CN101353726A - 一种真空蒸馏分离铅铂合金的方法 - Google Patents
一种真空蒸馏分离铅铂合金的方法 Download PDFInfo
- Publication number
- CN101353726A CN101353726A CNA2008101432492A CN200810143249A CN101353726A CN 101353726 A CN101353726 A CN 101353726A CN A2008101432492 A CNA2008101432492 A CN A2008101432492A CN 200810143249 A CN200810143249 A CN 200810143249A CN 101353726 A CN101353726 A CN 101353726A
- Authority
- CN
- China
- Prior art keywords
- lead
- platinum
- platinum alloy
- vacuum distillation
- vacuum
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明提供了一种真空蒸馏分离铅铂合金的方法,将铅铂合金置于真空蒸馏炉中,一定温度下铅蒸发并冷凝直接得到金属铅,同时,蒸余物中铂纯度得到提高,当铅蒸发完全时,可得到纯金属铂。该方法具有工艺流程短、简单高效、低能耗,没有废气、废水和废渣产生,无污染实现零排放等优点。
Description
技术领域
本发明涉及一种真空蒸馏分离铅铂合金,并分别得到铅金属和铂金属的方法。
背景技术
铂族金属具有独特的物理性能及化学性质,广泛应用于现代科技及生产的各个领域,但其世界储量有限,资源日益匮乏,价格不断上涨,因此,铂族金属的回收利用受到了极大重视。大部分铂族金属是作为有色冶金的副产品,在提取主金属的过程中附带回收的,另一个主要来源是从废珠宝、工业废料、电子元件等二次资源中回收。
铅是金、银及铂族金属的良好捕集剂,并由此形成了测定矿石中微量贵金属的经典方法“火试金”。用铅做捕集剂是熔炼处理低品位物料,提取其中贵金属的有效方法之一。对于富集贵金属铂的熔体铅,可用灰吹法或者硝酸分铅法提取铂。其中灰吹法是在高温下对贵铅进行吹风氧化,该法能耗大,环境条件恶劣,另外所得的氧化铅需进一步回收和处理。硝酸分铅法中,用硝酸溶解大量存在的铅,可使贵金属得到富集,但是硝酸浸煮时,贵金属也会有部分溶解,而且溶解的铅以离子形态存在,需进一步处理回收,此外,该工艺过程产生大量的废水、废渣、废气,对环境易造成严重污染。因此,如何简单高效、低能耗、清洁地分离分离铅铂合金是一个值得研究的课题。
发明内容
本发明的目的是针对现有铅铂合金分离技术的不足,提供一种真空蒸馏分离铅铂合金的新方法,以流程短、操作简单、清洁的工艺,实现铅铂合金的有效分离,直接得到金属铅和铂。
为了实现这一目的,本发明采用真空蒸馏的方法,在真空条件下,蒸汽压较高的铅蒸发并冷凝得到纯金属;铅蒸馏分离后,剩余的铂金属纯度提高。
本发明以铅铂合金为原料,在真空蒸馏炉中,压力为20~100Pa、1000-1300K的温度下进行铅、铂蒸馏分离,蒸余物为纯度高的铂。
真空蒸馏分离优选时间为2-4小时。
本发明最优选在30Pa,升温至1250K,恒温蒸发3h,进行铅、铂蒸馏分离。
采用的是以铅捕集铂所得的铅铂合金为原料。
不同温度下,铅、铂的蒸汽压由下面的方程进行计算:
1gp=-AT-1+B-C1gT-DT
在不同温度下,计算所得铅、铂的蒸汽压分别如下表1所示。由表可知,铅、铂在不同温度下蒸汽压差别很大,真空蒸馏可实现有效分离。
表1不同温度下Pb、Pt的蒸汽压
温度/K | 1100 | 1150 | 1200 | 1250 |
Pb蒸汽压/Pa | 12.0 | 28.9 | 64.6 | 1.34×102 |
Pt蒸汽压/Pa | 5.24×10-14 | 6.60×10-13 | 6.72×10-12 | 5.67×10-11 |
针对不同温度下铅、铂蒸汽压差距大的特点,本发明将铅铂合金置于耐高温坩埚中,再放入真空蒸馏炉中进行真空蒸馏,使铅蒸发后再冷凝,得到金属铅,蒸余物为金属铂,从而实现铅铂合金的分离。具体实施方案包括以下几个步骤。
1以铅捕集铂所得的铅铂合金为原料,放入耐高温材料制成的坩埚中,再将坩埚放入真空蒸馏炉中,密封。
2开启真空泵,抽真空使压力达到20~100Pa,开启冷凝器的(冷凝器设置于真空蒸馏炉顶部)冷却水。
3开启加热系统,将铅铂合金升温至蒸馏所需温度,保持恒温一段时间,使铅蒸发成气态,铅蒸汽上升真空蒸馏炉的顶部至冷凝器时冷凝成金属铅,蒸余物为纯度高的金属铂,从而实现铅铂有效分离。
本发明具有工艺简单,流程短,节能,高效,清洁等优点,实现了铅铂合金的分离,直接得到金属铅和金属铂,不需进一步还原处理,控制适当的工艺条件可以得到纯金属铂,铅和铂的回收率均达到或者接近百分之百。
实验确定的最佳分离条件为:蒸发温度1250K,蒸发时间3h,真空度30Pa。
本发明可采用各种带有冷凝专置的真空加热炉实现铅-铂合金的有效分离。
具体实施方式
实施例1
将10g含Pb、Pt分别为90%、10%的铅铂合金置于耐高温材料制成的坩埚中,放入真空蒸馏炉中,密封后开启真空泵及冷却水系统,抽真空使压力为30Pa。启动加热装置,升温至1200K,恒温蒸发3h。铅蒸发上升至冷凝器处,冷凝并收集在冷凝器上,铂残留在蒸余物中,纯度得到提高。取出蒸出铅及蒸余物,蒸余物重量为1.45g,铅脱除率达到95.00%,铂纯度提高至68.97%。
实施例2
将10g含Pb、Pt分别为90%、10%的铅铂合金置于耐高温材料制成的坩埚中,放入真空蒸馏炉中,密封后开启真空泵及冷却水系统,抽真空使压力为80Pa。开启加热系统,使铅铂合金升温至1250K,恒温蒸发2.5h。铅蒸发上升至冷凝器处,冷凝并收集在冷凝器上,铂残留在蒸余物中。取出蒸出铅及蒸余物,蒸余物重量为1.31g。在温度1250K,蒸发时间2.5h,压力80Pa条件下,铅脱除率为96.56%,铂纯度由原来的10%提高为76.33%。
实施例3
将10g含Pb、Pt分别为90%、10%的铅铂合金置于耐高温材料制成的坩埚中,放入真空蒸馏炉中,密封后开启真空泵及冷却水系统,抽真空使压力为30Pa。开启加热系统,使铅铂合金升温至1250K,恒温蒸发2h。铅蒸发上升至冷凝系统,冷凝并收集在冷凝器上,铂残留在蒸余物中。取出蒸出铅及蒸余物,蒸余物重量为1.09g。在30Pa,1250K,蒸发时间2h条件下,铅脱出率为99%,铂纯度由原来的10%提高到91.74%。
实施例4
将10g含Pb、Pt分别为90%、10%的铅铂合金置于耐高温材料制成的坩埚中,放入真空蒸馏炉中,密封后开启真空泵及冷却水系统,抽真空使压力为30Pa。升温至1250K,恒温蒸发3h。铅蒸发上升至冷凝器,冷凝并收集在冷凝器上,铂残留在蒸余物中,纯度得到提高。取出蒸出铅及蒸余物,蒸余物重量为1.00g,铅脱除率达到100%,得到纯的金属铂。
Claims (4)
1、一种真空蒸馏分离铅铂合金的方法,其特征在于,以铅铂合金为原料,在真空蒸馏炉中,压力为20~100Pa、1000-1300K的温度下进行铅、铂蒸馏分离,蒸余物为纯度高的铂。
2、根据权利要求1所述的一种真空蒸馏分离铅铂合金的方法,其特征在于,真空蒸馏分离时间为2-4小时。
3、根据权利要求1所述的一种真空蒸馏分离铅铂合金的方法,其特征在于,以铅捕集铂所得的铅铂合金为原料。
4、根据权利要求1-3任一项所述的一种真空蒸馏分离铅铂合金的方法,其特征在于,在30Pa,升温至1250K,恒温蒸发3h,进行铅、铂蒸馏分离。