CN102211876A - 太阳能电池封装用玻璃的制备方法 - Google Patents
太阳能电池封装用玻璃的制备方法 Download PDFInfo
- Publication number
- CN102211876A CN102211876A CN2010101459030A CN201010145903A CN102211876A CN 102211876 A CN102211876 A CN 102211876A CN 2010101459030 A CN2010101459030 A CN 2010101459030A CN 201010145903 A CN201010145903 A CN 201010145903A CN 102211876 A CN102211876 A CN 102211876A
- Authority
- CN
- China
- Prior art keywords
- glass
- deionized water
- solution
- solar battery
- sio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (2)