CN102019801A - 撒点着色仿古效果在楼梯、木地板表面上的施工应用 - Google Patents
撒点着色仿古效果在楼梯、木地板表面上的施工应用 Download PDFInfo
- Publication number
- CN102019801A CN102019801A CN2009101962351A CN200910196235A CN102019801A CN 102019801 A CN102019801 A CN 102019801A CN 2009101962351 A CN2009101962351 A CN 2009101962351A CN 200910196235 A CN200910196235 A CN 200910196235A CN 102019801 A CN102019801 A CN 102019801A
- Authority
- CN
- China
- Prior art keywords
- nitro
- add
- polyurethane
- viscosity
- effect
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种撒点着色仿古效果在楼梯、木地板表面上的施工方法。其特征在于由以下步骤构成:(1)白身砂光;(2)聚氨酯头度;(3)砂磨;(4)聚氨酯白底;(5)砂磨;(6)聚氨酯白底;(7)喷涂撒点漆;(8)硝基清底;(9)硝基格丽斯;(10)硝基清底;(11)砂磨;(12)干刷;(13)硝基清底;(14)格丽斯整理;(15)硝基面漆。本发明的优点是可以在楼梯、木地板表面形成一种特殊着色仿古效果,将体现装饰中对色彩、古典风格的追求。所产生的效果,消费者在使用时能起到防滑的作用,如长期使用还能促进脚底血液循环,对脚底起到保健效果。
Description
技术领域
本发明涉及一种撒点着色仿古效果的施工工艺,具体涉及在楼梯、木地板基材上的着色仿古效果涂装工艺
技术背景
目前现有的楼梯、木地板表面上的油漆施工一般采用喷涂或刷涂,由此基本上呈现平面的油漆面的效果,而过于平整的油漆表面比较光滑,当鞋底有水份或鞋底较平时容易打滑,因此亟待发明一中能够将装饰艺术的多彩性与健康生活理念相结合,满足了人们对古典艺术的追求的油漆施工方法。
发明内容
本发明需要解决的技术问题是公开一种撒点着色仿古效果在楼梯、木地板表面的施工工艺,以满足人们的需求。其特征在于,由以下步骤组成:
(1)白身砂光:用240#砂纸将白身打磨平整、光滑;
(2)聚氨酯头度:用聚氨酯头度按配比加底漆固化剂加聚氨酯稀释剂,将粘度调至8~9秒,均匀喷涂一遍,半个“十”字,待干2~3小时;
(3)砂磨:用320#砂纸将素材打磨平整、光滑,勿砂穿;
(4)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(5)砂磨:用320#砂纸打磨平整、光滑;
(6)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(7)喷涂撒点漆:用撒点漆按配比加固化剂,调至高粘度,喷涂处撒点效果,待干4~6小时;
(8)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(9)硝基格丽斯:用白棉布蘸上硝基格丽斯,均匀擦拭干净,局部略抓明暗,使其达到深浅不一的效果;
(10)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(11)砂磨:用400#棉纱轻砂平滑;
(12)干刷:用毛刷蘸上格丽斯在楼梯、木地板表面边缘局部轻打,使其达到一种因使用时间过长而被弄旧弄坏的自然效果;
(13)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(14)格丽斯整理:用白棉布蘸上格丽斯整体修饰效果,加深立体感,使其表现更为自然生动;
(15)硝基面漆:硝基面漆按配比加硝基稀释剂,将粘度调至12~13秒,均匀喷涂,待干24小时即可;
本发明的优点是可以在楼梯、木地板表面形成一种特殊着色仿古效果,将体现装饰中对色彩、古典风格的追求。所产生的效果,消费者在使用时能起到防滑的作用,如长期使用还能促进脚底血液循环,对脚底起到保健效果。
上述文中所说的素材是指MDF板、各类实木木材或其他胶合板组合成的楼梯、木地板;
上述所说的聚氨酯头度、聚氨酯白底、撒点漆、硝基清底、硝基格丽斯、硝基面漆、干刷格丽斯、固化剂、稀释剂均为上海富臣化工有限公司产品,也可以是市场同类产品;
上述所说的一个“十”字是指施工喷涂时被喷涂物从头一端喷到尾,然后再从另一端喷到尾,所产生的一个交叉为一个“十”字;
上述所说的施工粘度是指用岩田2#杯所测的粘度。
具体实施方式
实施例1
(1)白身砂光:用240#砂纸将白身打磨平整、光滑;
(2)聚氨酯头度:用聚氨酯头度按配比加底漆固化剂加聚氨酯稀释剂,将粘度调至8~9秒,均匀喷涂一遍,半个“十”字,待干2~3小时;
(3)砂磨:用320#砂纸将素材打磨平整、光滑,勿砂穿;
(4)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(5)砂磨:用320#砂纸打磨平整、光滑;
(6)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(7)喷涂撒点漆:用专配的撒点漆按配比加固化剂,调至高粘度,喷涂处撒点效果,待干4~6小时;
(8)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(9)硝基格丽斯:用白棉布蘸上硝基格丽斯,均匀擦拭干净,局部略抓明暗,使其达到深浅不一的效果;
(10)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(11)砂磨:用400#棉纱轻砂平滑;
(12)干刷:用毛刷蘸上格丽斯在楼梯、木地板表面边缘局部轻打,使其达到一种因使用时间过长而被弄旧弄坏的自然效果;
(13)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(14)格丽斯整理:用白棉布蘸上格丽斯整体修饰效果,加深立体感,使其表现更为自然生动;
(15)硝基面漆:硝基面漆按配比加硝基稀释剂,将粘度调至12~13秒,均匀喷涂,待干24小时即可;
本发明的优点是可以在楼梯、木地板表面形成一种特殊着色仿古效果,将体现装饰中对色彩、古典风格的追求。所产生的效果,消费者在使用时能起到防滑的作用,如长期使用还能促进脚底血液循环,对脚底起到保健效果。
Claims (1)
1.撒点着色仿古效果的施工工艺在楼梯、木地板表面上的施工方法,其特征在于由以下步骤组成:
(1)白身砂光:用240#砂纸将白身打磨平整、光滑;
(2)聚氨酯头度:用聚氨酯头度按配比加底漆固化剂加聚氨酯稀释剂,将粘度调至8~9秒,均匀喷涂一遍,半个“十”字,待干2~3小时;
(3)砂磨:用320#砂纸将素材打磨平整、光滑;
(4)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(5)砂磨:用320#砂纸打磨平整、光滑;
(6)聚氨酯白底:用聚氨酯白底加底漆固化剂加聚氨酯稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干4~6小时;
(7)喷涂撒点漆:用撒点漆按配比加固化剂,调至高粘度,喷涂处撒点效果,待干4~6小时;
(8)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(9)硝基格丽斯:用白棉布蘸上硝基格丽斯,均匀擦拭干净,局部略抓明暗,使其达到深浅不一的效果;
(10)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(11)砂磨:用400#棉纱轻砂平滑;
(12)干刷:用毛刷蘸上格丽斯在楼梯、木地板表面边缘局部轻打,使其达到一种因使用时间过长而被弄旧弄坏的自然效果;
(13)硝基清底:用硝基清底按配比加硝基稀释剂,将粘度调至14~16秒,均匀喷涂2个“十”字,待干40~60分钟;
(14)格丽斯整理:用白棉布蘸上格丽斯整体修饰效果,加深立体感,使其表现更为自然生动;
(15)硝基面漆:硝基面漆按配比加硝基稀释剂,将粘度调至12~13秒,均匀喷涂,待干24小时即可。