CN101357467B - 水性木器仿古涂装工艺在松木家具基材上的应用 - Google Patents

水性木器仿古涂装工艺在松木家具基材上的应用 Download PDF

Info

Publication number
CN101357467B
CN101357467B CN 200710044424 CN200710044424A CN101357467B CN 101357467 B CN101357467 B CN 101357467B CN 200710044424 CN200710044424 CN 200710044424 CN 200710044424 A CN200710044424 A CN 200710044424A CN 101357467 B CN101357467 B CN 101357467B
Authority
CN
China
Prior art keywords
make
waterborne
aqueous
evenly
viscosity
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN 200710044424
Other languages
English (en)
Other versions
CN101357467A (zh
Inventor
钟华胜
刘林生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI ZHANCHEN PAINT Co.,Ltd.
Zhuhai zhanchen New Material Co., Ltd
Original Assignee
SHENZHEN ZHANCHENDA CHEMICAL INDUSTRY Co Ltd
Shanghai Fuchen Chemical Co Ltd
Beijing Zhanchen Chemical Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENZHEN ZHANCHENDA CHEMICAL INDUSTRY Co Ltd, Shanghai Fuchen Chemical Co Ltd, Beijing Zhanchen Chemical Co Ltd filed Critical SHENZHEN ZHANCHENDA CHEMICAL INDUSTRY Co Ltd
Priority to CN 200710044424 priority Critical patent/CN101357467B/zh
Publication of CN101357467A publication Critical patent/CN101357467A/zh
Application granted granted Critical
Publication of CN101357467B publication Critical patent/CN101357467B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及水性木器仿古涂装在松木家具基材上的应用。其特征在于包括下列步骤:1、素材处理,2、底色,3、水性木器底漆,4、水性白色灰尘漆,5、水性木器底漆,6、水性金粉灰尘漆,7、水性木器底漆,8、砂光,9、做旧,喷点,10、水性木器面漆,所述的水性木器底漆、水性白色灰尘漆、水性金粉灰尘漆、水性木器面漆均为市售产品,所述的素材为松木。本发明的优点是水性木器仿古涂装在松木家具上表现更自然,更反璞归真,同时更加环保。

Description

水性木器仿古涂装工艺在松木家具基材上的应用
技术领域
本发明涉及水性木器仿古涂装在松木家具基材上的应用。
背景技术
目前松木家具作为出口家具中较畅销的一支主力军,其仿古涂装大多为硝基涂装,但随着人们对生存环境日益关注、环保意识的加强,且“3C”认证的强制执行,水性木器仿古涂装横空出世,既能满足人们对古老时代的怀念和追求,又能更好的保护我们共同的家园——地球。参考文件《水性木器漆的施工》(朱万章、刘学英,《上海涂料》2002年第三期,)中论述的是水性木器涂料通用的施工方法,是专业技术人员都知道的基本方法,不可能达到像本发明的仿古涂装效果,因此,不能满足有关涂装的需要。
发明内容
本发明的目的是解决现有技术中松木家具仿古的涂装采用硝基涂装所存在的对于环境及市内空气产生挥发的问题,提供一种水性木器仿古涂装在松木家具基材上的仿古涂装工艺。本发明设计水性木器仿古涂装在松木家具基材上的仿古涂装工艺,其特征在于包括下列步骤:
1、素材处理
(1)破坏处理:用破坏工具把素材故意性敲打,使其达到一种该物品被使用时间过长而被损坏的自然效果;
(2)砂光:用240#砂纸顺木纹砂磨,去除素材表面毛刺、砂痕;
2、底色:喷涂、喷湿使其深入木材纹理体现效果;
3、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一度,干燥时间2~3小时;
4、水性白色灰尘漆:用配制的白色灰尘漆,均匀擦拭。将表面擦拭干净,并略抓明暗,使其达到深浅不一的自然效果;
5、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一个“十”字,干燥时间6~8小时;
6、水性金粉灰尘漆:用配制的金粉灰尘漆,均匀擦拭。将表面擦拭干净,并略抓明暗,使其加深深浅不一的自然效果。
7、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一个“十”字,干燥时间8~12小时;
8、砂光:轻砂,顺木纹砂磨平整,光滑。
9、做旧,喷点:用配制的颜色刷边做旧,并用喷枪做喷点效果,使其再一次加深仿古的自然效果。
10、水性木器面漆:用水性的消光类面漆按配比调至粘度为12~13秒,均匀喷涂一个“十”字,干燥48小时后包装,所述的水性木器底漆、水性白色灰尘漆、水性金粉灰尘漆、水性木器面漆均为市售产品,以上粘度均为岩田—2#杯粘度,所述的素材为松木。本发明的优点是水性木器仿古涂装在松木家具上表现更自然,更反璞归真,同时更加环保。
下面结合实例对本发明作详细说明。
具体实施方式
1、素材处理
(1)破坏处理:用破坏工具把素材故意性敲打,使其达到一种该物品被使用时间过长而被损坏的自然效果;
(2)砂光:用240#砂纸顺木纹砂磨,去除素材表面毛刺、砂痕;
2、底色:喷涂、喷湿使其深入木材纹理体现效果;
3、水性木器底漆:按配比调至粘度为15秒,均匀喷涂一度,干燥时间3小时;
4、水性白色灰尘漆:用配制的白色灰尘漆,均匀擦拭。将表面擦拭干净,并略抓明暗,使其达到深浅不一的自然效果;
5、水性木器底漆:按配比调至粘度为15秒,均匀喷涂一个“十”字,干燥时间8小时;
6、水性金粉灰尘漆:用配制的金粉灰尘漆,均匀擦拭。将表面擦拭干净,并略抓明暗,使其加深深浅不一的自然效果。
7、水性木器底漆:按配比调至粘度为15秒,均匀喷涂一个“十”字,干燥时间10小时;
8、砂光:轻砂,顺木纹砂磨平整,光滑。
9、做旧,喷点:用配制的颜色刷边做旧,并用喷枪做喷点效果,使其再一次加深仿古的自然效果。
10、水性木器面漆:用水性消光类面漆按配比调至粘度为13秒,均匀喷涂一个“十”字,干燥48小时后包装。

Claims (1)

1.水性木器漆仿古涂装工艺在松木家具基材上应用,其特征在于包括下列步骤:
(1)、素材处理
(A)破坏处理:用破坏工具把素材故意性敲打,使其达到一种该物品被使用时间过长而被损坏的自然效果;
(B)砂光:用240#砂纸顺木纹砂磨,去除素材表面毛刺、砂痕;
(2)、底色:喷涂素材到喷湿,使其底色深入木材纹理体现效果;
(3)、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一度,干燥时间2~3小时;
(4)、水性白色灰尘漆:用配制的白色灰尘漆,均匀擦拭;将表面擦拭干净,并略抓明暗,使其达到深浅不一的自然效果;
(5)、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一个“十”字,干燥时间6~8小时;
(6)、水性金粉灰尘漆:用配制的金粉灰尘漆,均匀擦拭;将表面擦拭干净,并略抓明暗,使其加深深浅不一的自然效果;
(7)、水性木器底漆:按配比调至粘度为14~15秒,均匀喷涂一个“十”字,干燥时间8~12小时;
(8)、砂光:轻砂,顺木纹砂磨平整,光滑;
(9)、做旧,喷点:用配制的颜色刷边做旧,并用喷枪做喷点效果,使其再一次加深仿古的自然效果;
(10)、水性木器面漆:用水性消光类面漆按配比调至粘度为12~13秒,均匀喷涂一个“十”字,干燥48小时后包装。
CN 200710044424 2007-07-31 2007-07-31 水性木器仿古涂装工艺在松木家具基材上的应用 Active CN101357467B (zh)