CN101066053A - 一种纳米硒/竹炭保鲜剂的水热合成方法 - Google Patents

一种纳米硒/竹炭保鲜剂的水热合成方法 Download PDF

Info

Publication number
CN101066053A
CN101066053A CN 200710111699 CN200710111699A CN101066053A CN 101066053 A CN101066053 A CN 101066053A CN 200710111699 CN200710111699 CN 200710111699 CN 200710111699 A CN200710111699 A CN 200710111699A CN 101066053 A CN101066053 A CN 101066053A
Authority
CN
China
Prior art keywords
bamboo charcoal
preservative
selenium
nanometer selenium
hydrothermal synthesis
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200710111699
Other languages
English (en)
Other versions
CN100433976C (zh
Inventor
覃爱苗
韦冬华
曾志超
庞振芳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guilin University of Technology
Original Assignee
Guilin University of Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guilin University of Technology filed Critical Guilin University of Technology
Priority to CNB2007101116999A priority Critical patent/CN100433976C/zh
Publication of CN101066053A publication Critical patent/CN101066053A/zh
Application granted granted Critical
Publication of CN100433976C publication Critical patent/CN100433976C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种纳米硒/竹炭新型保鲜剂的水热合成方法。将0.2-1.2克的颗粒竹炭或粉末竹炭、0.017-0.086克亚硒酸钠、32毫升蒸馏水及0.05-0.3毫升浓度为80%的水合肼混合物置于50毫升的内衬聚四氟乙烯的不锈钢反应釜中,将反应釜放入烘箱加热至100-180℃,升温速率约为6℃/min,保温24小时,冷却至室温;最终产物过滤,用去离子水、无水乙醇冲洗除去最终产物中可能残留的离子,然后在60-80℃烘箱中进行干燥24小时,得到红色纳米硒/竹炭保鲜剂。本发明设备简单,操作方便,容易控制,得到不同形貌的红色纳米硒/竹炭对杜鹃花均具有明显的保鲜作用。

Description

一种纳米硒/竹炭保鲜剂的水热合成方法
技术领域
本发明涉及一种用水热合成方法制备具有明显保鲜作用的纳米硒/竹炭保鲜剂的方法。
背景技术
竹炭是竹材在高温下热解后的固体产物,其机械强度较高,孔结构发达,导电性能良好,可以用作吸附剂、导电材料等。竹炭的成分除碳(75%-95(wt)%)外,还含有生物成长所需要保持平衡的钙、钾、钠、镁等矿物质以及多种药物成分。另外,竹炭还有增加碱性、辐射远红外线、产生负离子效应等特殊功效,可以用来消毒杀菌、治疗疾病、改善居住环境。目前竹炭在许多领域如燃料、水质净化、居室调湿、吸附异味等方面已开发很多用途。硒是环境中一种重要的生命元素,植物体内的硒主要以硒蛋白、硒核酸、硒多糖等多种生物大分子以及硒代半胱氨酸和硒代蛋氨酸等生物小分子有机化合物存在。作物施硒可提高食物链硒水平,改善作物品质,增强作物抗逆性和提高作物产量。红色纳米硒因其具有抗氧化、免疫调节等特殊的生物学功能在动物科学领域中的应用已引起广泛的研究。
发明内容
本发明的目的是提供一种以竹炭为载体,制备具有明显保鲜作用的红色纳米硒/竹炭保鲜剂的方法。
本发明具体步骤为:
将0.2-1.2克的颗粒竹炭或粉末竹炭、0.017-0.086克亚硒酸钠、32毫升蒸馏水及0.05-0.3毫升浓度为80%的水合肼混合物置于50毫升的内衬聚四氟乙烯的不锈钢反应釜中,将反应釜放入烘箱加热至100-180℃,升温速率约为6℃/min,保温24小时,然后在空气中自然冷却至室温。最终产物过滤,用去离子水、无水乙醇冲洗除去最终产物中可能残留的离子,然后在60-80℃烘箱中进行干燥24小时。得到红色纳米硒/竹炭保鲜剂。
本发明设备简单,操作方便,容易控制,通过水热合成法将单质纳米硒负载于竹炭上,得到不同形貌的红色纳米硒/竹炭对杜鹃花均具有明显的保鲜作用,对插在蒸馏水中的杜鹃花能延迟花期6-10天。
具体实施方式
实施例1
将0.6克的颗粒竹炭、0.043克的亚硒酸钠、32毫升蒸馏水及0.13毫升浓度为80%的水合肼混合置于50毫升的内衬聚四氟乙烯的不锈钢反应釜中,将反应釜放入烘箱加热至180℃,升温速率约为6℃/min,保温24小时,然后在空气中自然冷却至室温。最终产物过滤,用去离子水、无水乙醇冲洗除去最终产物中可能残留的离子,然后在60℃烘箱中进行干燥,得到Se形貌为棒状和球状的红色纳米硒/竹炭。0.3克产物置于200ml蒸馏水中,可使一支含两朵新鲜杜鹃花具有延长8天花期的作用。
实施例2
将0.6克的粉末竹炭、0.043克的亚硒酸钠、32毫升蒸馏水、0.13毫升浓度为80%的水合肼混合物置于50ml的内衬聚四氟乙烯的不锈钢反应釜中,将反应釜放入烘箱加热至180℃,升温速率约为6℃/min,保温24小时,然后在空气中自然冷却至室温。最终产物过滤,用去离子水、无水乙醇冲洗除去最终产物中可能残留的离子,然后在60℃烘箱中进行干燥,得到Se形貌为球状的红色纳米硒/竹炭。0.3克产物置于200ml蒸馏水中,可使一支含两朵新鲜杜鹃花具有延长6天花期的作用。

Claims (3)

1.一种纳米硒/竹炭保鲜剂的水热合成方法,其特征在于具体步骤为:
将0.2-1.2克的颗粒竹炭或粉末竹炭、0.017-0.086克亚硒酸钠、32毫升蒸馏水及0.05-0.3毫升浓度为80%的水合肼混合物置于50毫升的内衬聚四氟乙烯的不锈钢反应釜中,将反应釜放入烘箱加热至100-180℃,升温速率约为6℃/min,保温24小时,然后在空气中自然冷却至室温;最终产物过滤,用去离子水、无水乙醇冲洗除去最终产物中可能残留的离子,然后在60-80℃烘箱中进行干燥24小时,得到红色纳米硒/竹炭保鲜剂。
2.如权利要求1所述的合成方法,其特征在于所述的纳米硒/竹炭中的硒形貌随温度及竹炭原料不同而不同。
3.如权利要求1所述的合成方法,其特征在于所述反应在水热中进行。
CNB2007101116999A 2007-06-09 2007-06-09 一种纳米硒/竹炭保鲜剂的水热合成方法 Expired - Fee Related CN100433976C (zh)