CN103030590A - 一种高品位阻聚剂及其制造工艺 - Google Patents

一种高品位阻聚剂及其制造工艺 Download PDF

Info

Publication number
CN103030590A
CN103030590A CN 201110304701 CN201110304701A CN103030590A CN 103030590 A CN103030590 A CN 103030590A CN 201110304701 CN201110304701 CN 201110304701 CN 201110304701 A CN201110304701 A CN 201110304701A CN 103030590 A CN103030590 A CN 103030590A
Authority
CN
China
Prior art keywords
stopper
tetramethylpiperidinol
polymerization inhibitor
quality
molecular distillation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201110304701
Other languages
English (en)
Inventor
陈建华
徐鸿彬
夏跃雄
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG CITY ZHENXING FINE CHEMICAL CO Ltd
Original Assignee
NANTONG CITY ZHENXING FINE CHEMICAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG CITY ZHENXING FINE CHEMICAL CO Ltd filed Critical NANTONG CITY ZHENXING FINE CHEMICAL CO Ltd
Priority to CN 201110304701 priority Critical patent/CN103030590A/zh
Publication of CN103030590A publication Critical patent/CN103030590A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种高品位4-甲氧基-2,2,6,6-四甲基哌啶醇(简称阻聚剂705)及其制造工艺:首先制得四甲基哌啶醇,然后经过混合、氧化、过滤、分子蒸馏、包装等过程制得;所述制得阻聚剂705的工艺为:用四甲基哌啶醇与乙醛经氧化而得。本发明通过将分子蒸馏提纯得到阻聚剂705,来为客户和本公司提供优质产品。

Description

一种高品位阻聚剂及其制造工艺
技术领域
本发明涉及一种高品位阻聚剂705的制造工艺,通过将精制工艺改为分子蒸馏工艺一种方法。 
背景技术
高品位阻聚剂705对丙烯酸酯类物质具体较好的阻聚效果,作为一种高档的阻聚剂,该产品附加值极高。由于该产品合成时反应剧烈,本发明采用文丘里管混合滴加方法,反应温和;产品热敏性极强,纯度很难达到99%,国内目前对该产品开发还停在小试阶段。针对国内现状,采用精制工艺需成本高,收率低。本发明采用分子蒸馏来提纯获得高品位阻聚剂705。 
发明内容
本发明的目的在于提供一种满足市场需求高品位阻聚剂705,且优化了生产方法达到节能减排目的。 
本发明技术解决方案是:一种高品位阻聚剂705其特征在于:所述四甲基哌啶醇:乙醛:50%双氧水的摩尔比为1.1:1:0.8。高品位阻聚 
剂705的分子结构式如下:
Figure 585014DEST_PATH_IMAGE001
一种制造阻聚剂705的工艺,首先制得四甲基哌啶醇,然后经过混合、氧化、过滤、分子蒸馏、包装等过程制得;其特征在于:所述制得阻聚剂705的工艺为:用四甲基哌啶醇与乙醛经氧化而得。      
所述关键条件氧化合成采用混合滴加方式;后处理采用分子蒸馏
代替结晶。
所述四甲基哌啶醇:乙醛:双氧水的摩尔比为1:1:0.8。 
有益效果:高品位阻聚剂705对丙烯酸酯类物质具体较好的阻聚效果,作为一种高档的阻聚剂,该产品附加值极高。其品质好坏对下游开发的光稳定剂起到非常重要的地位,本工艺通后处理在不提高成本的前提下来为公司和客户提供优质的高品位阻聚剂705。 
最新的技术发展对光稳定剂体系的纯度方面的特性都提出了更高的要求。因此原材料的性能直接关系光稳定剂的应用范围。 
本发明通过将分子蒸馏提纯得到阻聚剂705,来为客户和本公司提供优质产品。 
具体的实施方式: 
下面结合实例对本发明作进一步说明:
实施例1:
制备方法四甲基哌啶醇、乙醛、50%双氧水。
(a )在装有冷凝器、回流管、温度计、搅拌器的500ml的四口瓶中,将加入定量15.7g的2,2,6,6-四甲基-4-哌啶醇、11g乙醛投入合成釜内,在65-68℃下开动搅拌器,开始混合滴加法加入双氧水,同时开始给反应器加热,保温至65-68℃反应10小时,取样检测合格;过滤;再采用分子蒸馏得到合格产品,提高收率,达到降低消耗,提高产品质量目的。 

Claims (4)

1.一种高品位4-甲氧基-2,2,6,6-四甲基哌啶醇(以下简称阻聚剂705),其特征在于:阻聚剂705的分子结构式如下:                                                
2.一种制造权利要求1所述的阻聚剂705的制造工艺,首先制得四甲基哌啶醇,然后经过混合、氧化、过滤、分子蒸馏、包装等过程制得;其特征在于:所述制得阻聚剂705的工艺为:用四甲基哌啶醇与乙醛经氧化而得。
3.根据权利要求2所述的一种制造阻聚剂705的制造工艺,其特征在于:所述关键条件氧化合成采用混合滴加方式;后处理采用分子蒸馏代替结晶。
4.根据权利要求2所述的一种制造阻聚剂705的制造工艺,其特征在于:所述四甲基哌啶醇:乙醛:双氧水的摩尔比为1:1:0.8。
CN 201110304701 2011-10-10 2011-10-10 一种高品位阻聚剂及其制造工艺 Pending CN103030590A (zh)