CN102220468B - 同步器滑套和齿座套淬工艺 - Google Patents
同步器滑套和齿座套淬工艺 Download PDFInfo
- Publication number
- CN102220468B CN102220468B CN 201110147685 CN201110147685A CN102220468B CN 102220468 B CN102220468 B CN 102220468B CN 201110147685 CN201110147685 CN 201110147685 CN 201110147685 A CN201110147685 A CN 201110147685A CN 102220468 B CN102220468 B CN 102220468B
- Authority
- CN
- China
- Prior art keywords
- toothholder
- sliding sleeve
- quenching
- synchronizer
- tempering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明公开了一种同步器滑套和齿座套淬工艺,包括以下步骤:a、将齿座与滑套配套组装;b、将装配好的齿座和滑套预热至500℃±10℃,并保温30min;c、将预热好的齿座和滑套装入加热炉加热至880℃±10℃,并保温20min;d、将加热后的齿座和滑套在淬火介质中淬火;e、将淬火后齿座和滑套放入回火炉,在回火温度为180℃±10℃状态下回火90min。本发明同步器滑套和齿座套淬工艺,将装配好的齿座和齿套进行整体淬火,消除了淬火后的齿座和齿套不能组装的问题,提高了产品合格率;同时齿座和齿套同时进行淬火,淬火效率高,工艺流程短,生产成本低。
Description
技术领域
本发明涉及一种同步器的淬火工艺,特别涉及同步器的滑套和齿座的淬火工艺。
背景技术
重型车辆的变速箱同步器一般包括滑套和齿座,滑套外套于齿座并与齿座通过齿轮啮合齿在圆周方向上固定配合。滑套和齿座在制造过程中要求进行淬火,以提升滑套和齿座和综合力学性能。
现有的滑套和齿座采用单独淬火的方式,单独淬火需要为滑套设置一个与滑套配合的保护芯,以防止滑套在淬火过程中内腔和齿发生变形,造成不能和齿座配合;齿座淬火时也需要设置一个与齿座外圆和齿配合的保护套圈,以防止齿座在淬火过程中发生变形,造成不能同滑套配合。这种淬火方式,工序长,且成本较高,对热处理变形的控制效果一般,产品报废率较高。
因此需要对现有技术中的同步器滑套和齿座淬火工艺进行改进,以缩短淬火工艺流程,提高生产效率,降低制造成本,并提高产品合格率。
发明内容
有鉴于此,本发明的目的是提供一种同步器滑套和齿座套淬工艺,其具有淬火工艺短、生产效率高的特点,可降低制造成本,并能提高产品合格率。
本发明同步器滑套和齿座套淬工艺,包括以下步骤:
a、将齿座与滑套配套组装;
b、将装配好的齿座和滑套预热至500℃±10℃,并保温30min;
c、将预热好的齿座和滑套装入加热炉加热至880℃±10℃ ,并保温20min;
d、将加热后的齿座和滑套在淬火介质中淬火;
e、将淬火后齿座和滑套放入回火炉,在回火温度为180℃±10℃状态下回火 90min。
进一步,所述步骤d和步骤e之间还设置有步骤f:清洗淬火后的齿座和滑套;
进一步,所述步骤e中的回火炉为油炉。
本发明的有益效果:本发明同步器滑套和齿座套淬工艺,将装配好的齿座和齿套进行整体淬火,消除了淬火后的齿座和齿套不能组装的问题,提高了产品合格率;同时齿座和齿套同时进行淬火,淬火效率高,工艺流程短,生产成本低。
具体实施方式
实施例一:本实施例中同步器滑套和齿座套淬工艺,包括以下步骤:
a、将齿座与滑套配套组装;
b、将装配好的齿座和滑套预热至490℃,并保温30min;
c、将预热好的齿座和滑套装入加热炉加热至870℃,并保温20min;
d、将加热后的齿座和滑套在淬火介质中淬火;
e、将淬火后齿座和滑套放入回火炉,在回火温度为170℃状态下回火 90min。
作为对本实施方案的改进,所述步骤d和步骤e之间还设置有步骤f:清洗淬火后的齿座和滑套,可提高齿座和滑套的外观质量。
本实施例中,所述步骤e中的回火炉为油炉,当然在具体实施中还可以选择其它形式的回火炉。
实施例二:本实施例中同步器滑套和齿座套淬工艺,包括以下步骤:
a、将齿座与滑套配套组装;
b、将装配好的齿座和滑套预热至500℃,并保温30min;
c、将预热好的齿座和滑套装入加热炉加热至880℃,并保温20min;
d、将加热后的齿座和滑套在淬火介质中淬火;
e、将淬火后齿座和滑套放入回火炉,在回火温度为180℃状态下回火 90min。
作为对本实施方案的改进,所述步骤d和步骤e之间还设置有步骤f:清洗淬火后的齿座和滑套,可提高齿座和滑套的外观质量。
本实施例中,所述步骤e中的回火炉为油炉,当然在具体实施中还可以选择其它形式的回火炉。
实施例三:本实施例中同步器滑套和齿座套淬工艺,包括以下步骤:
a、将齿座与滑套配套组装;
b、将装配好的齿座和滑套预热至510℃,并保温30min;
c、将预热好的齿座和滑套装入加热炉加热至890℃ ,并保温20min;
d、将加热后的齿座和滑套在淬火介质中淬火;
e、将淬火后齿座和滑套放入回火炉,在回火温度为190℃状态下回火 90min。
作为对本实施方案的改进,所述步骤d和步骤e之间还设置有步骤f:清洗淬火后的齿座和滑套,可提高齿座和滑套的外观质量。
本实施例中,所述步骤e中的回火炉为油炉,当然在具体实施中还可以选择其它形式的回火炉。
最后说明的是,以上实施例仅用以说明本发明的技术方案而非限制,尽管参照较佳实施例对本发明进行了详细说明,本领域的普通技术人员应当理解,可以对本发明的技术方案进行修改或者等同替换,而不脱离本发明技术方案的宗旨和范围,其均应涵盖在本发明的权利要求范围当中。
Claims (3)
1.一种同步器滑套和齿座套淬工艺,其特征在于:包括以下步骤:
a、将齿座与滑套配套组装;
b、将装配好的齿座和滑套预热至500℃±10℃,并保温30min;
c、将预热好的齿座和滑套装入加热炉加热至880℃±10℃ ,并保温20min;
d、将加热后的齿座和滑套在淬火介质中淬火;
e、将淬火后齿座和滑套放入回火炉,在回火温度为180℃±10℃状态下回火 90min。
2.根据权利要求1所述的同步器滑套和齿座套淬工艺,其特征在于:所述步骤d和步骤e之间还设置有步骤f:清洗淬火后的齿座和滑套。
3.根据权利要求1所述的同步器滑套和齿座套淬工艺,其特征在于:所述步骤e中的回火炉为油炉。