CN100441759C - 靛兰针织牛仔吸湿汗布的制造方法 - Google Patents

靛兰针织牛仔吸湿汗布的制造方法 Download PDF

Info

Publication number
CN100441759C
CN100441759C CNB2005100409688A CN200510040968A CN100441759C CN 100441759 C CN100441759 C CN 100441759C CN B2005100409688 A CNB2005100409688 A CN B2005100409688A CN 200510040968 A CN200510040968 A CN 200510040968A CN 100441759 C CN100441759 C CN 100441759C
Authority
CN
China
Prior art keywords
indigo
cloth
moisture
knitted
cowboy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB2005100409688A
Other languages
English (en)
Other versions
CN1718890A (zh
Inventor
李雪明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2005100409688A priority Critical patent/CN100441759C/zh
Publication of CN1718890A publication Critical patent/CN1718890A/zh
Application granted granted Critical
Publication of CN100441759C publication Critical patent/CN100441759C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及内衣面料制造技术领域,尤其是一种靛兰针织牛仔吸湿汗布的制造方法,具有如下工艺步骤:a.染色;b.织布,将靛兰纯棉面纱与四管道异型聚酯纤维Coolmax分别喂入针织纬编机,针织纬编成表面为由纯棉面纱构成的靛兰针织牛仔吸湿层、底面为由四管道异型聚酯纤维Coolmax构成的无色导湿层的双面织物;c.用轧车进行后整理:①进布展平;②柔软;③整斜;④展平;⑤定型;⑥烘干;⑦冷却;d.检测,包装。用本发明制造的靛兰针织牛仔吸湿汗布经纬向弹力稳定、耐水洗抗皱折、吸湿率高、透气性好、手感柔软,是制作精品内衣的理想面料,穿着凉爽舒适,特别适用于高强度活动、体育运动、体力劳动、出差或旅游时穿着。

Description

靛兰针织牛仔吸湿汗布的制造方法
技术领域
本发明涉及内衣面料制造技术领域,尤其是一种靛兰针织牛仔吸湿汗布的制造方法。
背景技术
现有内衣汗布面料绝大多数是纯棉或纯棉与涤纶混合和其它化纤相结合,面料虽然松软轻薄透气,但面料的吸湿效果并不理想,人体经过高强度活动、体育运动、体力劳动,或出差、旅游过程中由于涌挤而出汗较多时,人体与汗湿的内衣接触较长时间,人体会产生湿冷感和粘贴效应。
发明内容
为了克服现有的内衣汗布面料的不足,本发明的目的是提供一种具有良好吸湿效果的靛兰针织牛仔吸湿汗布的制造方法。
本发明解决其技术问题所采用的技术方案是:一种靛兰针织牛仔吸湿汗布的制造方法,其特征在于具有如下工艺步骤:
a.染纱,先对纯棉纱整经,再用染色机进行束状靛兰还原染色,然后通过分经机分经,再经制筒机械制成靛兰筒子纱;
b.织布,将靛兰筒子纱即靛兰纯棉面纱与四管道异型聚酯纤维Coolmax分别喂入针织纬编机,针织纬编成表面为由靛兰纯棉面纱构成的靛兰针织牛仔吸湿层、底面由四管道异型聚酯纤维Coolmax构成的无色导湿层的双面织物;
c.用轧车进行后整理,①进布,将织好的布经轧车进布辊和分丝辊进布并展平,轧车压力为3Kg;②柔软,展平的布浸入储有柔软液的轧车水槽,柔软液的浓度为5%,由润滑柔软剂NF-15加95%的水构成,柔软液的温度为55℃~65℃;③整斜,经柔软处理的布经整斜辊整斜;④展平,将整斜处理后的布经分丝辊展平;⑤定型,对展平后的布进行热定型,⑥烘干,对热定型的布进行烘干处理,烘箱温度为150℃~200℃;⑦冷却;
d.检测,包装。
用本发明制造的靛兰针织牛仔吸湿汗布制成内衣穿着时,底面无色导湿层与皮肤接触,由于四管道异型聚酯纤维(Coolmax)为中空结构,截面呈十字,皮肤表面的汗水和湿气被四管道异型聚酯纤维(Coolmax)的四管道迅速导离并被表面靛兰针织牛仔吸湿层的纯棉面纱吸收,让汗水挥发更快,时刻保持皮肤干爽舒适。
本发明的有益效果是,用本发明制造的靛兰针织牛仔吸湿汗布经纬向弹力稳定、耐水洗抗皱折、吸湿率高、透气性好、手感柔软,是制作精品内衣的理想面料,穿着凉爽舒适,特别适用于高强度活动、体育运动、体力劳动、出差或旅游时穿着。
附图说明
下面结合附图和实施例对本发明进一步说明。
图1是用本发明制造的靛兰针织牛仔吸湿汗布的结构示意图。
图2为图1的A-A剖面图。
图中:1.靛兰纯棉面纱,2.四管道异型聚酯纤维Coolmax。
具体实施方式
一种靛兰针织牛仔吸湿汗布的制造方法,其特征在于具有如下工艺步骤:
a.染纱,先对纯棉纱整经,再用染色机进行束状靛兰还原染色,然后通过分经机分经,再经制筒机械制成靛兰筒子纱;
b.织布,将靛兰筒子纱即靛兰纯棉面纱1与四管道异型聚酯纤维Coolmax2分别喂入针织纬编机,针织纬编成如图1和图2所示的表面为由靛兰纯棉面纱1构成的靛兰针织牛仔吸湿层、底面由四管道异型聚酯纤维Coolmax2构成的无色导湿层的双面织物;
c.用轧车进行后整理,①进布,将织好的布经轧车进布辊和分丝辊进布并展平,轧车压力为3Kg;②柔软,展平的布浸入储有柔软液的轧车水槽,柔软液的浓度为5%,由润滑柔软剂NF-15加95%的水构成,柔软液的温度为55℃~65℃;③整斜,经柔软处理的布经整斜辊整斜;④展平,将整斜处理后的布经分丝辊展平;⑤定型,对展平后的布进行热定型,⑥烘干,对热定型的布进行烘干处理,烘箱温度为150℃~200℃;⑦冷却;
d.检测,包装。
用本发明制造的靛兰针织牛仔吸湿汗布制成内衣穿着时,底面无色导湿层与皮肤接触,由于四管道异型聚酯纤维Coolmax为中空结构,截面呈十字,皮肤表面的汗水和湿气被四管道异型聚酯纤维Coolmax2的四管道迅速导离并被表面靛兰针织牛仔吸湿层的靛兰纯棉面纱1吸收,让汗水挥发更快,时刻保持皮肤干爽舒适。

Claims (1)

1、一种靛兰针织牛仔吸湿汗布的制造方法,其特征在于具有如下工艺步骤:
a.染纱,先对纯棉纱整经,再用染色机进行束状靛兰还原染色,然后通过分经机分经,再经制筒机械制成靛兰筒子纱;
b.织布,将靛兰筒子纱即靛兰纯棉面纱(1)与四管道异型聚酯纤维Coolmax(2)分别喂入针织纬编机,针织纬编成表面为由纯棉面纱(1)构成的靛兰针织牛仔吸湿层、底面为由四管道异型聚酯纤维Coolmax(2)构成的无色导湿层的双面织物;
c.用轧车进行后整理,①进布,将织好的布经轧车进布辊和分丝辊进布并展平,轧车压力为3Kg;②柔软,展平的布浸入储有柔软液的轧车水槽,柔软液的浓度为5%,由润滑柔软剂NF-15加95%的水构成,柔软液的温度为55℃~65℃;③整斜,经柔软处理的布经整斜辊整斜;④展平,将整斜处理后的布经分丝辊展平;⑤定型,对展平后的布进行热定型,⑥烘干,对热定型的布进行烘干处理,烘箱温度为150℃~200℃;⑦冷却;
d.检测,包装。
CNB2005100409688A 2005-07-08 2005-07-08 靛兰针织牛仔吸湿汗布的制造方法 Expired - Fee Related CN100441759C (zh)