底、鞋帮底部和贴合处上;
第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;
第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;烘箱温度控制在100℃;
第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。
Claims (3)
1.一种鞋大底、鞋帮底部和贴合处的喷胶方法,其特征在于,包括以下步骤:
第一步、将鞋大底、鞋帮底部和贴合处刷处理剂,将需要喷胶的鞋大底、鞋帮底部和贴合处进行处理;
第二步、喷热溶胶粉:通过喷粉机将热溶胶粉喷在已经刷有处理剂的鞋大底、鞋帮底部和贴合处上;
第三步、多余的热溶胶粉回收,喷粉机对鞋大底、鞋帮底部和贴合处喷粉后,会有余粉残留,并通过喷粉机的回收装置进行回收;
第四步、烘箱加热,对喷好热溶胶粉的鞋大底、鞋帮底部和贴合处进行加热,使热溶胶溶化成胶体;
第五步、将粘有热溶胶的鞋大底与鞋帮粘贴。
2.根据权利要求1所述的鞋大底、鞋帮底部和贴合处的喷胶方法,其特征在于,所述处理剂为粘着剂。
3.根据权利要求1所述的鞋大底、鞋帮底部和贴合处的喷胶方法,其特征在于,所述烘箱温度在以下范围选择:60℃-100℃。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013101288990A CN103271513A (zh) | 2013-04-15 | 2013-04-15 | 一种鞋大底、鞋帮底部和贴合处的喷胶方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2013101288990A CN103271513A (zh) | 2013-04-15 | 2013-04-15 | 一种鞋大底、鞋帮底部和贴合处的喷胶方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN103271513A true CN103271513A (zh) | 2013-09-04 |
Family
ID=49053753
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2013101288990A Pending CN103271513A (zh) | 2013-04-15 | 2013-04-15 | 一种鞋大底、鞋帮底部和贴合处的喷胶方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN103271513A (zh) |
Cited By (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN104041998A (zh) * | 2014-06-26 | 2014-09-17 | 无锡市崇安区科技创业服务中心 | 鞋底热熔挤压连接器 |
CN105077851A (zh) * | 2014-05-13 | 2015-11-25 | 诚泰工业科技股份有限公司 | 鞋底构造粘附工艺方法 |
CN105266279A (zh) * | 2014-07-24 | 2016-01-27 | 南宝树脂化学工厂股份有限公司 | 单面上胶制鞋的方法 |
TWI593554B (zh) * | 2016-08-26 | 2017-08-01 | Application of single-sided plastic powder glue on the shoe method | |
CN107373904A (zh) * | 2017-08-30 | 2017-11-24 | 成都南红鞋业有限公司 | 一种高效制鞋方法 |
CN108720180A (zh) * | 2017-04-25 | 2018-11-02 | 欧利速精密工业股份有限公司 | 改良式制鞋装配方法及应用的修正溶液 |
CN110269322A (zh) * | 2019-06-29 | 2019-09-24 | 际华三五一五皮革皮鞋有限公司 | 一种制鞋用帮脚及其单涂胶方法 |
CN115821682A (zh) * | 2022-11-28 | 2023-03-21 | 江苏三叶人造草坪有限公司 | 一种反光型人造草坪、制备方法及设备 |
Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB1016493A (en) * | 1961-06-30 | 1966-01-12 | Bostik Ltd | Improvements in or relating to methods of bonding soles to shoe bottoms in the manufacture of shoes |
GB1199272A (en) * | 1966-08-12 | 1970-07-22 | British United Shoe Machinery | Improvements in or relating to bonding outsoles to shoe bottoms |
DE2439463A1 (de) * | 1973-08-23 | 1975-03-06 | Usm Corp | Klebstoffverbindung |
CN2599048Y (zh) * | 2002-12-10 | 2004-01-14 | 庄承霖 | 具远红外线陶瓷粉末混合胶的积层结构布 |
CN102725129A (zh) * | 2009-10-15 | 2012-10-10 | 株式会社爱世克私 | 激光粘接用橡胶部件和鞋 |
-
2013
- 2013-04-15 CN CN2013101288990A patent/CN103271513A/zh active Pending
Patent Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB1016493A (en) * | 1961-06-30 | 1966-01-12 | Bostik Ltd | Improvements in or relating to methods of bonding soles to shoe bottoms in the manufacture of shoes |
GB1199272A (en) * | 1966-08-12 | 1970-07-22 | British United Shoe Machinery | Improvements in or relating to bonding outsoles to shoe bottoms |
DE2439463A1 (de) * | 1973-08-23 | 1975-03-06 | Usm Corp | Klebstoffverbindung |
CN2599048Y (zh) * | 2002-12-10 | 2004-01-14 | 庄承霖 | 具远红外线陶瓷粉末混合胶的积层结构布 |
CN102725129A (zh) * | 2009-10-15 | 2012-10-10 | 株式会社爱世克私 | 激光粘接用橡胶部件和鞋 |
Cited By (12)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN105077851A (zh) * | 2014-05-13 | 2015-11-25 | 诚泰工业科技股份有限公司 | 鞋底构造粘附工艺方法 |
CN105077851B (zh) * | 2014-05-13 | 2017-06-13 | 诚泰工业科技股份有限公司 | 鞋底构造粘附工艺方法 |
CN104041998A (zh) * | 2014-06-26 | 2014-09-17 | 无锡市崇安区科技创业服务中心 | 鞋底热熔挤压连接器 |
CN104041998B (zh) * | 2014-06-26 | 2015-08-26 | 无锡市崇安区科技创业服务中心 | 鞋底热熔挤压连接器 |
CN105266279A (zh) * | 2014-07-24 | 2016-01-27 | 南宝树脂化学工厂股份有限公司 | 单面上胶制鞋的方法 |
CN105266279B (zh) * | 2014-07-24 | 2018-02-06 | 南宝树脂化学工厂股份有限公司 | 单面上胶制鞋的方法 |
TWI593554B (zh) * | 2016-08-26 | 2017-08-01 | Application of single-sided plastic powder glue on the shoe method | |
CN108720180A (zh) * | 2017-04-25 | 2018-11-02 | 欧利速精密工业股份有限公司 | 改良式制鞋装配方法及应用的修正溶液 |
CN107373904A (zh) * | 2017-08-30 | 2017-11-24 | 成都南红鞋业有限公司 | 一种高效制鞋方法 |
CN110269322A (zh) * | 2019-06-29 | 2019-09-24 | 际华三五一五皮革皮鞋有限公司 | 一种制鞋用帮脚及其单涂胶方法 |
CN110269322B (zh) * | 2019-06-29 | 2022-04-26 | 际华三五一五皮革皮鞋有限公司 | 一种制鞋用帮脚及其单涂胶方法 |
CN115821682A (zh) * | 2022-11-28 | 2023-03-21 | 江苏三叶人造草坪有限公司 | 一种反光型人造草坪、制备方法及设备 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN103271513A (zh) | 一种鞋大底、鞋帮底部和贴合处的喷胶方法 | |
CN105266279B (zh) | 单面上胶制鞋的方法 | |
CN105077851B (zh) | 鞋底构造粘附工艺方法 | |
CN106490768A (zh) | 气雾喷胶制鞋方法 | |
CN203803743U (zh) | 自动涂胶机的刮胶装置 | |
CN204974290U (zh) | 一种自动喷涂机的改进工装 | |
CN107522411A (zh) | 一种化妆品包装瓶的喷涂方法 | |
CN106360884B (zh) | 一种鞋面及其定型工艺 | |
CN203917000U (zh) | 鞋底喷漆专用贴纸 | |
CN108724888A (zh) | 瓦楞纸板塑化工艺 | |
CN104927683A (zh) | 一种纯铜导线与氯丁橡胶粘接方法 | |
CN107373904A (zh) | 一种高效制鞋方法 | |
CN101200621A (zh) | 粘合技术的接着方法 | |
CN105672029A (zh) | 一种遇水即粘型铺贴纸的生产方法及其铺贴工艺 | |
CN204564468U (zh) | 一种多功能节能胶枪 | |
CN103802254A (zh) | 一种表面颗粒结构的浸胶手套制备方法 | |
CN203264987U (zh) | Eva片材涂覆金葱粉生产流水线 | |
CN103141999A (zh) | 制鞋过程中防止多余粘结胶污染鞋体的方法 | |
CN106540834A (zh) | 一种自动喷涂机的改进工装 | |
CN203207324U (zh) | 一种喷粉机 | |
CN108485453A (zh) | 一种浸塑板、该浸塑板的制造工艺及其制造设备 | |
CN105754498A (zh) | 一种玻璃钢容器的修复粘接工艺 | |
CN208523894U (zh) | 一种可避免胶液由边缘溢出的喷胶鞋底及其鞋制品 | |
CN204232394U (zh) | 一种带绒毛的鞋子大底及其生产设备 | |
CN208875731U (zh) | 一种新型的环保封边条 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20130904 |
|
RJ01 | Rejection of invention patent application after publication |