CN102003133A CN 201010299117 CN201010299117A CN102003133A CN 102003133 A CN102003133 A CN 102003133A CN 201010299117 CN201010299117 CN 201010299117 CN 201010299117 A CN201010299117 A CN 201010299117A CN 102003133 A CN102003133 A CN 102003133A
Authority
CN
China
Prior art keywords
paper
resin
door panels
paint
emulsion paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010299117
Other languages
English (en)
Inventor
毛庆德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHEJIANG KAIYANG DOORS CO Ltd
Original Assignee
ZHEJIANG KAIYANG DOORS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG KAIYANG DOORS CO Ltd filed Critical ZHEJIANG KAIYANG DOORS CO Ltd
Priority to CN 201010299117 priority Critical patent/CN102003133A/zh
Publication of CN102003133A publication Critical patent/CN102003133A/zh
Pending legal-status Critical Current

Links

Images

Abstract

一种压漆模压门面板及其制作方法,压漆模压门面板包括面板层和纸层,纸层为树脂漆浸渍纸,所述的树脂漆浸渍纸是实色印刷纸或木纹纸经树脂漆浸渍、干燥而成。其制作方法为采用实色印刷纸或木纹纸,经树脂漆浸渍、干燥制成树脂漆浸渍纸,压漆前将树脂漆浸渍纸按门板的规格裁成相同的尺寸,再将浸渍纸表放置在已模压成型的模压门面板上,一同装入热压机的模具内进行热压,在热压的作用下使树脂漆固化在模压门面板的表面,形成即环保又牢固的树脂漆层。本发明改变了模压门面板传统喷涂工艺,实现了模压门面板的规模化、工业化生产,环保、节省油漆,节省人工,提高生产效率。

Description

一种压漆模压门面板及其制作方法 
技术领域
本发明属于一种门的面板及其加工方法,尤其是涉及一种模压门面板及其加工方法。 
背景技术
模压门是采用模压门面板制作的带有凹凸造型的或有木纹或无木纹的一种木质室内门。模压木门因价格较实木门更经济实惠,且安全方便,而受到中等收入家庭的青睐。传统的模压门面板表面涂饰,采用溶剂性涂料(水性、油性)喷涂或刷涂工艺,不仅因大量有害性溶剂的蒸发和涂料的流失造成严重的环境污染和涂料损失,而且需要昂贵的人工费用(如油漆工、打磨工),同时还因人工操作而不能形成规模化的工业化生产,是所有家具、木门及装璜行业中规模化、工业化生产的瓶颈。 
发明内容
为解决上述问题,本发明旨在提供一种压漆模压门面板及其制作方法,污染少、成本低、效率高,非常适用于规模化、工业化生产。 
本发明解决的技术问题所采用的技术方案是: 
一种压漆模压门面板,包括面板层和纸层,其特征是所述的纸层为树脂漆浸渍纸,所述的树脂漆浸渍纸是实色印刷纸或木纹纸经树脂漆浸渍、干燥而成。所述的树脂为尿醛改性树脂、三聚氰铵改性树脂或不饱和树脂。所述的实色印刷纸或木纹纸规格为70-95g/m2。 
一种压漆模压门面板的制作方法,其特征是包括如下步骤:是采用实色印刷纸或木纹纸,经树脂漆浸渍、干燥制成树脂漆浸渍纸,压漆前将树脂漆浸渍纸按门板的规格裁成相同的尺寸,再将浸渍纸表放置在已模压成型的模压门面板(或未成型的平板)上,一同装入热压机的模具内进行热压,在热压的作用下使树脂漆固化在模压门面板的表面,形成即环保又牢固的树脂漆层。 
在具体实施中,所述的在热压机的模具内进行热压步骤,其温度为130-160℃之间;压力为2.0-4.0Mpa之间,其热压时间10-30S。 
在具体实施中,所述的树脂漆为尿醛改性树脂、三聚氰铵改性树脂或不饱和树脂。
在具体实施中,所述的实色印刷纸或木纹纸规格为70-95g/m2。 
在批量生产时候,树脂漆浸渍纸可预先制作好,贮存备用。 
在模压门面板的表面形成即环保又牢固的树脂漆层,根据模具表面的光亮度和浮雕纹理,压制成不同光亮的漆膜或浮雕纹理,漆膜无毒、无味、环保,并完全达到或超过人工喷涂漆面的效果。该树脂漆层也可以打磨,用200#以上砂布打磨后,还可以在其表面进行修色或再涂装,进行改色或增加表面漆面效果。 
由于通过模压机热压,使得模压门面板的表面形成即环保又牢固的树脂漆层,通过模压机热压时,会对模压门面板的基板同时进行压缩量,同时会把树脂漆浸渍纸嵌入基板上,立体感加强。 
本发明改变了采用溶剂性涂料(水性、油性)喷涂或刷涂工艺,没有有害性溶剂的蒸发和涂料的流失,大大减小了环境污染,并且加强了操作工的劳动保护,减少了人员开支,降低了成本。采用本发明 的工艺,非常适用于模压门的规模化的工业化生产,提高了效率。 
有益效果:本发明工艺技术彻底改变了一次成型或二次成型的模压门面板传统喷涂工艺,实现了模压门面板或家具部件的规模化、工业化生产,环保、节省油漆达50%以上,节省人工,提高生产效率,彻底解决了人工喷涂的环境污染的问题,为规模化、工业化生产模压复合门或实木复合门提供了技术保证。 
附图说明
下面结合附图和实施例对发明进一步说明。 
图1是本发明实施例1的结构示意图。 
图中:1、面板层2、纸层3、凹凸造型 
具体实施方式
下面结合实施例对本发明做进一步的详细说明,以下实施例是对本发明的解释,而本发明并不局限于以下实施例。 
实施例1: 
如图1一种压漆模压门面板,包括面板层1和纸层2,面板1制作的带有凹凸造型3,纸层2为树脂漆浸渍纸。树脂漆浸渍纸是实色印刷纸或木纹纸经三聚氰铵改性树脂漆浸渍、干燥而成。纸层2为实色印刷纸或木纹纸,其规格为90g/m2。 
实施例2: 
压漆模压门面板生产工艺,是采用实色(各种颜色纸)印刷纸或木纹纸,其规格为80g/m2),经三聚氰铵改性树脂浸渍、干燥制成树脂漆浸渍纸(批量生产可贮存待用),压漆前将树脂漆 浸渍纸按门板的规格裁成相同的尺寸,再将浸渍纸表在已模压成型的模压门面板(或未成型的平板)上,一同装入热压机的模具内,在150℃左右的温度;3.0Mpa单位压力下,热压时间15s,在高温、高压的作用下使树脂漆固化在模压门面板的表面,并形成即环保又牢固的树脂漆层,根据模具表面的光亮度和浮雕纹理,压制成不同光亮的漆膜或浮雕纹理,漆膜无毒、无味、环保,并完全达到或超过人工喷涂漆面的效果。该树脂漆层也可以打磨,用200#以上砂布打磨后,还可以在其表面进行修色或再涂装,进行改色或增加表面漆面效果。 

Claims (7)

1.一种压漆模压门面板,包括面板层和纸层,其特征是所述的纸层为树脂漆浸渍纸,所述的树脂漆浸渍纸是实色印刷纸或木纹纸经树脂漆浸渍、干燥而成。
2.根据权利要求1所述的一种压漆模压门面板,其特征是:所述的树脂为尿醛改性树脂、三聚氰铵改性树脂或不饱和树脂。
3.根据权利要求1所述的一种压漆模压门面板,其特征是:所述的实色印刷纸或木纹纸规格为70-95g/m2。
4.一种压漆模压门面板的制作方法,其特征是包括如下步骤:采用实色印刷纸或木纹纸,经树脂漆浸渍、干燥制成树脂漆浸渍纸,压漆前将树脂漆浸渍纸按门板的规格裁成相同的尺寸,再将浸渍纸表放置在已模压成型的模压门面板(或未成型的平板)上,一同装入热压机的模具内进行热压,在热压的作用下使树脂漆固化在模压门面板的表面,形成即环保又牢固的树脂漆层。
5.根据权利要求4所述的一种压漆模压门面板的制作方法,其特征是:所述的在热压机的模具内进行热压步骤,其温度为130-160℃之间;压力为2.0-4.0Mpa之间,其热压时间10-30S。
6.根据权利要求4所述的一种压漆模压门面板的制作方法,其特征是:所述的树脂漆为尿醛改性树脂、三聚氰铵改性树脂或不饱和树脂。
7.根据权利要求4所述的一种压漆模压门面板的制作方法,其特征是:所述的实色印刷纸或木纹纸规格为70-95g/m2。
CN 201010299117 2010-09-30 2010-09-30 一种压漆模压门面板及其制作方法 Pending CN102003133A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201010299117 CN102003133A (zh) 2010-09-30 2010-09-30 一种压漆模压门面板及其制作方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201010299117 CN102003133A (zh) 2010-09-30 2010-09-30 一种压漆模压门面板及其制作方法

Publications (1)

Publication Number Publication Date
CN102003133A true CN102003133A (zh) 2011-04-06

Family

ID=43810804

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201010299117 Pending CN102003133A (zh) 2010-09-30 2010-09-30 一种压漆模压门面板及其制作方法

Country Status (1)

Country Link
CN (1) CN102003133A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103144179A (zh) * 2013-04-07 2013-06-12 黑龙江华信家具有限公司 低碳环保节能高级生态门及制作方法
CN103865356A (zh) * 2014-04-01 2014-06-18 桦甸市惠邦木业有限责任公司 一种模压树脂漆及其制作方法及其上漆方法

Citations (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2003040509A1 (de) * 2001-11-02 2003-05-15 Eduard Tasch Türblatt mit mindestens einer deckplatte aus stein, vorzugsweise für eine zimmertür und verfahren zu seiner herstellung
US6607627B2 (en) * 2001-03-05 2003-08-19 Premark Rwp Holdings, Inc. Compound injection molded high pressure laminate flooring
CN200945668Y (zh) * 2006-09-28 2007-09-12 卢达权 一种环保防火板材
CN101474808A (zh) * 2009-01-23 2009-07-08 桦甸市惠邦木业有限责任公司 三聚氰氨饰面模压纤维板及生产工艺
CN201448013U (zh) * 2009-07-21 2010-05-05 张春平 一种模压门
CN201474538U (zh) * 2009-08-14 2010-05-19 方永贤 一种有三聚氰胺饰面的模压门板
CN201835700U (zh) * 2010-09-30 2011-05-18 浙江开洋门业有限公司 一种压漆模压门面板

Patent Citations (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6607627B2 (en) * 2001-03-05 2003-08-19 Premark Rwp Holdings, Inc. Compound injection molded high pressure laminate flooring
WO2003040509A1 (de) * 2001-11-02 2003-05-15 Eduard Tasch Türblatt mit mindestens einer deckplatte aus stein, vorzugsweise für eine zimmertür und verfahren zu seiner herstellung
CN200945668Y (zh) * 2006-09-28 2007-09-12 卢达权 一种环保防火板材
CN101474808A (zh) * 2009-01-23 2009-07-08 桦甸市惠邦木业有限责任公司 三聚氰氨饰面模压纤维板及生产工艺
CN201448013U (zh) * 2009-07-21 2010-05-05 张春平 一种模压门
CN201474538U (zh) * 2009-08-14 2010-05-19 方永贤 一种有三聚氰胺饰面的模压门板
CN201835700U (zh) * 2010-09-30 2011-05-18 浙江开洋门业有限公司 一种压漆模压门面板

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103144179A (zh) * 2013-04-07 2013-06-12 黑龙江华信家具有限公司 低碳环保节能高级生态门及制作方法
CN103865356A (zh) * 2014-04-01 2014-06-18 桦甸市惠邦木业有限责任公司 一种模压树脂漆及其制作方法及其上漆方法
CN103865356B (zh) * 2014-04-01 2017-10-03 桦甸市惠邦木业有限责任公司 一种模压树脂漆的上漆方法

Similar Documents

Publication Publication Date Title
CN102152564B (zh) 合成树脂浸渍薄木饰面人造板及生产工艺
CN104149363A (zh) 一种玻璃钢制品的制作工艺
CN203818901U (zh) 合成板材
CN101695891A (zh) 一种水转印膜的制作工艺
CN208293308U (zh) 纸塑制品表面涂布设备及其制作的纸塑制品
CN107972155B (zh) 一种中密度纤维板粉末涂料静电涂装方法
CN202319328U (zh) 一种附立体纹路热转印膜
CN102584029B (zh) 采用数码喷绘制作的钢化玻璃装饰板及其制作方法
CN103481723B (zh) 一种规模化生产浮雕装饰画的方法
CN103317821A (zh) 一种三聚氰胺饰面人造板的制造工艺
CN103496287A (zh) 一种柔性蜜胺美耐片及其制法
CN104163021A (zh) 一种粉末涂料金属贴面装饰板及其制作方法
CN102003133A (zh) 一种压漆模压门面板及其制作方法
CN1205859C (zh) 一种鱼竿的制造方法
CN109177215A (zh) 一种电镀片材注塑成型工艺及其产品
CN201835700U (zh) 一种压漆模压门面板
CN101544005A (zh) 新型的木制品表面处理技术
KR101223099B1 (ko) 시트에 엠보싱을 형성하는 방법
CN102501480B (zh) 一种薄木饰面模压树脂漆门面板及其生产工艺
CN110696443A (zh) 一种染色三聚氰胺胶浸渍表层纸饰面人造板的生产工艺
CN202344960U (zh) 一种薄木饰面模压树脂人造板
CN102700343A (zh) 一种植物纤维模塑墙体装饰板水转印方法
CN203557775U (zh) 一种整体厨卫用装饰板
CN109016918A (zh) 一种金属单板木纹胶水热转印的生产工艺
CN212404635U (zh) 一种玻璃镜面亮金卡纸张结构

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20110406