CN100544083C - 一种锂离子薄膜电池负极及其制备方法 - Google Patents
一种锂离子薄膜电池负极及其制备方法 Download PDFInfo
- Publication number
- CN100544083C CN100544083C CNB2007100640671A CN200710064067A CN100544083C CN 100544083 C CN100544083 C CN 100544083C CN B2007100640671 A CNB2007100640671 A CN B2007100640671A CN 200710064067 A CN200710064067 A CN 200710064067A CN 100544083 C CN100544083 C CN 100544083C
- Authority
- CN
- China
- Prior art keywords
- lithium
- negative pole
- ion
- cell negative
- fog
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (3)