CN102903955A - 锂离子电池用电解液 - Google Patents
锂离子电池用电解液 Download PDFInfo
- Publication number
- CN102903955A CN102903955A CN2012103957720A CN201210395772A CN102903955A CN 102903955 A CN102903955 A CN 102903955A CN 2012103957720 A CN2012103957720 A CN 2012103957720A CN 201210395772 A CN201210395772 A CN 201210395772A CN 102903955 A CN102903955 A CN 102903955A
- Authority
- CN
- China
- Prior art keywords
- electrolyte
- battery
- additive
- lithium ion
- ion battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种锂离子电池用电解液,由锂盐、有机溶剂和添加剂组成,各组分按质量百分比为:锂盐10%~15%、有机溶剂80%~89%、添加剂0.01%~5%混合均匀。其添加剂为提供电子能力强的氧化剂,能够迅速将负极表面沉积的铁元素氧化,阻止电池中铁元素在负极表面还原析出及积累,解决了由于铁枝晶生成而刺破隔膜的问题,有效改善了电池自放电特性,提高电池在使用和贮存过程中的安全性。
Description
技术领域
本发明属于锂离子电池技术领域,具体涉及一种锂离子电池用电解液。
背景技术
锂离子电池由正极、负极、隔膜、电解液和外壳组成。在电池充放电过程中,伴随着锂离子在正负极活性材料中脱出和嵌入,而电解液则作为锂离子在正负极之间传递的媒介。
目前锂离子电池电解液一般采用环状碳酸酯【碳酸乙烯酯(EC)、碳酸丙烯酯(PC)】和链状碳酸酯【(碳酸二乙酯(DEC)、碳酸二甲酯(DMC)、甲基乙基碳酸酯(EMC)】的混合物作为有机溶剂,用六氟磷酸锂作为电解质,添加剂可有可无。而添加剂的种类和用途多种多样,有提高容量、提高循环性能、提高首次充放电效率、提高高低温放电特性的,以及减少电池产气的添加剂等。
锂离子电池从原材料的生产到电池的生产,再到电池的使用,期间各环节不可避免要混入铁元素,而现有锂电池电解液中的添加剂不能消除铁元素,导致电池发生自放电以及产生安全隐患。
发明内容
本发明的目的是克服现有锂电池电解液的不足之处,提供一种能改善锂离子电池自放电特性、提高安全性能的锂离子电池用电解液。
本发明的技术方案是:锂离子电池用电解液,由锂盐、有机溶剂和添加剂组成,其特征在于各组分质量百分比为:锂盐:10%~15%,有机溶剂:80%~89%,添加剂:0.01%~5%,所述添加剂为氧化剂。
所述氧化剂为氯甲酸甲酯、高氯酸铵、过氧化苯甲酰、过苯甲酸特丁酯中的一种或多种混合物。
本发明采用了可以提供电子能力强的氧化剂作为添加剂,能够迅速将负极表面沉积的铁元素氧化。阻止了电池中铁元素在负极表面还原析出及积累,解决了由于铁枝晶生成而刺破隔膜的问题,有效的改善了电池自放电特性,提高电池在使用和贮存过程中的安全性。电解液中各组分配比科学合理,保证了本发明取得积极效果。
具体实施方式
下面通过实施例,对本发明做进一步描述。
实施例1 :
将质量百分数为0.1%的过氧化苯甲酰和13%的六氟磷酸锂溶于86.9%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
实施例2:
将质量百分数为1.5%的过苯甲酸特丁酯和13%的六氟磷酸锂溶于85.5%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
实施例3:
将质量百分数为3%的氯甲酸甲酯和13%的六氟磷酸锂溶于84%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
实施例4 :
将质量百分数为5%的高氯酸铵和12%的六氟磷酸锂溶于83%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
实施例5:
将质量百分数为1%的氯甲酸甲酯、2%的高氯酸铵和13%的六氟磷酸锂溶于84%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
比较例1:
将质量百分数为13%的六氟磷酸锂溶于87%的有机溶剂(碳酸乙烯酯和碳酸二甲酯质量比为1.1:1)中,混合均匀后制成电解液。
将实施例和比较例所述的电解液注入10Ah磷酸铁锂电池后,满电常温搁置28天 测试结果:
Claims (2)
1.一种锂离子电池用电解液,由锂盐、有机溶剂和添加剂组成,其特征在于各组分质量百分比为:锂盐:10%~15%,有机溶剂:80%~89%,添加剂:0.01%~5%,所述添加剂为氧化剂。
2.根据权利要求1所述的锂离子电池用电解液,其特征在于,所述氧化剂是氯甲酸甲酯、高氯酸铵、过氧化苯甲酰、过苯甲酸特丁酯中的一种或多种混合物。