CN100402737C - 含羊毛的免烫定型易护理西裤的生产方法 - Google Patents
含羊毛的免烫定型易护理西裤的生产方法 Download PDFInfo
- Publication number
- CN100402737C CN100402737C CNB2005100410596A CN200510041059A CN100402737C CN 100402737 C CN100402737 C CN 100402737C CN B2005100410596 A CNB2005100410596 A CN B2005100410596A CN 200510041059 A CN200510041059 A CN 200510041059A CN 100402737 C CN100402737 C CN 100402737C
- Authority
- CN
- China
- Prior art keywords
- trousers
- western
- style trousers
- lining
- wool
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明涉及一种含羊毛的免烫定型易护理西裤,其特征为在西裤的羊毛纤维表面覆有一层水溶性聚胺脂保型性助剂。本发明还涉及含羊毛的免烫定型易护理西裤的生产方法。本发明具有全面的抗皱性能,在西裤的裤挺缝不仅能保持挺括,裤面和裤内、外侧缝也能保持挺括平整;且西裤在洗涤晾干后,不需熨烫就能保形良好,使西裤易于护理;同时西裤具有长久的抗皱性能,西裤在多次洗涤后外观能持久不变形,裤子外观平整度好,且不起毛,不起球。
Description
一、技术领域
本发明涉及一种西裤,尤其是一种含羊毛的免烫定型易护理西裤及其生产方法。
二、技术背景
目前,国内外服装正朝风格多样化、功能多元化的方向发展,其中含羊毛的西裤穿着多次或水洗后,裤腿的前、后挺缝、裤面和内、外侧缝就不能达到挺括、平整、服贴的效果,甚至前、后挺缝消失。因此在护理时裤子只能洗涤后再进行熨烫,且穿着多次就后不再保持挺缝挺括,使裤子的护理极为不便。为此,目前市场上开发了抗皱定型裤,以使西裤具有抗皱的功能,该抗皱定型裤是在裤子的前、后裤挺缝内侧的凹槽处复合有定型涂层,由于此抗皱定型裤的涂层为胶枪将定型胶粘合在前、后裤挺缝内侧,使得西裤的前、后裤挺缝处比较硬,容易引起穿着的不舒服,西裤在洗涤后定型涂层容易混粘在一起或脱落,且在西裤洗涤后内、外侧缝仍然会出现褶皱不平和裤面的不平整,使西裤无法达到机洗后免烫定型易护理的效果。
三、技术内容
为克服上述缺点,本发明的目的在于提供一种含羊毛的免烫定型易护理西裤,使西裤易于机洗和护理,及西裤的裤挺缝、裤面和裤内、外侧缝长久保持挺括平整。
本发明的技术内容是这样实现的,一种含羊毛的免烫定型易护理西裤,其特征为在西裤的羊毛纤维表面覆有一层水溶性聚氨酯保型性助剂。
本发明的另一目的在于提供一种含羊毛的免烫定型易护理西裤的生产方法。
一种含羊毛的免烫定型易护理西裤的生产方法,包括如下生产步骤:
(1)、将含羊毛的西裤面料用浸轧法将在浓度为45~55g/L、PH=7~8的水溶性聚氨酯保型性助剂溶液中进行浸轧,并使面料的带液量为70~80%;
(2)、将浸轧助剂后的西裤面料在80℃以下烘干;
(3)、将西裤面料进行裁剪;
(4)、制裤,再将缝制的西裤熨烫定型;
(5)、采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为145~155℃,焙烘时间为3~5分钟;
(6)、检验并包装成品。
水溶性聚氨酯保型性助剂优选为瑞士汽巴(Ciba)公司的WSR、德国拜尔(Bayer)公司的Bap、德国龙塔(Rotta)公司的367和意大利宁柏迪(Lamberti)公司的PV4。
在西裤面料的羊毛纤维表面涂覆一层水溶性聚氨酯助剂,在西裤熨烫定型后进行高温焙烘,使水溶性聚氨酯助剂的胺基与西裤面料上羊毛纤维的羟基、胺基和羧基基团反应,使水溶性聚氨酯助剂成为固定覆盖在羊毛纤维表面上的一层高分子薄膜,以覆盖住羊毛表面的鳞片层,使羊毛纤维在新的位置重新定型后不易产生变形,并使羊毛纤维运动时不会发生毡缩和达到不起球的效果,从而使西裤易于机洗且在多次机洗后西裤的裤挺缝、裤面和裤内、外侧缝能长久保持挺括平整。
本发明与现有技术相比所具有的优点为:
1、西裤具有全面的抗皱性能,即不仅西裤的裤挺缝能保持挺括,裤面和裤内、外侧缝也能保持挺括平整。
2、西裤具有全面的可机洗功能。
3、西裤在洗涤晾干后,保形良好,不需熨烫,使西裤易于护理。
4、西裤具有长久的抗皱性能,褶裥保持长久,西裤在多次洗涤后外观能持久不变形,裤子外观平整度好,且不起毛,不起球。
四、具体实施例
例1、将含羊毛70%,布克重为320g/m,纱支为98Nm/2×98Nm/2的毛涤贡丝锦用浓度为50g/L、PH=7.5的水溶性聚氨酯助剂溶液进行浸轧处理,并使面料的带液量为75%,助剂为瑞士汽巴公司的WSR;将浸轧后的西裤面料在70℃烘干;将西裤面料进行裁剪;制裤,再将缝制的西裤熨烫定型;采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为150℃,焙烘4分钟;检验并包装成品。
例2、将含羊毛70%,布克重为320g/m,纱支为98Nm/2×98Nm/2的毛涤贡丝锦用浓度为50g/L、PH=7.5的水溶性聚氨酯助剂溶液进行浸轧处理,并使面料的带液量为75%,助剂为德国龙塔(Rotta)公司的367;将浸轧后的西裤面料在70℃烘干;将西裤面料进行裁剪;制裤,再将缝制的西裤熨烫定型;采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为150℃,焙烘4分钟;检验并包装成品。
例3、将布克重为250g/m,纱支为70Nm/2×50Nm/2的全毛薄花呢用浓度为50g/L、PH=7.5的水溶性聚氨酯助剂溶液进行浸轧处理,并使面料的带液量为80%,助剂为德国拜尔公司的Bap;将浸轧后的西裤面料在75℃烘干;将西裤面料进行裁剪;制裤,再将缝制的西裤熨烫定型;采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为150℃,焙烘4分钟;检验并包装成品。
例4、将布克重为250g/m,纱支为70Nm/2×50Nm/2的全毛薄花呢用浸轧法在浓度为50g/L、PH=7.5的水溶性聚氨酯助剂溶液中进行浸轧,并使面料的带液量为80%,助剂为意大利宁柏迪(Lamberti)公司的PV4;将浸轧后的西裤面料在75℃烘干;将西裤面料进行裁剪;制裤,再将缝制的西裤熨烫定型;采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为150℃,焙烘4分钟;检验并包装成品。
例1~例4的的物理指标测量数据如下表:
物理指标 | 实例1 | 实例2 | 实例3 | 实例4 |
边缘收缩率差(3×5A)经/纬(%) | 0.3/0.5 | 0.4/0.8 | 0.5/0.4 | -0.6/0.7 |
呢面平整度(1×7A)(级) | 4 | 4 | 4 | 4 |
线缝平整度(1×7A+1×5A)(级) | 4 | 4 | 4 | 4 |
褶裥保持度(1×7A+1×5A)(级) | 5 | 5 | 5 | 5 |
抗起球(级) | 4-5 | 4-5 | 4-5 | 4-5 |
折皱回复角(度) | 325 | 328 | 330 | 324 |
机洗缩率(3×5A)经/纬(%) | 1.0/1.2 | 0.8/1.0 | 0.5/0.8 | 0.9/1.2 |
Claims (1)
1.含羊毛的免烫定型易护理西裤的生产方法,包括如下生产步骤:(1)、将含羊毛的西裤面料用浸轧法将在浓度为45~55G/L、PH=7~8的水溶性聚氨酯保型性助剂溶液中进行浸轧,并使面料的带液量为70~80%;水溶性聚氨酯保型性助剂为WSR、Bap、367或PV4;
(2)、将浸轧后的西裤面料在80℃以下烘干;
(3)、将西裤面料进行裁剪;
(4)、制裤,将缝制的西裤熨烫定型;
(5)、采用焙烘定型机将熨烫定型后的西裤高温焙烘,焙烘温度为145~155℃,焙烘3~5分钟;
(6)、检验并包装成品。