CN103046709B - 一种内墙面的建筑施工方法 - Google Patents

一种内墙面的建筑施工方法 Download PDF

Info

Publication number
CN103046709B
CN103046709B CN201310012307.9A CN201310012307A CN103046709B CN 103046709 B CN103046709 B CN 103046709B CN 201310012307 A CN201310012307 A CN 201310012307A CN 103046709 B CN103046709 B CN 103046709B
Authority
CN
China
Prior art keywords
wall surface
layer
face
cement
metope
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310012307.9A
Other languages
English (en)
Other versions
CN103046709A (zh
Inventor
张敏
翟素珍
孙小江
李振华
范凌云
李永红
王宏江
弓晓丽
王巧利
刘果萍
张波
郝鑫
燕向远
郑宏飞
张帆
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Second Construction Group Co Ltd
Original Assignee
Shanxi No2 Construction Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanxi No2 Construction Co Ltd filed Critical Shanxi No2 Construction Co Ltd
Priority to CN201310012307.9A priority Critical patent/CN103046709B/zh
Publication of CN103046709A publication Critical patent/CN103046709A/zh
Application granted granted Critical
Publication of CN103046709B publication Critical patent/CN103046709B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种内墙面的建筑施工方法,属于建筑领域,灰砂浆配料为水泥:细砂:水渣=1:3:1;抹灰砂浆的方法包括:基层处理、墙面喷浆、墙面贴灰饼、冲筋、抹底灰层、抹面灰层、在面灰层上挂网格布的工艺环节,其中在面灰层挂网格布的工艺环节是:待面灰层含水量达到30%~40%时,先用素水泥浆将网格布的上端粘贴住,然后中间部位采用点粘法用素水泥固定,最后整个墙面采用素水泥将网格布压入面灰层内压光。本发明用抹灰完成后在墙面挂设网格布来解决抹灰面层空鼓、开裂等质量问题。该施工技术发明操作方便,解决实际问题,面层观感好。

Description

一种内墙面的建筑施工方法
技术领域
本发明属于建筑领域的一种施工技术,具体涉及一种内墙面的建筑施工方法。
背景技术
目前全国大多数住宅楼内墙粗装饰面层采用的是传统的混合砂浆抹灰施工工艺。该工艺虽然已经成熟,但是在施工中由于施工管理、施工操作、材料、工人施工水平等多个方面的原因造成抹灰面层空鼓、开裂等质量问题。施工管理、施工操作、工人施工水平等原因可以在施工过程中加以控制,可是由于地域的局限性,材料是否合格成了制约抹灰面层开裂、空鼓的关键因素。部分地区没有中砂,只有细砂,给施工单位在抹灰施工中带来了巨大的质量隐患。内墙抹灰掺水渣、面层挂网格布施工方法有效的解决了这一难题。
发明内容
为了解决部分地区没有中砂,只有细砂的问题,消除普通内墙抹灰空鼓、开裂的质量问题,更好地改进内墙抹灰质量预控措施和施工技术方法,提高内墙抹灰的质量水平,本发明提出一种内墙面的建筑施工方法。
本发明的技术方案是:包括灰砂浆配料和抹灰砂浆方法,灰砂浆配料的重量份为:水泥:细砂:水渣=1:3:1。
抹灰砂浆的方法包括:基层处理、墙面喷浆、墙面贴灰饼、冲筋、抹底灰层、抹面灰层、在面灰层上挂网格布的工艺环节,其中在面灰层挂网格布的工艺环节是:待面灰层含水量达到30%~40%时,先用素水泥浆将网格布的上端粘贴住,然后中间部位采用点粘法用素水泥固定,最后整个墙面采用素水泥将网格布压入面灰层内压光。
所述的网格布为GRC制品增强网格布 ,其常规规格: 
网眼尺寸: 8mm × 8mm 或10mm × 10mm或12mm × 12mm ;
幅宽: 60cm、 90cm 、1m; 
每平方米重: 125g ;
所述素水泥浆为水重10%的108胶:素水泥=1 :3混合均匀。
所述墙面喷浆是将水泥:细砂:801胶=1:1:1.15混合均匀,用喷浆机喷涂均匀于墙体表面。
墙面贴灰饼、冲筋工艺环节是:首先是贴灰饼,贴灰饼是用灰砂浆抹成5cm见方的形状,其目的是找墙面的平整度和垂直度;其次是冲筋,冲筋包括横筋和立筋,冲筋就是用灰砂浆将各灰饼之间抹成的宽为5cm的连线,冲筋间距不大于2m。
抹底灰层工艺是冲筋完毕2h,用灰砂浆先后抹两层,每层灰砂浆的厚度为7—9mm,第一层用大杠垂直抹一遍,第二层用大杠水平抹一遍,然后用木抹子槎毛。
抹面灰层工艺环节是当底灰层含水量达到30%~40%时,用灰砂浆抹成毛光面的面灰层,面灰层厚度为8mm~10mm。
本发明的配料比例均是质量份比。
本发明所述的细砂的粒径是0.25~0.1mm。
本发明所述的水泥的标号是32.5级
本发明所述的水渣的粒径是1~3mm。
本发明能够摒弃了从外地运入中砂的高额费用,利用本地区便宜水渣、细砂,大大降低了抹灰成本,抹灰面层挂网格布,增加了面层的整体性,使抹灰质量得到进一步提高并且挂网格布施工完毕的面层光滑平整,色泽一致,观感好。该施工方法,消除了空鼓、裂缝的质量通病的发生,减少了竣工后的维修、返工、修补等费用。
具体实施方式
一、施工准备
1、必须经过有关部门进行结构工程的验收,合格后方可进行抹灰工程。
2、施工材料、机具设备、作业条件到位的情况下,才能开始施工。
3、抹灰前检查门窗洞口位置正确,门窗框安装位置、标高正确,与墙体连接牢固。连接处缝隙用相应水泥砂浆或水泥混合砂浆分层做嵌塞密实,若缝隙较大时,在砂浆中细石嵌塞,使其塞缝密实。
所述的细石的粒径是5~10mm。
4、将过梁、圈梁及构造柱表面凸出部分混凝土剔平,对蜂窝、麻面、露筋剔到实处,刷素水泥浆一次;剔除外露的钢筋头,铅丝头,补齐窗台砖;用斜砖砌严内隔墙与顶板、梁底交接处。
所述的素水泥浆为水重10%的108胶:素水泥=1 :3混合均匀。
将高于剪力墙表面的混凝土凸出部分剔平,对蜂窝、麻面部位用水泥砂浆找平;脚手架洞眼用C20细石砼堵严;补齐窗台砼。
所述水泥砂浆是水泥:细砂:水=1∶2~2.5:0.38~ 0.5 。
5、将墙面上的线槽用水湿润并刷素水泥浆一次,墙面上的线槽用水泥:砂浆:水=1∶3:0.5的水泥砂浆抹实抹平后,在线槽上钉好225mm宽镀锌钢丝网(网眼规格为13mm×13mm,钢丝直径为0.8mm);电线管、消火栓箱、配电箱安装完毕,并将背后露明部分钉好钢丝网;接线盒用纸堵严。
所述素水泥浆为砼界面剂:素水泥=1:1.5混合均匀。 
6、砼、砌体基层表面的灰尘、污垢、油渍和养护液、模板、胶带清除干净,并浇水湿润。
7、根据室内高度和抹灰现场的具体情况,提前准备好抹灰高凳或脚手架,架子离开墙面及墙角200~250mm,以利操作。
8、室内大面积施工前,先做样板间,经鉴定合格后才能大面积施工。
9、屋面防水工程完工前进行室内抹灰时,必须采取防护措施。
二、 基层处理
在抹灰前做好水、电、暖开关及配电箱的安装,穿墙管道的埋设;将墙体基层表面凹凸不平处凿平;清除基层表面的砂浆、残浆、污垢、油漆;对剔墙的管槽用水泥:砂浆:水=1:3:0.5的水泥砂浆密封;外漏钢筋头剔除,磨平,点涂防锈漆;窗台砼补齐。
三、 喷浆前墙面浇水
喷浆前2天,用胶皮管自上而下浇水。
四、 墙面喷浆
采用专用界面粘结剂,它具有粘结强度高,对多种基材具有良好的附着力。抹灰前3天,将水泥:细砂:专用界面粘结剂=1:1:1.15,混合均匀用喷浆机喷涂于墙体表面,喷涂要均匀、满涂,并浇水养护,待达到强度100%后抹灰。
所述专用界面粘结剂是指801胶。
五、墙面贴灰饼、冲筋
1、室内墙体抹灰层的平均总厚度不大于20mm。在抹灰前再将墙体浇水湿润。墙面贴灰饼、冲筋:首先是用与抹灰层相同的砂浆贴灰饼,其目的是找墙面的平整度和垂直度;其次是冲筋,冲筋就是相应的灰饼之间的连线,冲筋间距不大于2m,筋宽为5cm,冲筋包括横筋和立筋。
2、操作时先抹上灰饼后抹下灰饼;抹灰饼时要根据室内抹灰的要求,以确定下灰饼的正确位置,用靠尺板找好垂直与平整。灰饼抹成5cm见方形状。
    六、抹底灰层:
1、配合比
底灰层、面灰层的材料质量份配料为水泥:细砂:水渣=1:3:1。
2、抹底灰层:
冲筋完毕2h,先薄薄地抹一层,接着分层装档、找平(每层厚度为7—9mm,共抹两层),即用大杠垂直抹一遍,水平抹一遍,再用木抹子槎毛。
然后全面检查底灰平整、阴阳角方正、管道处抹灰抹齐、墙与顶交接光滑平整后,用靠尺板找好垂直度与平整度。
   七、抹面灰层:
当底灰层含水量达到30%~40%时,开始抹面灰(如底灰过干应浇水湿润)。面灰层厚度为8mm~10mm,面灰宜抹成毛光面。
    八、在面灰层上挂网格布
    待面灰层含水量达到30%~40%时,先用素水泥浆将网格布的上端找好位置粘贴住,然后中间部位采用点粘法固定,最后整个墙面采用素水泥将网格布压入面灰层压光。未发现抹灰施工出现质量通病,且施工完毕后的面层色泽一致,观感好。
所述的网格布为GRC制品增强网格布 ,其常规规格: 
网眼尺寸: 8mm × 8mm或10mm × 10mm或12mm × 12mm ;
幅宽: 60cm、 90cm 、1m; 
每平方克重: 125g ;
每卷长度: 100m或 50m 
   九、养护:抹灰施工完成后,应及时进行抹灰墙面的养护工作,养护时间不小于3天。

Claims (8)

1.一种内墙面的建筑施工方法,其特征在于:灰砂浆配料的重量份为水泥:细砂:水渣=1:3:1;抹灰砂浆的方法包括:基层处理、墙面喷浆、墙面贴灰饼、冲筋、抹底灰层、抹面灰层、在面灰层上挂网格布的工艺环节,其中在面灰层挂网格布的工艺环节是:待面灰层含水量达到30%~40%时,先用素水泥浆将网格布的上端粘贴住,然后中间部位采用点粘法用素水泥固定,最后整个墙面采用素水泥将网格布压入面灰层内压光;所述素水泥浆为水重10%的108胶:素水泥=1 :3混合均匀。
2.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:所述墙面喷浆是将水泥:细砂:801胶=1:1:1.15混合均匀,用喷浆机喷涂均匀于墙体表面。
3.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:墙面贴灰饼、冲筋工艺环节是:首先是贴灰饼,贴灰饼是用灰砂浆抹成5cm见方的形状,其目的是找墙面的平整度和垂直度;其次是冲筋,冲筋包括横筋和立筋,冲筋就是用灰砂浆将各灰饼之间抹成的宽为5cm的连线,冲筋间距不大于2m。
4.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:抹底灰层工艺是冲筋完毕2h,用灰砂浆先后抹两层,每层灰砂浆的厚度为7—9mm,第一层用大杠垂直抹一遍,第二层用大杠水平抹一遍,然后用木抹子槎毛。
5.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:抹面灰层工艺环节是当底灰层含水量达到30%~40%时,用灰砂浆抹成毛光面的面灰层,面灰层厚度为8mm~10mm。
6.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:所述网格布为GRC制品增强网格布,其网眼尺寸是: 8mm × 8mm或10mm × 10mm或12mm × 12mm 。
7.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:所述的细砂的粒径是0.25~0.1mm。
8.根据权利要求1所述的一种内墙面的建筑施工方法,其特征在于:所述的水渣的粒径是1~3mm。
CN201310012307.9A 2013-01-14 2013-01-14 一种内墙面的建筑施工方法 Active CN103046709B (zh)