Prior art keywords
yarns
wool
relative humidity
yarn
spinning
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201110240032
Other languages
English (en)
Inventor
刘自忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 201110240032 priority Critical patent/CN102953179A/zh
Publication of CN102953179A publication Critical patent/CN102953179A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Yarns And Mechanical Finishing Of Yarns Or Ropes (AREA)

Abstract

本发明涉及纺织技术领域,具体涉及一种混纺毛纱生产工艺。其特征在于打破传统的各类纺纱设备的使用界限,创造性的进行重新配置、改造和调整,从而使粗纺类短纤维纺制成离支半精纺纱。采用了牵伸法纺纱,而吸取了毛纺原料混合和梳理及棉纺的并合牵伸,从而使纺制出的纱线色泽均匀,纤维混合均匀,纱线表面光洁,手感蓬松、柔软。本方案的工艺方法对原料的适应性比较广泛,纺纱支数可高可低,技术易普及,设备投资低,占用厂房面积少。

Description

一种混纺毛纱生产工艺
技术领域
本发明涉及纺织技术领域,具体涉及一种混纺毛纱生产工艺。
背景技术
随着人们对服装的审美程度和需求角度也有所变化,人们不仅追求其服用性,更要求将服用性,功能性及装饰性于一体;也不再热衷于风格过于粗犷的面料,开始追求细节之美。传统工艺的粗纺纱已经无法满足当下对于粗纺面料风格的高要求,半精纺技术应运而生。半精纺与以往传统毛精纺、粗纺工艺的最大区别在于,它将棉纺技术与毛纺技术融为一体,形成了一种新型的多组分混合工艺。在设备配置上,将棉纺技术与毛纺技术融为一体,形成了一种新型纺纱工艺。它前道为粗纺的和毛设备加上棉纺的梳棉、并条、粗纱、细纱机等,后道为精纺的络筒、并线,倍捻设备,装备与工艺的改变,解决了原来毛纺设备不能解决的问题。
在毛纺行业因为纺纱设备和工艺的限制,制约了该类产品的开发。一般的粗纺纺纱设备可纺支数大多在20支以下,即使是先进的进口粗纺设备,纱支能够纺到20支以上,但对原料要求却是极高的,即使使用高支的进口澳毛条或高品质的山羊绒,纱支稍高也需要加入大比例的化纤来支撑纺纱强力。该类高支粗纺纱一是成本很高;二是关键不能适应机织产品制造的需要,主要是纱线强力和纱线的抗蠕动摩擦性差,因此大多是用来作针织用纱,很难生产出轻薄的粗纺机织产品。精纺纱支虽然较高,但因纱线中纤维长度和排列等原因却又很难做出粗纺类产品的手感和绒面,因此只有用粗纺类短纤维纺制高支半精纺纱,才能达到效果。而纺制高支半精纺纱,就要充分借鉴棉纺设备和工艺特点,打破传统的各类纺纱设备的使用界限,创造性的进行重新配置、改造和调整,从而使粗纺类短纤维纺制成高支半精纺纱。
发明内容
本发明为了克服现有纺织工艺上的不足之处,提供了一种混纺毛纱生产工艺。该工艺,从原料的选配技术、纺前的预处理技术、工艺及设备改进技术、关键工序相对湿度、空调控制工艺进行改进,解决毛粒(丝粒)均匀度差,纺纱过程静电严重、粘缠严重、产品的掉绒的问题。
为了实现上述目的,本发明的具体技术方案如下:
一、羊毛预处理:按羊毛重量2%的比例,称取油剂,装入喷雾器,羊毛逐层平铺地上,逐层均匀喷油,完成后用塑料薄膜遮盖,堆置24小时,油剂配方如下:抗静电剂:0.3~0.7/%;和毛油:0.2~0.8/%;硅溶胶:0.1~0.15/%。
二、清梳联工序:将梳棉机锡林和道夫改进为变频调速,主要工艺参数:定量干重20g/5m,刺辊速度590r/min,锡林速度260~300r/min,道夫速度15~18r/min,锡林至盖板隔足距为:0.305、0.305、0.254、0.254、0.305mm;
三、并条工序:采取三道并合,将并条机改进为变频调速,主要工艺参数:三道并条均采用6根并合,头并定量干重为:19.7g/5m,后区牵伸倍数为:1.797倍;二并定量干重为:18.2g/5m,三并定量干重为:17.4g/5m;
四、络筒工序:对筒纱进行蒸纱定型,蒸纱温度90℃,时间30分钟;
五、关键工序相对湿度控制:清花工序相对湿度为50~60/%,梳棉工序为63~70/%,相对湿度为50~60/%,并粗工序相对湿度为60~66/%,细纱工序相对湿度为60~70/%。
本发明的有益效果在于:①打破传统的各类纺纱设备的使用界限,创造性的进行重新配置、改造和调整,从而使粗纺类短纤维纺制成离支半精纺纱。②工艺流程较短,成本比毛纺低。③采用了牵伸法纺纱,而吸取了毛纺原料混合和梳理及棉纺的并合牵伸,从而使纺制出的纱线色泽均匀,纤维混合均匀,纱线表面光洁,手感蓬松、柔软。④本方案的工艺方法对原料的适应性比较广泛,纺纱支数可高可低,技术易普及,设备投资低,占用厂房面积少。
具体实施方式
下面结合实施例对本发明作进一步说明:
一、原料的选择:根据产品的需要分别选用绵羊毛、澳毛条、山羊绒等。指标要求:细度:16.5~2011m,含粗:≤0.3%,含杂:≤0.5%,短绒:≤20%,色泽:白色。为了获得主体分布长度趋于一致的纤维,必须应用纤维牵断技术,通过多道回转速度不同的罗拉反复牵伸,将卷曲形态的纤维拉直,在拉直状态下将超长纤维牵断变短,短纤维长度维持不变。
二、纺前的预处理:毛在棉纺设备上生产时,经过摩擦容易产生静电,严重影响纺纱过程,特别是在梳棉,并条工序。所以油剂处理成为纺纱好坏关键的一道工序(包括油剂选择,油剂配方选择,油剂含量分析)。
1、油剂选择:硅溶胶,一种微蓝色乳光的胶体溶液,具有较大的比表面积,较强的吸附性,可附着在纤维表面,而不再溶于水,从而起到增强纤维抱合力的作用。和毛油,主要用于毛纺行业具有显著的渗透、润湿及抗静电性能,可明显改善毛纤维在纺纱过程中的飞毛及断头现象,还可以改善羊绒的韧性,减少纤维在棉纺设备梳理及罗拉牵伸过程中的损伤,减少短绒率。抗静电剂,消除毛纤维在摩擦过程中产生的静电,提高可纺性。
2、油剂配方:抗静电剂:0.6%,和毛油:0.5%,硅溶胶:0.12%。所述抗静电剂选用阴离子型毛用抗静电剂。
所述和毛油使用商品和毛油,是自乳化分散法制成的液态产品。

Claims (3)

1.一种混纺毛纱生产工艺其特征在于该工艺包含以下步骤:
(1)、羊毛预处理:按羊毛重量2%的比例,称取油剂,装入喷雾器,羊毛逐层平铺地上,逐层均匀喷油,完成后用塑料薄膜遮盖,堆置24小时,油剂配方如下:抗静电剂:0.3~0.7/%;和毛油:0.2~0.8/%;硅溶胶:0.1~0.15/%;
(2)、清梳联工序:将梳棉机锡林和道夫改进为变频调速,主要工艺参数:定量干重20g/5m,刺辊速度590r/min,锡林速度260~300r/min,道夫速度15~18r/min,锡林至盖板隔足巨0.305、0.305、0.254、0.254、0.305mm;
(3)、并条工序:采取三道并合,将并条机改进为变频调速,主要工艺参数:三道并条均采用6根并合,头并定量干重19.7g/5m,后区牵伸倍数1.797倍;二并定量干重18.2g/5m,三并定量干重17.4g/5m;
(4)、络筒工序:对筒纱进行蒸纱定型,蒸纱温度90℃,时间30分钟;
(5)五、关键工序相对湿度控制:清花工序相对湿度为50~60/%,梳棉工序63~70相对湿度为50~60/%,并粗工序相对湿度为60~66/%,细纱工序相对湿度为60~70/%。
2.如权利要求1所述的一种混纺毛纱生产工艺,其特征在于所述抗静电剂选用阴离子型毛用抗静电剂。
3.如权利要求1所述的一种混纺毛纱生产工艺,其特征在于所述和毛油使用商品和毛油,是自乳化分散法制成的液态产品。
CN 201110240032 2011-08-16 2011-08-16 一种混纺毛纱生产工艺 Pending CN102953179A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201110240032 CN102953179A (zh) 2011-08-16 2011-08-16 一种混纺毛纱生产工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201110240032 CN102953179A (zh) 2011-08-16 2011-08-16 一种混纺毛纱生产工艺

Publications (1)

Publication Number Publication Date
CN102953179A true CN102953179A (zh) 2013-03-06

Family

ID=47762534

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201110240032 Pending CN102953179A (zh) 2011-08-16 2011-08-16 一种混纺毛纱生产工艺

Country Status (1)

Country Link
CN (1) CN102953179A (zh)

Cited By (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103320926A (zh) * 2013-06-09 2013-09-25 江阴兴吴呢绒科技有限公司 一种羊毛气流混纺工艺
CN103938307A (zh) * 2014-03-27 2014-07-23 浙江中鼎纺织有限公司 一种半精纺梳毛工艺及其设备
CN105332126A (zh) * 2015-11-20 2016-02-17 天津纺织工程研究院有限公司 一种毛半精纺纺纱方法
CN105442126A (zh) * 2015-12-15 2016-03-30 桐乡市濮院羊毛衫职业技术学校 混纺羊绒纱线的生产方法
CN106032591A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种锦纶棉的生产工艺
CN106032592A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种锦纶麻的生产工艺
CN106032590A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于涤纶棉的制备方法
CN106032595A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于锦纶粘胶短纤维的生产工艺
CN106032593A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于锦纶粘胶长丝的生产工艺
CN109440243A (zh) * 2018-12-10 2019-03-08 太原理工大学 羊驼绒/超细羊毛/涤纶高弹丝赛络菲尔复合纱制作方法
CN111945267A (zh) * 2020-08-14 2020-11-17 张家港扬子纺纱有限公司 一种纯天然颜色羊毛纱线的制备工艺

Cited By (13)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103320926A (zh) * 2013-06-09 2013-09-25 江阴兴吴呢绒科技有限公司 一种羊毛气流混纺工艺
CN103320926B (zh) * 2013-06-09 2016-08-10 江阴兴吴呢绒科技有限公司 一种羊毛气流混纺工艺
CN103938307B (zh) * 2014-03-27 2016-04-27 浙江中鼎纺织有限公司 一种半精纺梳毛工艺及其设备
CN103938307A (zh) * 2014-03-27 2014-07-23 浙江中鼎纺织有限公司 一种半精纺梳毛工艺及其设备
CN106032595A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于锦纶粘胶短纤维的生产工艺
CN106032591A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种锦纶棉的生产工艺
CN106032592A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种锦纶麻的生产工艺
CN106032590A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于涤纶棉的制备方法
CN106032593A (zh) * 2015-03-14 2016-10-19 南通神马线业有限公司 一种适用于锦纶粘胶长丝的生产工艺
CN105332126A (zh) * 2015-11-20 2016-02-17 天津纺织工程研究院有限公司 一种毛半精纺纺纱方法
CN105442126A (zh) * 2015-12-15 2016-03-30 桐乡市濮院羊毛衫职业技术学校 混纺羊绒纱线的生产方法
CN109440243A (zh) * 2018-12-10 2019-03-08 太原理工大学 羊驼绒/超细羊毛/涤纶高弹丝赛络菲尔复合纱制作方法
CN111945267A (zh) * 2020-08-14 2020-11-17 张家港扬子纺纱有限公司 一种纯天然颜色羊毛纱线的制备工艺

Similar Documents

Publication Publication Date Title
CN102953179A (zh) 一种混纺毛纱生产工艺
CN101469470A (zh) 毛半精纺纺纱工艺
CN100580163C (zh) 超细柔软毛纱线的生产方法
CN102358972B (zh) 一种丝光毛与锦纶、抗起球腈纶的混纺纱线的制备方法
CN106192110B (zh) 一种t/c/r竹节雪花纱线的生产方法
CN105755622B (zh) 一种粗纱法ab纱生产工艺
CN101979735A (zh) 竹纤维与精梳棉紧密赛络纺纱线工艺
CN101285228A (zh) 多组份天然纤维混纺高支纱及其生产工艺
CN101377031A (zh) 一种精梳棉、绢丝、羊绒混纺纱及其加工方法
CN101671893A (zh) 天丝和亚麻混转杯纺纱的生产方法
CN104005133B (zh) 一种涤纶、再生棉、彩麻混纺针织纱及加工方法
CN102493065A (zh) 一种再生棉雪花混纺纱及其混纺工艺
CN102425019A (zh) 麻、竹纤维、莫代尔涡流纺混纺特种纱
CN110055651A (zh) Sorona纤维、Seawool纤维和再生涤纶的混纺纱线及其纺纱工艺
CN101586278B (zh) 高伸长率羊绒纱线及其生产工艺
CN103820906A (zh) 环锭纺羊绒/绢丝混纺高支纱线及其生产方法
CN104846503B (zh) 一种半精纺地毯纱
CN108914295A (zh) 一种莫代尔纤维、精梳棉、柞蚕丝混纺纱线及其纺纱工艺
CN104862841A (zh) 一种混纺纱线的纺纱方法
CN106906549A (zh) 阳离子涤纶/棉混纺纱的生产方法
CN106757610A (zh) 一种牦牛绒纱线及其制备方法
CN103060982A (zh) 亚麻与天丝的混纺纱线及其制备方法
CN103603112A (zh) 一种半精纺色纺针织纱及其生产工艺
CN1121518C (zh) 用棉纺设备生产阳离子涤粘绲纺纱的工艺
CN106987949A (zh) 远红外纤维/竹纤维/棉混纺纱的生产方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130306