WO2016076173A1 - ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子 - Google Patents

ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子 Download PDF

Info

Publication number
WO2016076173A1
WO2016076173A1 PCT/JP2015/081030 JP2015081030W WO2016076173A1 WO 2016076173 A1 WO2016076173 A1 WO 2016076173A1 JP 2015081030 W JP2015081030 W JP 2015081030W WO 2016076173 A1 WO2016076173 A1 WO 2016076173A1
Authority
WO
WIPO (PCT)
Prior art keywords
melting point
metal layer
point metal
low melting
electrodes
Prior art date
Application number
PCT/JP2015/081030
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
吉弘 米田
武雄 木村
佐藤 浩二
裕治 古内
Original Assignee
デクセリアルズ株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by デクセリアルズ株式会社 filed Critical デクセリアルズ株式会社
Priority to KR1020177011371A priority Critical patent/KR101950619B1/ko
Priority to CN201580059056.7A priority patent/CN107735849B/zh
Publication of WO2016076173A1 publication Critical patent/WO2016076173A1/ja

Links

Images

Classifications

    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01HELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES
    • H01H37/00Thermally-actuated switches
    • H01H37/74Switches in which only the opening movement or only the closing movement of a contact is effected by heating or cooling
    • H01H37/76Contact member actuated by melting of fusible material, actuated due to burning of combustible material or due to explosion of explosive material
    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01HELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES
    • H01H85/00Protective devices in which the current flows through a part of fusible material and this current is interrupted by displacement of the fusible material when this current becomes excessive
    • H01H85/02Details
    • H01H85/04Fuses, i.e. expendable parts of the protective device, e.g. cartridges
    • H01H85/05Component parts thereof
    • H01H85/055Fusible members
    • H01H85/08Fusible members characterised by the shape or form of the fusible member
    • H01H85/11Fusible members characterised by the shape or form of the fusible member with applied local area of a metal which, on melting, forms a eutectic with the main material of the fusible member, i.e. M-effect devices
    • HELECTRICITY
    • H01ELECTRIC ELEMENTS
    • H01HELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES
    • H01H85/00Protective devices in which the current flows through a part of fusible material and this current is interrupted by displacement of the fusible material when this current becomes excessive
    • H01H85/02Details
    • H01H85/04Fuses, i.e. expendable parts of the protective device, e.g. cartridges
    • H01H85/05Component parts thereof
    • H01H85/055Fusible members
    • H01H85/12Two or more separate fusible members in parallel

Definitions

  • the present invention relates to a fuse element that is mounted on a current path and cuts off due to self-heating when a current exceeding the rating flows, or heat generated by a heating element, and particularly a fuse element excellent in quick disconnection, And a fuse element, a protection element, a short-circuit element, and a switching element using the same.
  • a fuse element that melts by self-heating when a current exceeding the rating flows and interrupts the current path has been used.
  • the fuse element for example, a holder-fixed fuse in which solder is enclosed in a glass tube, a chip fuse in which an Ag electrode is printed on the surface of a ceramic substrate, or a screw fixing in which a part of a copper electrode is thinned and incorporated in a plastic case or Plug-in fuses are often used.
  • a high melting point solder containing Pb having a melting point of 300 ° C. or higher is preferable for the fuse element in terms of fusing characteristics so as not to melt by the heat of reflow.
  • Pb-containing solder is only limitedly recognized, and it is considered that the demand for Pb-free solder will increase in the future.
  • the fuse element can be surface-mounted by reflow and has excellent mountability to the fuse element, it can handle a large current by raising its rating, and the current path is quickly interrupted when overcurrent exceeds the rating. It is required to have fast fusing properties.
  • an object of the present invention is to provide a fuse element that can be surface-mounted and can achieve both improvement in rating and quick fusing, and a fuse element, a protection element, a short-circuit element, and a switching element using the fuse element. To do.
  • the fuse element according to the present invention is formed by laminating three or more metal layers having different melting points.
  • the fuse element according to the present invention has a fuse element in which three or more metal layers having different melting points are laminated, and the fuse element is blown when an overcurrent exceeding the rating flows.
  • the protection element according to the present invention includes an insulating substrate, a heating element formed on or in the insulating substrate, first and second electrodes provided on the insulating substrate, A heating element extraction electrode electrically connected to the heating element; and a soluble conductor connected across the second electrode from the first electrode through the heating element extraction electrode.
  • the molten conductor is composed of a fuse element in which three or more metal layers having different melting points are laminated, and is melted by energization heat generation of the heating element to cut off between the first and second electrodes.
  • the short-circuit element includes an insulating substrate, a heating element formed on or in the insulating substrate, and first and second electrodes provided adjacent to the insulating substrate.
  • a third electrode that is provided on the insulating substrate and is electrically connected to the heating element, and a soluble conductor that is connected across the first and third electrodes.
  • the molten conductor is composed of a fuse element in which three or more metal layers having different melting points are laminated, melted by energization heat generation of the heating element, short-circuits the first and second electrodes, and the first The third electrode is cut off.
  • the switching element according to the present invention includes an insulating substrate, first and second heating elements formed on the insulating substrate or in the insulating substrate, and a first element provided adjacent to the insulating substrate.
  • First and second electrodes, a third electrode provided on the insulating substrate and electrically connected to the first heating element, and a first electrode connected across the first and third electrodes A soluble conductor, a fourth electrode provided on the insulating substrate and electrically connected to the second heating element, and a fifth electrode provided adjacent to the fourth electrode on the insulating substrate.
  • a second soluble conductor connected across the fifth electrode from the second electrode through the fourth electrode, and the first and second soluble conductors Consists of a fuse element in which three or more metal layers having different melting points are laminated, and is heated by the heat generated by the second heating element.
  • the second fusible conductor is melted to cut off the second and fifth electrodes, and the first fusible conductor is melted by energization heat generation of the first heating element, thereby the first and second electrodes. Are short-circuited between the electrodes.
  • the fuse element does not blow out as a fuse element even when the mounting temperature such as reflow exceeds the melting temperature of the low melting point metal layer by laminating the high melting point metal layer. . Therefore, according to the present invention, the fuse element can be efficiently mounted by reflow.
  • the fuse element according to the present invention is melted by self-heating or heat generation of the heating element. At this time, in the fuse element, the melted low melting point metal layer erodes the high melting point metal layer, so that the high melting point metal layer is melted at a temperature lower than its melting point. Therefore, according to the present invention, the fuse element can be blown in a short time using the erosion action of the high melting point metal layer by the low melting point metal layer.
  • the fuse element according to the present invention is formed by laminating a low-melting metal layer with a low-melting point on a low-melting metal layer, the conductor resistance can be greatly reduced, and a conventional chip fuse of the same size Compared to the above, the current rating can be greatly improved. In addition, it can be made thinner than conventional chip fuses having the same current rating, and is excellent in quick fusing.
  • the fuse element according to the present invention maintains a resistance against a high temperature environment such as a reflow temperature and a low resistance characteristic as compared with a fuse element made of a laminated soluble conductor made of two kinds of metals having different melting points, and has a fast melting property. Excellent cutting ability.
  • FIG. 1 is a cross-sectional view showing a fuse element according to the present invention.
  • FIG. 2 is a cross-sectional view showing a fuse element in which a first low melting point metal layer is laminated as the outermost layer.
  • FIG. 3 is a cross-sectional view showing another fuse element according to the present invention formed by repeating a predetermined laminated pattern.
  • FIG. 4 is a cross-sectional view showing another fuse element according to the present invention in which a predetermined lamination pattern is repeated and a first low melting point metal layer is laminated as the outermost layer.
  • FIG. 5 is a cross-sectional view showing another fuse element according to the present invention.
  • FIG. 6 is a cross-sectional view showing another fuse element in which a second low melting point metal layer is laminated as the outermost layer.
  • FIG. 7 is a cross-sectional view showing another fuse element according to the present invention formed by repeating a predetermined laminated pattern.
  • FIG. 8 is a cross-sectional view showing another fuse element according to the present invention in which a predetermined lamination pattern is repeated and a second low melting point metal layer is laminated as the outermost layer.
  • FIG. 9 is a cross-sectional view showing a fuse element to which the present invention is applied.
  • FIG. 10 is a plan view in which the cover member of the fuse element to which the present invention is applied is omitted.
  • FIG. 11 is a cross-sectional view showing a fuse element in which a flux applied to the fuse element is impregnated with a sheet.
  • FIG. 12 is a cross-sectional view showing a fuse element in which a flux in which a fibrous material is mixed is applied to the fuse element.
  • FIG. 13 is a circuit diagram of the fuse element, where (A) shows before the fuse element is blown and (B) shows after the fuse element is blown.
  • FIG. 14 is a cross-sectional view showing a state where the fuse element of the fuse element to which the present invention is applied is melted.
  • 15A and 15B are diagrams showing a protective element to which the present invention is applied, in which FIG. 15A is a plan view showing the cover member omitted, and FIG.
  • FIG. 15B is a cross-sectional view.
  • FIG. 16 is a cross-sectional view showing a protective element obtained by impregnating a sheet with a flux applied to a fuse element.
  • FIG. 17 is a cross-sectional view illustrating a protection element in which a flux in which a fibrous material is mixed is applied to a fuse element.
  • FIG. 18 is a circuit diagram of a protection element to which the present invention is applied.
  • 19A and 19B are diagrams showing the protection element in a state where the fuse element is melted, where FIG. 19A is a plan view with the cover member omitted, and FIG. 19B is a circuit diagram.
  • 20A and 20B are diagrams showing a short-circuit element to which the present invention is applied, in which FIG.
  • FIG. 20A is a plan view showing the cover member omitted
  • FIG. 20B is a cross-sectional view.
  • FIG. 21 is a cross-sectional view showing a short-circuit element in which a flux applied to a fuse element is impregnated with a sheet.
  • FIG. 22 is a cross-sectional view showing a short-circuit element in which a flux in which a fibrous material is mixed is applied to a fuse element.
  • FIG. 23 is a circuit diagram of the short-circuit element, where (A) shows a state where the switch is turned off, and (B) shows a state where the switch is short-circuited.
  • FIG. 21 is a cross-sectional view showing a short-circuit element in which a flux applied to a fuse element is impregnated with a sheet.
  • FIG. 22 is a cross-sectional view showing a short-circuit element in which a flux in which a fibrous material is mixed is applied to a fuse element.
  • FIG. 24 is a cross-sectional view of the short-circuit element showing a state where the insulated first and second electrodes are short-circuited by the molten conductor.
  • FIG. 25A is a plan view showing the short-circuit element with the cover member omitted.
  • FIG. 25B is a cross-sectional view of the short-circuit element.
  • FIG. 25C is a cross-sectional view in which a flux sheet is mounted on each of the two fuse elements of the short-circuit element.
  • FIG. 25D is a cross-sectional view in which a sheet is impregnated with a flux applied to two fuse elements of the short-circuit element.
  • FIG. 25E is a cross-sectional view in which a flux mixed with a fibrous material is applied to each of two fuse elements of a short-circuit element.
  • FIG. 25F is a cross-sectional view in which a flux mixed with a fibrous material is applied across two fuse elements of a short-circuit element.
  • FIG. 26A is a plan view showing a switching element to which the present invention is applied with a cover member omitted.
  • FIG. 26B is a cross-sectional view of a switching element to which the present invention is applied.
  • FIG. 27 is a cross-sectional view of a switching element in which a flux applied to a fuse element is impregnated with a sheet.
  • FIG. 28 is a cross-sectional view of a switching element in which a flux in which a fibrous material is mixed is applied to a fuse element.
  • FIG. 29 is a circuit diagram of the switching element before the fusing of the fuse element.
  • FIG. 30 is a plan view showing a state where the second fuse element is previously melted in the switching element, omitting the cover member.
  • the second, fourth, and fifth electrodes of the switching element were cut off by melting the fusible conductor that was connected, and the insulated first and second electrodes were short-circuited by the molten conductor. It is a top view which abbreviate
  • FIG. 31A the second, fourth, and fifth electrodes of the switching element were cut off by melting the fusible conductor that was connected, and the insulated first and second electrodes were short-circuited by the molten conductor.
  • FIG. 32 is a circuit diagram of the switching element after the fuse element is melted.
  • the fuse element 1 to which the present invention is applied is used as a fusible conductor for a fuse element, a protective element, a short-circuit element, and a switching element, which will be described later. Alternatively, it is melted by the heat generated by the heating element.
  • the fuse element 1 is formed by laminating three or more metal layers having different melting points. For example, as shown in FIG. 1, a high melting point metal layer 2 and a first melting point having a lower melting point than the high melting point metal layer 2 are used.
  • the first low melting point metal layer 3 and the second low melting point metal layer 4 having a melting point lower than that of the first low melting point metal layer 3 are formed, for example, in a substantially rectangular plate shape.
  • the refractory metal layer 2 is preferably made of, for example, Ag, Cu, or an alloy mainly composed of Ag or Cu, and has a high melting point that does not melt even when the fuse element 1 is mounted on an insulating substrate by a reflow furnace. Have.
  • first low-melting-point metal layer 3 for example, a material generally called “Pb-free solder” made of Sn or an alloy containing Sn as a main component is preferably used.
  • the melting point of the first low melting point metal layer 3 is not necessarily higher than the temperature of the reflow furnace, and may be melted at about 200 ° C.
  • the second low melting point metal layer 4 for example, Bi, In or Bi or an alloy containing In is preferably used.
  • the melting point of the second low melting point metal layer 4 is lower than that of the first low melting point metal layer 3, and starts melting at, for example, 120 ° C to 140 ° C.
  • the fuse element 1 is formed by laminating three or more metal layers having different melting points, so that the fuse element, the protective element, the short-circuit element, and the switching element are excellent in mountability on an insulating substrate. It is possible to improve the mountability of each element using 1 on an external circuit board. Moreover, the fuse element 1 can implement
  • the fuse element 1 when the fuse element 1 includes the refractory metal layer 2, the fuse element 1 is exposed to a high heat environment above the melting point of the first and second low melting metal layers 3 and 4 for a short time by an external heat source such as a reflow furnace.
  • an external heat source such as a reflow furnace.
  • fusing and deformation can be prevented, and deterioration of the fusing characteristics associated with initial interruption, initial short circuit, or fluctuation in rating can be prevented. Therefore, the fuse element 1 can efficiently realize mounting of each element such as a fuse element on an insulating substrate and mounting of each element such as a fuse element on an external circuit board by reflow mounting, thereby improving the mountability. Can be made.
  • the fuse element 1 is formed by laminating the low-resistance refractory metal layer 2, the conductor resistance can be greatly reduced as compared with the fusible conductor using the conventional lead-based refractory solder.
  • the current rating can be greatly improved as compared with a conventional chip fuse of the same size.
  • it can be made thinner than conventional chip fuses having the same current rating, and is excellent in quick fusing.
  • the fuse element 1 includes a first low melting point metal layer 3 having a melting point lower than that of the refractory metal layer 2 and a second low melting point metal layer 4 having a melting point lower than that of the first low melting point metal layer 3. Therefore, melting can be started from the melting point of the second low-melting-point metal layer 4 by self-heating due to overcurrent or heat generation by the heating element, and the fast fusing characteristics can be improved.
  • the second low melting point metal layer 4 is made of Sn—Bi alloy or In—Sn alloy
  • the fuse element 1 starts to melt from a low temperature of about 140 ° C. or about 120 ° C.
  • the melted first and second low melting point metal layers 3 and 4 erode the refractory metal layer 2 (solder erosion), so that the refractory metal layer 2 is melted at a temperature lower than the melting point. Therefore, the fuse element 1 can improve the fast fusing property by utilizing the erosion action of the high melting point metal layer 2 by the first and second low melting point metal layers 3 and 4.
  • the refractory metal layer 2 is preferably laminated between the first low melting point metal layer 3 and the second low melting point metal layer 4. .
  • the fuse element 1 has a high melting point from a lower temperature of the second low melting point metal layer 4 by sandwiching the high melting point metal layer 2 between two kinds of first and second low melting point metal layers 3 and 4 having different melting points. Erosion of one surface of the metal layer 2 is started, and then the refractory metal layer 2 is eroded from both surfaces at the temperature of the first low melting metal layer 3.
  • the fuse element 1 can improve the fast fusing characteristics while being resistant to a high temperature environment such as a reflow temperature. That is, in a fuse element in which a low melting point metal layer made of a general Pb-free solder having a melting point of around 220 ° C. and a high melting point metal layer such as Ag is laminated, resistance to a high temperature environment such as a reflow temperature is to be provided. Then, it is necessary to increase the thickness of the refractory metal layer, so that the fusing time is extended.
  • the low melting point metal layer is formed of a relatively inexpensive Sn / Bi alloy in order to shorten the fusing time of the fuse element, the resistance value becomes high and the rating cannot be improved.
  • the fuse element 1 is preferably made of a first low melting point metal layer 3 in which an alloy containing Sn or Sn as a main component is preferably used and an alloy containing Bi, In, Bi or In.
  • the high melting point metal layer 2 is laminated between the second low melting point metal layer 4 having a lower melting point than the low melting point metal layer 3.
  • the fuse element 1 has the first and / or second low melting point metal layers 3 and 4 having a high thickness.
  • the melting point metal layer 2 can be melted quickly by eroding from both sides.
  • the fuse element 1 includes Bi, In, or an alloy containing Bi or In while maintaining low resistance by including the first low melting point metal layer 3 in which Sn or an alloy containing Sn as a main component is suitably used. Is suitably used, and the second low melting point metal layer 4 having a melting point lower than that of the first low melting point metal layer 3 is provided, so that melting can be started from a low temperature and the quick fusing property can be improved.
  • the refractory metal layer 2 is laminated between the first low melting point metal layer 3 and the second low melting point metal layer 4 having a melting point lower than that of the first low melting point metal layer 3.
  • the melting point of the first low melting point metal layer 3 is increased. Decrease, the melting rate is accelerated, and the fast fusing property can be further improved.
  • the fuse element 1 is preferably laminated with four or more layers of the high melting point metal layer 2, the first low melting point metal layer 3, and the second low melting point metal layer 4. At this time, as shown in FIG. 1, the fuse element 1 is arranged in the order of the first low melting point metal layer 3, the high melting point metal layer 2, the second low melting point metal layer 4, and the high melting point metal layer 2 from the lower layer. Four layers may be laminated.
  • the fuse element 1 shown in FIG. 1 can be melted quickly by laminating one high melting point metal layer 2 between the first and second low melting point metal layers 3 and 4.
  • the fuse element 1 may be used as a connection material for connecting the lowermost first low melting point metal layer 3 on the electrodes of the fuse element, the protective element, the short-circuit element, and the switching element described later. That is, the fuse element 1 may be connected to the electrode of each element by the first low melting point metal layer 3.
  • the fuse element 1 has the inner layer provided between the pair of high melting point metal layers 2 as the second low melting point metal layer 4 and the outer layer as the high melting point metal layer 2, so that each element such as a fuse element can be formed.
  • Resistance to surge (pulse resistance) in which an abnormally high voltage is instantaneously applied to the incorporated electric system can be improved.
  • the fuse element 1 should not be blown until, for example, a current of 100 A flows for several milliseconds.
  • the fuse element 1 is provided with a refractory metal layer 2 such as Ag plating having a low resistance value as an outer layer. It is easy to flow the current applied by the surge, and it is possible to prevent fusing due to self-heating. Therefore, the fuse element 1 can greatly improve the resistance to a surge as compared with a fuse made of a conventional solder alloy.
  • the fuse element 1 can be manufactured by forming the high melting point metal 2 on the surfaces of the first and second low melting point metal layers 3 and 4 by using a plating technique.
  • the fuse element 1 can be efficiently manufactured by, for example, performing Ag plating on the surface of a long solder foil, and can be easily used by cutting according to the size at the time of use.
  • the fuse element 1 may be manufactured by bonding the low melting point metal foils constituting the first and second low melting point metal layers 3 and 4 and the high melting point metal foils constituting the high melting point metal layer 2 together. Good.
  • the fuse element 1 includes, for example, a solder foil constituting the second low-melting point metal layer 4 that is rolled between two rolled Cu foils or Ag foils. It can be manufactured by laminating and pressing the solder foil constituting the first low melting point metal layer 3. In this case, as the low melting point metal foil, it is preferable to select a softer material than the high melting point metal foil. Thereby, the dispersion
  • the film thickness of the low melting point metal foil is reduced by pressing, it is preferable to make it thick beforehand.
  • the low-melting-point metal foil protrudes from the end face of the fuse element by pressing, it is preferable to trim off and adjust the shape.
  • the fuse element 1 is formed by laminating the first and second low melting point metal layers 3 and 4 and the refractory metal layer 2 by using a thin film forming technique such as vapor deposition or another known lamination technique. A fuse element 1 can be formed.
  • an antioxidant film (not shown) may be formed on the surface of the outermost refractory metal layer 2.
  • the fuse element 1 further prevents the oxidation of Cu even when, for example, Cu plating or Cu foil is formed as the refractory metal layer 2 by coating the outermost refractory metal layer 2 with an antioxidant film. be able to. Therefore, the fuse element 1 can prevent a situation where the fusing time is prolonged due to oxidation of Cu, and can be blown in a short time.
  • the fuse element 1 can be made of an inexpensive but easily oxidized metal such as Cu as the refractory metal layer 2 and can be formed without using an expensive material such as Ag.
  • the high melting point metal antioxidant film can be made of the same material as the first and second low melting point metal layers 3 and 4, for example, Pb-free solder containing Sn as a main component.
  • the antioxidant film can be formed by performing tin plating on the surface of the refractory metal layer 2.
  • the antioxidant film can be formed by Au plating or preflux.
  • the fuse element to which the present invention is applied includes the first low melting point metal layer 3, the high melting point metal layer 2, the second low melting point metal layer 4, and the high melting point metal layer 2.
  • the first low melting point metal layer 3 may be laminated as the outermost layer.
  • the inner layer provided between the pair of high melting point metal layers 2 is the second low melting point metal layer 4
  • the outer layer is the high melting point metal layer 2
  • the outermost layer is the first low melting point metal layer 2.
  • a metal layer 3 is formed, and a pair of refractory metal layers 2 are laminated between the first and second low melting point metal layers 3 and 4.
  • the fuse element to which the present invention is applied is a laminate of a first low melting point metal layer 3, a high melting point metal layer 2, a second low melting point metal layer 4, and a high melting point metal layer 2. You may form by repeating a pattern.
  • the fuse element 20 shown in FIG. 3 can reduce the resistance by increasing the thickness of the fuse element and suppress deformation at the time of reflow while maintaining the fast fusing property by repeating the laminated pattern.
  • the fuse element 20 repeats the laminated pattern to maintain a fast fusing property, secure a desired thickness, improve the rating by lowering resistance, and improve resistance to high temperature environments. can do.
  • the fuse element 20 is formed by stacking eight layers by repeating the stacking pattern. However, the fuse element to which the present invention is applied may be stacked by eight or more layers by repeating the stacking pattern.
  • the fuse element to which the present invention is applied is a laminate of a first low melting point metal layer 3, a high melting point metal layer 2, a second low melting point metal layer 4, and a high melting point metal layer 2. While repeating the pattern, the first low melting point metal layer 3 may be laminated as the outermost layer.
  • the fuse element 30 shown in FIG. 4 is obtained by laminating eight layers by repeating the laminating pattern, and then laminating the first low melting point metal layer 3 as the outermost layer.
  • the second low melting point metal layers 3 and 4 are laminated.
  • the fuse element to which the present invention is applied includes a second low melting point metal layer 4, a high melting point metal layer 2, a first low melting point metal layer 3, and a high melting point metal layer from the lower layer.
  • Four layers may be laminated in the order of 2.
  • the fuse element 40 shown in FIG. 5 can be quickly blown by laminating one high melting point metal layer 2 between the first and second low melting point metal layers 3 and 4. can do.
  • the fuse element 40 may be used as a connection material for connecting the lowermost second low melting point metal layer 4 on the electrodes of the fuse element, the protection element, the short-circuit element, and the switching element described later. That is, the fuse element 40 may be connected to the electrode of each element by the second low melting point metal layer 4.
  • the fuse element to which the present invention is applied includes a second low melting point metal layer 4, a high melting point metal layer 2, a first low melting point metal layer 3, and a high melting point metal layer 2.
  • the second low melting point metal layer 4 may be laminated as the outermost layer.
  • the fuse element 50 shown in FIG. 6 has an inner layer provided between the pair of high melting point metal layers 2 as the first low melting point metal layer 3, the outer layer as the high melting point metal layer 2, and the outermost layer as the second low melting point metal layer 2.
  • a metal layer 4 is formed, and a pair of high melting point metal layers 2 are laminated between the first and second low melting point metal layers 3 and 4.
  • the fuse element to which the present invention is applied is a laminate of a second low melting point metal layer 4, a high melting point metal layer 2, a first low melting point metal layer 3, and a high melting point metal layer 2.
  • the fuse element 60 shown in FIG. 7 is formed by repeating the laminated pattern, thereby maintaining the fast fusing property as well as the above-described fuse elements 20 and 30, while reducing the resistance by increasing the thickness of the fuse element and increasing the rigidity. It is possible to suppress deformation during reflow.
  • the fuse element 60 is formed by stacking eight layers by repeating the stack pattern, but the fuse element to which the present invention is applied may be stacked by eight layers or more by repeating the stack pattern.
  • the fuse element to which the present invention is applied is a laminate of a second low melting point metal layer 4, a high melting point metal layer 2, a first low melting point metal layer 3, and a high melting point metal layer 2. While repeating the pattern, the second low melting point metal layer 4 may be laminated as the outermost layer.
  • the fuse element 70 shown in FIG. 8 is obtained by laminating eight layers by repeating the lamination pattern, and then laminating the second low melting point metal layer 4 as the outermost layer.
  • the second low melting point metal layers 3 and 4 are laminated.
  • the fuse elements 1, 10, 20, 30, 40, 50, 60, and 70 are preferably Bi, In, or an alloy containing Bi or In as a metal constituting the second low melting point metal layer.
  • In has a lower resistivity than Sn, it is a rare metal and an expensive material. Therefore, if comprehensive judgment is made including manufacturing costs, availability of materials, etc., In is shown in FIGS.
  • the fuse elements 40, 50, 60, and 70 shown in FIGS. 5 to 8 are preferable to the fuse elements 1, 10, 20, and 30.
  • the volume of the first low melting point metal layer 3 is preferably larger than the volume of the refractory metal layer 2.
  • the fuse elements 1, 10, 20, 30, 40, 50, 60, 70 can be effectively shortened by erosion of the refractory metal layer 2 by increasing the volume of the first refractory metal layer 3. Fusing can be performed.
  • the volume of the second low melting point metal layer 4 is preferably larger than the volume of the refractory metal layer 2.
  • fuse elements, protective elements, short-circuit elements, and switching elements using the above-described fuse elements 1, 10, 20, 30, 40, 50, 60, 70 will be described.
  • each element using the fuse element 1 will be described.
  • the fuse elements 10, 20, 30, 40, 50, 60, 70 may be used.
  • a fuse element 80 to which the present invention is applied includes an insulating substrate 81, a first electrode 82 and a second electrode 83 provided on the insulating substrate 81, and a first electrode and a second electrode.
  • the fuse element 1 is mounted between the first electrode 82 and the second electrode 83.
  • the fuse element 1 is mounted between the first electrode 82 and the second electrode 83.
  • the insulating substrate 81 is formed in a square shape by an insulating member such as alumina, glass ceramics, mullite, zirconia, for example.
  • the insulating substrate 81 may be made of a material used for a printed wiring board such as a glass epoxy board or a phenol board.
  • First and second electrodes 82 and 83 are formed on opposite ends of the insulating substrate 81.
  • the first and second electrodes 82 and 83 are each formed by a conductive pattern such as Ag or Cu wiring, and Sn plating, Ni / Au plating, Ni / Pd plating, Ni / Pd are appropriately applied to the surface as anti-oxidation measures.
  • a protective layer 86 such as / Au plating is provided.
  • the first and second electrodes 82 and 83 are continued from the front surface 81a of the insulating substrate 81 to the first and second external connection electrodes 82a and 83a formed on the back surface 81b through castellation. .
  • the fuse element 80 is mounted on the current path of the circuit board via the first and second external connection electrodes 82a and 83a formed on the back surface 81b.
  • the fuse element 1 is connected to the first and second electrodes 82 and 83 via a connecting material 88 such as solder.
  • the fuse element 1 since the fuse element 1 includes the refractory metal layer 2 and has improved resistance to a high temperature environment, the fuse element 1 is excellent in mountability and has the first and second electrodes 82 and 83 via the connection material 88. After being mounted in between, it can be easily connected by reflow soldering or the like.
  • the fuse element 1 is connected to the first and second electrodes 82 and 83 using the first low melting point metal layer 3 or the second low melting point metal layer 4 provided in the lowermost layer as a connection material. May be.
  • the mounting state of the fuse element 1 will be described. As shown in FIG. 9, the fuse element 80 is mounted with the fuse element 1 spaced from the surface 81 a of the insulating substrate 81.
  • the molten metal of the fuse element adheres on the insulating substrate between the first and second electrodes. Leaks.
  • a fuse element in which a fuse element is formed by printing an Ag paste on a ceramic substrate the ceramic and silver are sintered and bite in and remain between the first and second electrodes. Therefore, a leakage current flows between the first and second electrodes due to the molten residue of the fuse element, and the current path cannot be completely interrupted.
  • the fuse element 80 the fuse element 1 is formed separately from the insulating substrate 81 and mounted away from the surface 81 a of the insulating substrate 81. Accordingly, the fuse element 80 is drawn onto the first and second electrodes 82 and 83 without the molten metal biting into the insulating substrate 81 even when the fuse element 1 is melted, and the first and second electrodes 82 are surely inserted. , 83 can be insulated.
  • the fuse element 80 includes a fuse element 1 for preventing oxidation of the refractory metal layer 2 or the first and second low melting point metal layers 3 and 4, removing oxide at the time of fusing, and improving solder fluidity.
  • a flux may be coated on the front surface or the back surface.
  • a flux sheet 87 may be disposed on the entire outermost layer on the fuse element 1. The flux sheet 87 is obtained by impregnating and holding a fluid or semi-fluid flux in a sheet-like support. For example, a non-woven fabric or a mesh-like cloth is impregnated with the flux.
  • the flux sheet 87 preferably has an area larger than the surface area of the fuse element 1.
  • the flux sheet 87 By disposing the flux sheet 87, the flux can be held over the entire surface of the fuse element 1 even in the heat treatment process when the fuse element 1 is mounted or when the fuse element 80 is mounted. While improving the wettability of the first and second low melting point metal layers 3 and 4 (for example, solder), the oxide while the first and second low melting point metals are dissolved is removed, and the high melting point metal (for example, the fast fusing property can be improved by using the erosion action on Ag).
  • the first and second low melting point metal layers 3 and 4 for example, solder
  • an anti-oxidation film such as Pb-free solder mainly composed of Sn is formed on the surface of the outermost refractory metal layer 2 by disposing the flux sheet 87.
  • the oxidation of the anti-oxidation film is also performed.
  • the material can be removed, the refractory metal layer 2 can be effectively prevented from being oxidized, and the fast fusing property can be maintained and improved.
  • the fuse element 80 is replaced with the flux sheet 87, as shown in FIG. 11, after the flux 85a is applied to the outermost layer of the fuse element 1, a non-woven fabric or a mesh-like fabric is disposed on the flux 85a, A flux may be impregnated.
  • the fuse element 80 may apply a flux 85 b in which a fibrous material is mixed to the entire outermost layer of the fuse element 1 instead of the flux sheet. Viscosity of the flux 85b is increased by mixing the fibrous material, and it is difficult for the flux 85b to flow even in a high-temperature environment. Thus, the oxide 85 can be removed and the wettability can be improved over the entire surface of the fuse element 1.
  • the fibrous material to be mixed with the flux 85b for example, fibers having insulating properties and heat resistance, such as nonwoven fabric fibers and glass fibers, are preferably used.
  • the fuse element 1 can be connected to the first and second electrodes 82 and 83 by reflow soldering as described above. In addition, the fuse element 1 can be connected to the first and second electrodes by ultrasonic welding. You may connect on the 2nd electrode 82,83.
  • a cover member 89 that protects the inside and prevents the molten fuse element 1 from scattering is attached to the surface 81a of the insulating substrate 81 on which the fuse element 1 is provided.
  • the cover member 89 can be formed of an insulating member such as various engineering plastics and ceramics, and is connected via an insulating adhesive 84.
  • the fuse element 80 since the fuse element 1 is covered by the cover member 89, the molten metal is captured by the cover member 89 and can be prevented from being scattered to the surroundings even when the self-heating is interrupted due to the occurrence of arc discharge due to overcurrent. .
  • the cover member 89 has a protrusion 89b extending from the top surface 89a toward the insulating substrate 81 at least to the side surface of the flux sheet 87. Since the side surface of the flux sheet 87 is subject to movement restriction by the projection 89b, the cover member 89 can prevent the positional deviation of the flux sheet 87.
  • the protrusion 89b has a size that holds a predetermined clearance rather than the size of the flux sheet 87, and is provided corresponding to the position where the flux sheet 87 should be held.
  • the protrusion part 89b is good also as a wall surface which wraps around the side surface of the flux sheet 87, and may protrude partially.
  • the cover member 89 is configured to have a predetermined interval between the flux sheet 87 and the top surface 89a. This is because when the fuse element 1 is melted, a clearance is required for the melted fuse element 1 to push up the flux sheet 87.
  • the cover member 89 has a height of the internal space of the cover member 89 (height to the top surface 89a) that is the height of the melted fuse element 1 on the surface 81a of the insulating substrate 81 and the thickness of the flux sheet 87. It is comprised so that it may become larger than the sum of.
  • Such a fuse element 80 has a circuit configuration shown in FIG.
  • the fuse element 80 is incorporated in the current path of the external circuit by being mounted on the external circuit via the first and second external connection electrodes 82a and 83a.
  • the fuse element 80 is not melted by self-heating while a predetermined rated current flows through the fuse element 1.
  • the fuse element 80 cuts off the current path of the external circuit by cutting off the first and second electrodes 82 and 83 by fusing the fuse element 1 by self-heating when an overcurrent exceeding the rating is energized. (FIG. 13B).
  • the fuse element 1 includes the first low melting point metal layer 3 having a melting point lower than that of the refractory metal layer 2 and the second low melting point having a melting point lower than that of the first low melting point metal layer 3. Since the metal layer 4 is laminated, melting starts from the melting point of the second low melting point metal layer 4 due to self-heating due to overcurrent, and the refractory metal layer 2 starts to erode. Therefore, the fuse element 1 is melted at a temperature lower than its melting point by utilizing the erosion action of the refractory metal layer 2 by the first and second refractory metal layers 3 and 4. And can be melted quickly.
  • the molten metal of the fuse element 1 is divided into left and right by the physical pulling action of the first and second electrodes 82 and 83, so that it can be performed quickly and reliably.
  • the current path between the first and second electrodes 82 and 83 can be cut off.
  • a protection element 90 to which the present invention is applied includes an insulating substrate 91, a heating element 93 laminated on the insulating substrate 91 and covered with an insulating member 92, and an insulating substrate.
  • the first electrode 94 and the second electrode 95 formed at both ends of the 91, and a heating element extraction electrode laminated on the insulating member 91 so as to overlap the heating element 93 and electrically connected to the heating element 93 96 and a fuse element 1 having both ends connected to the first and second electrodes 94 and 95 and the center connected to the heating element extraction electrode 96, respectively.
  • the protective element 90 is provided with a cover member 97 for protecting the inside on the insulating substrate 91.
  • the insulating substrate 91 is formed in a rectangular shape by an insulating member such as alumina, glass ceramics, mullite, zirconia, and the like, similarly to the insulating substrate 81.
  • the insulating substrate 91 may be made of a material used for a printed wiring board such as a glass epoxy board or a phenol board.
  • First and second electrodes 94 and 95 are formed on opposite ends of the insulating substrate 91.
  • the first and second electrodes 94 and 95 are each formed of a conductive pattern such as Ag or Cu wiring.
  • the first and second electrodes 94 and 95 are continued from the front surface 91a of the insulating substrate 91 to the first and second external connection electrodes 94a and 95a formed on the back surface 91b through castellation.
  • the protection element 90 is formed on the circuit board by connecting the first and second external connection electrodes 94a and 95a formed on the back surface 91b to connection electrodes provided on the circuit board on which the protection element 90 is mounted. It is incorporated into a part of the formed current path.
  • the heating element 93 is a conductive member that generates heat when energized, and is made of, for example, nichrome, W, Mo, Ru, or a material containing these.
  • the heating element 93 is a paste obtained by mixing powders of these alloys, compositions, or compounds with a resin binder or the like, and forming a pattern on the insulating substrate 91 using a screen printing technique, followed by firing. Etc. can be formed.
  • the heating element 93 is covered with the insulating member 92, and the heating element extraction electrode 96 is formed so as to face the heating element 93 through the insulating member 92.
  • the heating element lead electrode 96 is connected to the fuse element 1, whereby the heating element 93 is superimposed on the fuse element 1 via the insulating member 92 and the heating element lead electrode 96.
  • the insulating member 92 is provided to protect and insulate the heating element 93 and to efficiently transmit the heat of the heating element 93 to the fuse element 1, and is made of, for example, a glass layer.
  • the heating element 93 may be formed inside the insulating member 92 stacked on the insulating substrate 91. Further, the heating element 93 may be formed on the back surface 91b opposite to the surface 91a of the insulating substrate 91 on which the first and second electrodes 94 and 95 are formed, or the heating element 93 may be formed on the surface 91a of the insulating substrate 91. It may be formed adjacent to the first and second electrodes 94 and 95. Further, the heating element 93 may be formed inside the insulating substrate 91.
  • the heating element 93 has one end connected to the heating element extraction electrode 96 and the other end connected to the heating element electrode 99.
  • the heating element extraction electrode 96 is formed on the surface 91 a of the insulating substrate 91 and is laminated on the insulating member 92 so as to face the heating element 93 and is connected to the heating element 93, and the fuse element 1. And an upper layer portion 96b connected to each other.
  • the heating element 93 is electrically connected to the fuse element 1 via the heating element extraction electrode 96.
  • the heating element extraction electrode 96 is disposed opposite to the heating element 93 via the insulating member 92, so that the fuse element 1 can be melted and the molten conductor can be easily aggregated.
  • the heating element electrode 99 is formed on the front surface 91a of the insulating substrate 91, and is continuous with the heating element feeding electrode 99a formed on the back surface 91b of the insulating substrate 91 through castellation.
  • the protection element 90 is connected to the fuse element 1 across the second electrode 95 from the first electrode 94 via the heating element extraction electrode 96.
  • the fuse element 1 is connected to the first and second electrodes 94 and 95 and the heating element extraction electrode 96 through a connection material 100 such as solder.
  • the fuse element 1 since the fuse element 1 includes the refractory metal layer 2 and has improved resistance to a high temperature environment, the fuse element 1 is excellent in mountability, and the first and second electrodes 94 and 95 are connected via the connection material 100. And after mounting on the heating element lead-out electrode 96, it can be easily connected by reflow soldering or the like.
  • the fuse element 1 uses the first low melting point metal layer 3 or the second low melting point metal layer 4 provided as the lowermost layer as a connection material, and the first and second electrodes 94 and 95 and the heating element. It may be connected to the extraction electrode 96.
  • the protective element 90 includes a fuse element 1 for preventing oxidation of the high melting point metal layer 2 or the first and second low melting point metal layers 3, 4, removing oxide during fusing and improving solder fluidity.
  • a flux may be coated on the front surface or the back surface.
  • a flux sheet 101 may be disposed on the entire outermost layer on the fuse element 1. Similar to the flux sheet 87, the flux sheet 101 is obtained by impregnating and holding a fluid or semi-fluid flux in a sheet-like support. For example, a nonwoven fabric or a mesh-like cloth is impregnated with the flux. Is.
  • the flux sheet 101 preferably has an area larger than the surface area of the fuse element 1. Thereby, even when the fuse element 1 is completely covered with the flux sheet 101 and the volume expands due to melting, it is possible to reliably realize rapid fusing by removing oxides by flux and improving wettability.
  • the flux sheet 101 By disposing the flux sheet 101, the flux can be held over the entire surface of the fuse element 1 even in the heat treatment process when the fuse element 1 is mounted or when the protection element 90 is mounted. While improving the wettability of the first and second low melting point metal layers 3 and 4 (for example, solder), the oxide while the first and second low melting point metals are dissolved is removed, and the high melting point metal (for example, the fast fusing property can be improved by using the erosion action on Ag).
  • the first and second low melting point metal layers 3 and 4 for example, solder
  • an anti-oxidation film such as Pb-free solder containing Sn as a main component is formed on the surface of the outermost refractory metal layer 2 by arranging the flux sheet 101, the oxidation of the anti-oxidation film The material can be removed, the refractory metal layer 2 can be effectively prevented from being oxidized, and the fast fusing property can be maintained and improved.
  • the protective element 90 instead of the flux sheet 101, the protective element 90, as shown in FIG. 16, after the flux 104a is applied to the outermost layer of the fuse element 1, a non-woven fabric or a mesh-like fabric is disposed on the flux 104a, The flux 104a may be impregnated.
  • the protection element 90 may apply a flux 104 b in which a fibrous material is mixed to the entire outermost layer of the fuse element 1 instead of the flux sheet. Viscosity of the flux 104b is increased by mixing the fibrous material, and it is difficult for the flux 104b to flow even in a high-temperature environment. Thus, the oxide 104 can be removed from the entire surface of the fuse element 1 and the wettability can be improved.
  • a fiber having insulating properties and heat resistance such as a nonwoven fabric fiber and a glass fiber is preferably used.
  • the first and second electrodes 94 and 95, the heating element extraction electrode 96, and the heating element electrode 99 are formed of a conductive pattern such as Ag or Cu, and the surface thereof is appropriately Sn-plated, Ni / Au plated, Ni A protective layer 98 such as / Pd plating or Ni / Pd / Au plating is formed.
  • the surface is prevented from being oxidized, and the first and second electrodes 94 are formed by the connection material 100 such as the first and second low melting point metal layers 3 and 4 of the fuse element 1 and the solder for connecting the fuse element 1.
  • 95 and the heating element extraction electrode 96 can be suppressed.
  • first and second electrodes 94 and 95 are formed with an outflow prevention portion 102 made of an insulating material such as glass for preventing the molten conductor of the fuse element 1 and the connection material 100 of the fuse element 1 from flowing out. ing.
  • the protective element 90 has a cover member 97 attached to the surface 91a of the insulating substrate 91 provided with the fuse element 1 for protecting the inside and preventing the molten fuse element 1 from scattering.
  • the cover member 97 can be formed of an insulating member such as various engineering plastics and ceramics. Since the fuse element 1 is covered with the cover member 97, the protection element 90 can prevent the molten metal from being captured by the cover member 97 and scattered to the surroundings.
  • the cover member 97 has a protrusion 97b extending from the top surface 97a toward the insulating substrate 81 at least to the side surface of the flux sheet 101. Since the side surface of the flux sheet 101 is subject to movement restriction by the protrusion 97b, the cover member 97 can prevent the positional deviation of the flux sheet 101.
  • the protrusion 97b has a size that holds a predetermined clearance rather than the size of the flux sheet 101, and is provided corresponding to the position where the flux sheet 101 should be held.
  • the protrusion part 97b is good also as a wall surface which wraps around the side surface of the flux sheet 101, and may protrude partially.
  • the cover member 97 is configured to have a predetermined interval between the flux sheet 101 and the top surface 97a. This is because when the fuse element 1 is melted, a clearance is required for the melted fuse element 1 to push up the flux sheet 101.
  • the cover member 97 has a height of the internal space of the cover member 97 (a height up to the top surface 97a) that is the height of the fuse element 1 melted on the surface 91a of the insulating substrate 91 and the thickness of the flux sheet 101. It is comprised so that it may become larger than the sum of.
  • a heating path to the heating element 93 that reaches the heating element power supply electrode 99a, the heating element electrode 99, the heating element 93, the heating element extraction electrode 96, and the fuse element 1 is formed.
  • the protection element 90 is connected to an external circuit in which the heating element electrode 99 energizes the heating element 93 via the heating element power supply electrode 99a, and the energization across the heating element electrode 99 and the fuse element 1 is controlled by the external circuit. .
  • the protection element 90 constitutes a part of the energization path to the heating element 93 when the fuse element 1 is connected to the heating element extraction electrode 96. Therefore, when the fuse element 1 is melted and the connection with the external circuit is interrupted, the protection element 90 can also stop the heat generation because the energization path to the heating element 93 is also interrupted.
  • the protection element 90 to which the present invention is applied has a circuit configuration as shown in FIG. That is, the protective element 90 is energized via the connecting point between the fuse element 1 and the fuse element 1 connected in series across the first and second external connection electrodes 94a and 95a via the heating element lead electrode 96.
  • the circuit configuration includes a heating element 93 that melts the fuse element 1 by generating heat.
  • the first and second electrodes 94 and 95 and the heating element electrode 99 are connected to the first and second external connection electrodes 94a and 95a and the heating element feeding electrode 99a, respectively, to the external circuit board.
  • the fuse element 1 is connected in series on the current path of the external circuit via the first and second electrodes 94 and 95, and the heating element 93 is connected to the external circuit via the heating element electrode 99. It is connected to the provided current control element.
  • the protection element 90 having such a circuit configuration, when the current path of the external circuit needs to be interrupted, the heating element 93 is energized by the current control element provided in the external circuit. As a result, the protection element 90 melts the fuse element 1 incorporated on the current path of the external circuit due to the heat generated by the heating element 93, and as shown in FIG. The fuse element 1 is blown by being attracted to the heating element lead electrode 96 and the first and second electrodes 94 and 95 having high wettability. As a result, the fuse element 1 can reliably melt the space between the first electrode 94 and the heating element extraction electrode 96 and the second electrode 95 (FIG. 19B), and interrupt the current path of the external circuit. it can. Further, when the fuse element 1 is melted, power supply to the heating element 93 is also stopped.
  • the fuse element 1 includes the first low melting point metal layer 3 having a melting point lower than that of the refractory metal layer 2 and the second low melting point having a melting point lower than that of the first low melting point metal layer 3. Since the metal layer 4 is laminated, the melting starts from the melting point of the second low melting point metal layer 4 and the high melting point metal layer 2 starts to erode. Therefore, in the fuse element 1, the refractory metal layer 2 is melted at a temperature lower than the melting temperature by utilizing the erosion action of the refractory metal layer 2 by the first and second low melting metal layers 3 and 4. , Can be blown quickly.
  • FIG. 20A shows a plan view of the short-circuit element 110
  • FIG. 20B shows a cross-sectional view of the short-circuit element 110.
  • the short-circuit element 110 includes an insulating substrate 111, a heating element 112 provided on the insulating substrate 111, a first electrode 113 and a second electrode 114 provided adjacent to each other on the insulating substrate 111, and a first electrode A current path is configured by being provided adjacent to the electrode 113 and extending between the third electrode 115 electrically connected to the heating element 112 and the first and third electrodes 113 and 115.
  • the fuse element 1 which blows the current path between the first and third electrodes 113 and 115 by heating from the heating element 112 and short-circuits the first and second electrodes 113 and 114 via the molten conductor, Is provided.
  • a cover member 116 that protects the inside is attached on the insulating substrate 111.
  • the insulating substrate 111 is formed in a rectangular shape by an insulating member such as alumina, glass ceramics, mullite, zirconia.
  • the insulating substrate 111 may be made of a material used for a printed wiring board such as a glass epoxy board or a phenol board.
  • the heating element 112 is covered with an insulating member 118 on the insulating substrate 111. On the insulating member 118, first to third electrodes 113 to 115 are formed.
  • the insulating member 118 is provided to efficiently transmit the heat of the heating element 112 to the first to third electrodes 113 to 115, and is made of, for example, a glass layer.
  • the heating element 112 can make the molten conductor easily aggregate by heating the first to third electrodes 113 to 115.
  • the first to third electrodes 113 to 115 are formed of a conductive pattern such as Ag or Cu wiring.
  • the first electrode 113 is formed adjacent to the second electrode 114 on one side and insulated.
  • a third electrode 115 is formed on the other side of the first electrode 113.
  • the first electrode 113 and the third electrode 115 are brought into conduction when the fuse element 1 is connected to form a current path of the short-circuit element 110.
  • the first electrode 113 is connected to a first external connection electrode 113 a provided on the back surface 111 b of the insulating substrate 111 through a castellation that faces the side surface of the insulating substrate 111.
  • the second electrode 114 is connected to a second external connection electrode 114 a provided on the back surface 111 b of the insulating substrate 111 through a castellation that faces the side surface of the insulating substrate 111.
  • the third electrode 115 is connected to the heating element 112 via the heating element extraction electrode 120 provided on the insulating substrate 111 or the insulating member 118.
  • the heating element 112 is connected to the heating element power supply electrode 121 a provided on the back surface 111 b of the insulating substrate 111 through a heating element electrode 121 and a castellation that faces the side edge of the insulating substrate 111.
  • the fuse element 1 is connected to the first and third electrodes 113 and 115 via a connecting material 117 such as solder. As described above, since the fuse element 1 includes the refractory metal layer 2 and has improved resistance to a high temperature environment, the fuse element 1 has excellent mountability, and the first and third electrodes 113 and 115 are connected via the connection material 117. After being mounted in between, it can be easily connected by reflow soldering or the like.
  • the fuse element 1 is connected to the first and third electrodes 113 and 115 using the first low-melting-point metal layer 3 or the second low-melting-point metal layer 4 provided as the lowermost layer as a connection material. May be.
  • the short-circuit element 110 includes a fuse element 1 for preventing oxidation of the refractory metal layer 2 or the first and second low-melting metal layers 3, 4, removing oxide during fusing, and improving solder fluidity.
  • a flux may be coated on the front surface or the back surface.
  • a flux sheet 122 may be disposed on the entire outermost layer on the fuse element 1. Similar to the flux sheet 87 described above, the flux sheet 122 is obtained by impregnating and holding a fluid or semi-fluid flux in a sheet-like support. For example, a non-woven fabric or a mesh-like cloth is impregnated with the flux. It is a thing.
  • the flux sheet 122 preferably has an area larger than the surface area of the fuse element 1. Thereby, even when the fuse element 1 is completely covered with the flux sheet 122 and the volume expands due to melting, it is possible to surely realize oxide removal by flux and quick fusing by improving wettability.
  • the flux sheet 122 By disposing the flux sheet 122, the flux can be held over the entire surface of the fuse element 1 even in the heat treatment process when the fuse element 1 is mounted or when the short-circuit element 110 is mounted. While improving the wettability of the first and second low melting point metal layers 3 and 4 (for example, solder), the oxide while the first and second low melting point metals are dissolved is removed, and the high melting point metal (for example, the fast fusing property can be improved by using the erosion action on Ag).
  • the first and second low melting point metal layers 3 and 4 for example, solder
  • an anti-oxidation film such as Pb-free solder containing Sn as a main component is formed on the surface of the outermost refractory metal layer 2 by arranging the flux sheet 122, the oxidation of the anti-oxidation film The material can be removed, oxidation of the refractory metal layer 2 can be effectively prevented, and fast fusing property can be maintained and improved.
  • the short-circuit element 110 instead of the flux sheet 122, the short-circuit element 110, as shown in FIG. 21, after applying the flux 119a to the outermost layer of the fuse element 1, arrange a non-woven fabric or mesh-like fabric on the flux 119a, A flux 119a may be impregnated.
  • the short-circuit element 110 may apply a flux 119 b in which a fibrous material is mixed to the entire outermost layer of the fuse element 1 instead of the flux sheet. Viscosity of the flux 119b is increased by mixing the fibrous material, and it is difficult for the flux 119b to flow even in a high temperature environment. Thus, the oxide can be removed and the wettability can be improved over the entire surface of the fuse element 1.
  • a fiber having insulating properties and heat resistance such as a nonwoven fabric fiber and a glass fiber is preferably used.
  • the first electrode 113 preferably has a larger area than the third electrode 115.
  • the short-circuit element 110 can agglomerate more molten conductors on the first and second electrodes 113 and 114 and reliably short-circuit the first and second electrodes 113 and 114. Yes (see FIG. 24).
  • the first to third electrodes 113, 114, 115 can be formed using a general electrode material such as Cu or Ag, but at least on the surfaces of the first and second electrodes 113, 114. It is preferable that a coating 129 such as Ni / Au plating, Ni / Pd plating, or Ni / Pd / Au plating is formed by a known plating process. Thereby, the oxidation of the first and second electrodes 113 and 114 can be prevented, and the molten conductor can be reliably held. Further, when the short-circuit element 110 is reflow-mounted, the first electrode is obtained by melting the solder connecting the fuse element 1 or the first or second low melting point metal layer 3 or 4 forming the outer layer of the fuse element 1. It is possible to prevent 113 from being melted (soldered).
  • first to third electrodes 113 to 115 are formed with an outflow prevention portion 126 made of an insulating material such as glass for preventing the molten conductor of the fuse element 1 and the connection material 117 of the fuse element 1 from flowing out. ing.
  • the short-circuit element 110 has a cover member 116 attached to the surface 111a of the insulating substrate 111 on which the fuse element 1 is provided to protect the inside and prevent the molten fuse element 1 from scattering.
  • the cover member 116 can be formed of an insulating member such as various engineering plastics and ceramics. Since the fuse element 1 is covered with the cover member 116 in the short-circuit element 110, the molten metal is captured by the cover member 116 and can be prevented from being scattered to the surroundings.
  • the cover member 116 has a projection 116b extending from the top surface 116a toward the insulating substrate 111 at least to the side surface of the flux sheet 122. Since the side surface of the flux sheet 122 is restricted by the protrusion 116b, the cover member 116 can prevent the position of the flux sheet 122 from being displaced.
  • the protrusion 116b has a size that holds a predetermined clearance rather than the size of the flux sheet 122, and is provided corresponding to the position where the flux sheet 122 should be held.
  • the protrusion part 116b is good also as a wall surface which wraps around the side surface of the flux sheet 122, and may protrude partially.
  • the cover member 116 is configured to have a predetermined interval between the flux sheet 122 and the top surface 116a. This is because when the fuse element 1 is melted, a clearance is required for the melted fuse element 1 to push up the flux sheet 122.
  • the cover member 116 has a height of the internal space of the cover member 116 (height to the top surface 116 a) that is the height of the melted fuse element 1 on the surface 111 a of the insulating substrate 111 and the thickness of the flux sheet 122. It is comprised so that it may become larger than the sum of.
  • the short circuit element 110 as described above has a circuit configuration as shown in FIGS. That is, in the short-circuit element 110, when the first electrode 113 and the second electrode 114 are normally insulated (FIG. 23A), when the fuse element 1 is melted by the heat generated by the heating element 112, the molten conductor is A switch 123 that is short-circuited is formed (FIG. 23B).
  • the first external connection electrode 113a and the second external connection electrode 114a constitute both terminals of the switch 123.
  • the fuse element 1 is connected to the heating element 112 via the third electrode 115 and the heating element extraction electrode 120.
  • the short-circuit element 110 is incorporated into an electronic device or the like, so that the both terminals 113a and 114a of the switch 123 are connected to the current path of the electronic device, and the switch 123 is short-circuited when the current path is conducted.
  • the current path of the electronic component is formed.
  • the short-circuit element 110 when the electronic component provided on the current path of the electronic component and both terminals 113a and 114a of the switch 123 are connected in parallel and an abnormality occurs in the electronic component connected in parallel, the short-circuit element 110 generates a heating element. Electric power is supplied between the power supply electrode 121a and the first external connection electrode 113a, and heat is generated when the heating element 112 is energized. When the fuse element 1 is melted by this heat, the molten conductor aggregates on the first and second electrodes 113 and 114 as shown in FIG.
  • the agglomerated molten conductors are coupled to each other on the first and second electrodes 113 and 114, thereby the first and second electrodes 113. 114 are short-circuited.
  • the short-circuit element 110 is short-circuited between both terminals of the switch 123 (FIG. 23B), and forms a bypass current path that bypasses the electronic component in which an abnormality has occurred.
  • the fuse element 1 since the fuse element 1 is melted, the first and third electrodes 113 and 115 are fused, so that the power supply to the heating element 112 is also stopped.
  • the fuse element 1 includes the first low melting point metal layer 3 having a melting point lower than that of the refractory metal layer 2 and the second low melting point having a melting point lower than that of the first low melting point metal layer 3. Since the metal layer 4 is laminated, the melting starts from the melting point of the second low melting point metal layer 4 and the high melting point metal layer 2 starts to erode. Therefore, in the fuse element 1, the refractory metal layer 2 is melted at a temperature lower than the melting temperature by utilizing the erosion action of the refractory metal layer 2 by the first and second low melting metal layers 3 and 4. , Can be blown quickly.
  • the short-circuit element 110 does not necessarily need to cover the heating element 112 with the insulating member 118, and the heating element 112 may be installed inside the insulating substrate 111.
  • the heating element 112 can be heated in the same manner as when the insulating member 118 such as a glass layer is interposed.
  • the short-circuit element 110 includes the heating element 112 of the insulating substrate 111.
  • the first to third electrodes 113 to 115 may be provided on the surface opposite to the formation surface.
  • the heating element 112 can be formed by a simpler process than that in the insulating substrate 111. In this case, it is preferable to form an insulating member 118 on the heating element 112 in terms of protecting the resistor and ensuring insulation during mounting.
  • the heating element 112 is installed on the formation surface of the first to third electrodes 113 to 115 of the insulating substrate 111 and is also provided along with the first to third electrodes 113 to 115. Good.
  • the heating element 112 can be formed by a simpler process than in the insulating substrate 111. Also in this case, it is preferable that the insulating member 118 is formed on the heating element 112.
  • the short-circuit element according to the present invention is mounted over the fourth electrode 124 adjacent to the second electrode 114 and between the second and fourth electrodes 114 and 124.
  • the second fuse element 125 may be formed.
  • the second fuse element 125 has the same configuration as the fuse element 1.
  • the short circuit element 110 may be mounted with the flux sheet 122 over the fuse element 1 and the second fuse element 125. As shown in FIG. 25 (C), It may be mounted on each of the fuse element 1 and the second fuse element 125.
  • the short-circuit element 110 is formed by applying a non-woven fabric or a mesh-like cloth to the fuse element 1 and the first cloth after the flux 119a is applied to each of the fuse element 1 and the second fuse element 125.
  • Two fuse elements 125 may be mounted, or as shown in FIG. 25E, a nonwoven fabric or a mesh-shaped cloth may be mounted on each of the fuse element 1 and the second fuse element 125.
  • the short-circuit element 110 may apply a flux 119b in which the fibrous material is mixed and the viscosity is increased to each of the fuse element 1 and the second fuse element 125. .
  • the short-circuit element 110 when the fuse element 1 and the second fuse element 125 are melted, the molten conductor wets and spreads between the first and second electrodes 113 and 114, and the first and second electrodes 113, 114 is short-circuited.
  • the short-circuit element 110 shown in FIG. 25 is the same as that described above except that the fourth electrode 124 and the second fuse element 125 are provided. To do.
  • the first and second electrodes 113 and 114 have a larger area than the third and fourth electrodes 115 and 124.
  • the short-circuit element 110 can agglomerate more molten conductors on the first and second electrodes 113 and 114 and reliably short-circuit the first and second electrodes 113 and 114. it can.
  • FIG. 26A shows a plan view of the switching element 130
  • FIG. 26B shows a cross-sectional view of the switching element 130.
  • the switching element 130 includes an insulating substrate 131, a first heating element 132 and a second heating element 133 provided on the insulating substrate 131, a first electrode 134 provided adjacent to the insulating substrate 131, and Provided adjacent to the second electrode 135 and the first electrode 134, provided adjacent to the third electrode 136 electrically connected to the first heating element 132, and the second electrode 135 And a fourth electrode 137 electrically connected to the second heating element 133, a fifth electrode 138 provided adjacent to the fourth electrode 137, and the first and third electrodes 134.
  • the switching element 130 has a cover member 139 that protects the inside on the insulating substrate 131.
  • the insulating substrate 131 is formed in a rectangular shape by an insulating member such as alumina, glass ceramics, mullite, zirconia.
  • the insulating substrate 131 may be made of a material used for a printed wiring board such as a glass epoxy board or a phenol board.
  • the first and second heating elements 132 and 133 are conductive members that generate heat when energized, like the heating element 93 described above, and can be formed in the same manner as the heating element 93.
  • the first and second fuse elements 1A and 1B have the same configuration as the fuse element 1 described above.
  • first and second heating elements 132 and 133 are covered with the insulating member 140 on the insulating substrate 131.
  • First and third electrodes 134 and 136 are formed on the insulating member 140 covering the first heating element 132, and the second and second electrodes are formed on the insulating member 140 covering the second heating element 133.
  • 4, fifth electrodes 135, 137, 138 are formed.
  • the first electrode 134 is formed adjacent to the second electrode 135 on one side and is insulated.
  • a third electrode 136 is formed on the other side of the first electrode 134.
  • the first electrode 134 and the third electrode 135 are brought into conduction when the first fuse element 1A is connected to form a current path of the switching element 130.
  • the first electrode 134 is connected to a first external connection electrode 134 a provided on the back surface 131 b of the insulating substrate 131 through a castellation that faces the side surface of the insulating substrate 131.
  • the third electrode 136 is connected to the first heating element 132 via the first heating element extraction electrode 141 provided on the insulating substrate 131 or the insulating member 140.
  • the first heating element 132 is connected to the first heating element feeding electrode 142a provided on the back surface 131b of the insulating substrate 131 through the first heating element electrode 142 and a castellation facing the side edge of the insulating substrate 131. Connected with.
  • a fourth electrode 137 is formed on the other side of the second electrode 135 opposite to the one side adjacent to the first electrode 134.
  • a fifth electrode 138 is formed on the other side of the fourth electrode 137 opposite to the one side adjacent to the second electrode 135.
  • the second electrode 135, the fourth electrode 137, and the fifth electrode 138 are connected to the second fuse element 1B.
  • the second electrode 135 is connected to a second external connection electrode 135 a provided on the back surface 131 b of the insulating substrate 131 through a castellation that faces the side surface of the insulating substrate 131.
  • the fourth electrode 137 is connected to the second heating element 133 through the second heating element extraction electrode 143 provided on the insulating substrate 131 or the insulating member 140.
  • the second heating element 133 is connected to the second heating element feeding electrode 144a provided on the back surface 131b of the insulating substrate 131 through the second heating element electrode 144 and a castellation facing the side edge of the insulating substrate 131. Connected with.
  • the fifth electrode 138 is connected to a fifth external connection electrode 138 a provided on the back surface of the insulating substrate 131 through a castellation facing the side surface of the insulating substrate 131.
  • the switching element 130 is connected to the first fuse element 1A from the first electrode 134 to the third electrode 136, and from the second electrode 135 to the fifth electrode 138 through the fourth electrode 137.
  • the second fuse element 1B is connected.
  • the first and second fuse elements 1A and 1B are excellent in mountability due to the refractory metal layer 2 and thus improved in mountability, and can be connected to solder or the like. After being mounted on the first to fifth electrodes 134 to 138 via the material 145, they can be easily connected by reflow soldering or the like.
  • the fuse elements 1A and 1B are formed on the first to fifth electrodes 134 to 138 using the first low melting point metal layer 3 or the second low melting point metal layer 4 provided as the lowermost layer as a connecting material. You may connect to.
  • the switching element 130 includes a fuse element 1 for preventing oxidation of the refractory metal layer 2 or the first and second low melting point metal layers 3, 4, removing oxide during fusing, and improving solder fluidity.
  • a flux may be coated on the front surface or the back surface.
  • a flux sheet 146 may be disposed on the entire outermost layer on the fuse elements 1A and 1B. Similar to the flux sheet 87, the flux sheet 146 is obtained by impregnating and holding a fluid or semi-fluid flux in a sheet-like support. For example, a nonwoven fabric or a mesh-like cloth is impregnated with the flux. Is.
  • the flux sheet 146 preferably has an area larger than the surface area of the fuse elements 1A and 1B. Thereby, even when the fuse elements 1A and 1B are completely covered with the flux sheet 146 and the volume is expanded by melting, it is possible to surely realize the quick fusing by removing the oxide by the flux and improving the wettability. it can.
  • the flux sheet 146 By disposing the flux sheet 146, the flux can be held over the entire surface of the fuse elements 1A and 1B in the heat treatment process when the fuse element 1 is mounted or when the switching element 130 is mounted.
  • the first and second low melting point metal layers 3 and 4 (for example, solder) are improved in wettability, and oxides are removed while the first and second low melting point metals are dissolved, thereby obtaining a high melting point.
  • the fast fusing property can be improved by using an erosion action on a metal (for example, Ag).
  • an anti-oxidation film such as Pb-free solder containing Sn as a main component is formed on the surface of the outermost refractory metal layer 2 by arranging the flux sheet 146, the oxidation of the anti-oxidation film The material can be removed, the refractory metal layer 2 can be effectively prevented from being oxidized, and the fast fusing property can be maintained and improved.
  • the switching element 130 instead of the flux sheet 146, the switching element 130, as shown in FIG. 27, after applying the flux 148a to the outermost layer of the fuse element 1, arrange a non-woven fabric or mesh-like fabric on the flux 148a, A flux 148a may be impregnated.
  • the switching element 130 may apply a flux 148b in which a fibrous material is mixed to the entire outermost layer of the fuse elements 1A and 1B, instead of the flux sheet. Viscosity of the flux 148b is increased by mixing the fibrous material, and it is difficult for the flux 148b to flow even in a high-temperature environment, so that the oxide can be removed and the wettability can be improved over the entire surface of the fuse element 1.
  • a fibrous material mixed with the flux 148b for example, a fiber having insulating properties and heat resistance, such as a nonwoven fabric fiber and a glass fiber, is preferably used.
  • the switching element 130 may mount the flux sheet 146 over the fuse element 1A and the fuse element 1B, or may be mounted on each of the fuse element 1A and the fuse element 1B.
  • the switching element 130 may be mounted with a nonwoven fabric or a mesh-shaped fabric over the fuse element 1A and the fuse element 1B after the flux 148a is applied to each of the fuse element 1A and the fuse element 1B.
  • a mesh-shaped cloth may be mounted on each of the fuse element 1A and the fuse element 1B.
  • the switching element 130 may apply a flux 148b in which the fibrous material is mixed and the viscosity is increased to each of the fuse element 1A and the fuse element 1B.
  • the first to fifth electrodes 134, 135, 136, 137, and 138 can be formed using a general electrode material such as Cu or Ag, but at least the first and second electrodes 134, A coating 149 such as Ni / Au plating, Ni / Pd plating, or Ni / Pd / Au plating is preferably formed on the surface of 135 by a known plating process. Thereby, the oxidation of the first and second electrodes 134 and 135 can be prevented, and the molten conductor can be reliably held. Further, when the switching element 130 is reflow-mounted, the solder for connecting the first and second fuse elements 1A and 1B or the low melting point metal forming the outer layer of the first and second fuse elements 1A and 1B is melted. This can prevent the first and second electrodes 134 and 135 from being eroded (soldered).
  • first to fifth electrodes 134 to 138 include an outflow prevention portion made of an insulating material such as glass for preventing the molten conductor of the fuse elements 1A and 1B and the connection material 145 of the fuse elements 1A and 1B from flowing out. 147 is formed.
  • the switching element 130 has a cover member 139 for protecting the inside and preventing the molten fuse elements 1A and 1B from scattering on the surface 131a of the insulating substrate 131 provided with the fuse elements 1A and 1B.
  • the cover member 139 can be formed of an insulating member such as various engineering plastics and ceramics.
  • the fuse elements 1 ⁇ / b> A and 1 ⁇ / b> B are covered with the cover member 139, so that the molten metal is captured by the cover member 139 and can be prevented from being scattered to the surroundings.
  • the cover member 139 has a protrusion 139b extending from the top surface 139a toward the insulating substrate 131 at least to the side surface of the flux sheet 146.
  • the cover member 139 can prevent displacement of the flux sheet 146 because the side surface of the flux sheet 146 is restricted by the protrusions 139b.
  • the protrusion 139b has a size that holds a predetermined clearance rather than the size of the flux sheet 146, and is provided corresponding to the position where the flux sheet 146 should be held.
  • the protrusion part 139b is good also as a wall surface which wraps around the side surface of the flux sheet
  • the cover member 139 is configured to have a predetermined interval between the flux sheet 146 and the top surface 139a. This is because when the fuse elements 1A and 1B are melted, a clearance is required for the melted fuse elements 1A and 1B to push up the flux sheet 146.
  • the cover member 139 has a height of the internal space of the cover member 139 (a height up to the top surface 139a), the height of the melted fuse elements 1A and 1B on the surface 131a of the insulating substrate 131, and the flux sheet 146. It is comprised so that it may become larger than the sum of thickness.
  • the switching element 130 as described above has a circuit configuration as shown in FIG. That is, in the switching element 130, the first electrode 134 and the second electrode 135 are insulated in the normal state, and the first and second fuse elements 1A, 1A, When 1B is melted, the switch 150 is configured to be short-circuited through the molten conductor.
  • the first external connection electrode 134a and the second external connection electrode 135a constitute both terminals of the switch 150.
  • the first fuse element 1A is connected to the first heating element 132 via the third electrode 136 and the first heating element lead electrode 141.
  • the second fuse element 1B is connected to the second heating element 133 through the fourth electrode 137 and the second heating element extraction electrode 143, and further, the second heating element 1B is connected to the second heating element electrode 144 through the second heating element electrode 144.
  • the body power supply electrode 144a is connected. That is, the second electrode 135, the fourth electrode 137, and the fifth electrode 138 to which the second fuse element 1B and the second fuse element 1B are connected are the second fuse element 130 before the switching element 130 is operated.
  • the second electrode 135 and the fifth electrode 138 are brought into conduction through the element 1B, and the second fuse element 1B is blown so that the second electrode 135 and the fifth electrode 138 are connected. It functions as a protective element for blocking.
  • the switching element 130 When the switching element 130 is energized to the second heating element 133 from the second heating element feeding electrode 144a, the second fuse element 1B is generated by the heat generation of the second heating element 133 as shown in FIG. Melts and aggregates on the second, fourth, and fifth electrodes 135, 137, and 138, respectively. As a result, the current path extending between the second electrode 135 and the fifth electrode 138 connected via the second fuse element 1B is interrupted. Further, when the switching element 130 is energized to the first heating element 132 from the first heating element power supply electrode 142a, the first fuse element 1A is melted by the heat generated by the first heating element 132, and the first, Aggregates on the third electrodes 134 and 136, respectively.
  • the switching element 130 is a molten conductor of the first and second fuse elements 1A and 1B aggregated into the first electrode 134 and the second electrode 135. Are coupled to short-circuit the insulated first electrode 134 and second electrode 135. That is, the switching element 130 can short-circuit the switch 150 to switch the current path between the second and fifth electrodes 135 and 138 to the current path between the first and second electrodes 134 and 135 (FIG. 32). ).
  • the fuse elements 1A and 1B have the first low melting point metal layer 3 having a melting point lower than that of the refractory metal layer 2 and the second melting point lower than that of the first low melting point metal layer 3. Since the low melting point metal layer 4 is laminated, the melting of the second low melting point metal layer 4 is started from the melting point of the second low melting point metal layer 4 by the heat generation of the first and second heating elements 132 and 133, and the high melting point metal layer 2 is eroded. Begin to. Therefore, the fuse elements 1A and 1B use the erosion action of the refractory metal layer 2 by the first and second low melting point metal layers 3 and 4, so that the refractory metal layer 2 is at a temperature lower than the melting temperature. It is melted and can be blown quickly.
  • the energization of the first heating element 132 is stopped because the first fuse element 1A is melted and the first and third electrodes 134 and 136 are cut off, and the second heating element 133 is turned off. Since the second fuse element 1B is melted, the current between the second and fourth electrodes 135 and 137 and the fourth and fifth electrodes 137 and 138 are interrupted.
  • the switching element 130 it is preferable that the second fuse element 1B is melted prior to the first fuse element 1A. Since the first heating element 132 and the second heating element 133 generate heat separately, the switching element 130 causes the second heating element 133 to generate heat first as the energization timing, and then the first heating element 132 and the second heating element 133 generate heat. By causing the heat generating element 132 to generate heat, the second fuse element 1B is melted prior to the first fuse element 1A as shown in FIG. 30, and the first and first fuses are securely connected as shown in FIG.
  • the first and second electrodes 134 and 135 can be short-circuited by aggregating and bonding the molten conductors of the first and second fuse elements 1A and 1B on the two electrodes 134 and 135.
  • the switching element 130 forms the second fuse element 1B narrower than the first fuse element 1A, thereby fusing the second fuse element 1B before the first fuse element 1A. You may do it.
  • the fusing time can be shortened, so that the second fuse element 1B can be melted prior to the first fuse element 1A.
  • the area of the first electrode 134 is preferably larger than that of the third electrode 136, and the area of the second electrode 135 is preferably larger than those of the fourth and fifth electrodes 137 and 138. . Since the holding amount of the molten conductor increases in proportion to the electrode area, the areas of the first and second electrodes 134 and 135 are formed wider than the third, fourth, and fifth electrodes 136, 137, and 138. As a result, more molten conductors can be agglomerated on the first and second electrodes 134 and 135, and the first and second electrodes 134 and 135 can be reliably short-circuited.
  • the switching element 130 does not necessarily need to cover the first and second heating elements 132 and 133 with the insulating member 140, and the first and second heating elements 132 and 133 are installed inside the insulating substrate 131. May be.
  • the first and second heating elements 132 and 133 can be heated in the same manner as when the insulating member 140 such as a glass layer is interposed. .
  • the first and second heating elements 132 and 133 are installed on the back surface of the insulating substrate 131 opposite to the formation surface of the first to fifth electrodes 134, 135, 136, 137, and 138. Also good.
  • the first and second heating elements 132 and 133 can be formed by a simpler process than forming in the insulating substrate 131.
  • the insulating member 140 is formed on the first and second heating elements 132 and 133 in terms of protecting the resistor and ensuring insulation during mounting.
  • the switching element 130 includes first and second heating elements 132 and 133 installed on the formation surface of the first to fifth electrodes 134, 135, 136, 137, and 138 of the insulating substrate 131, and The first to fifth electrodes 134 to 138 may be provided together.
  • the first and second heating elements 132 and 133 can be formed by a simpler process than that in the insulating substrate 131. Also in this case, it is desirable that the insulating member 140 is formed on the first and second heating elements 132 and 133.

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Combustion & Propulsion (AREA)
  • Fuses (AREA)
  • Thermistors And Varistors (AREA)
PCT/JP2015/081030 2014-11-11 2015-11-04 ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子 WO2016076173A1 (ja)

Priority Applications (2)

Application Number Priority Date Filing Date Title
KR1020177011371A KR101950619B1 (ko) 2014-11-11 2015-11-04 퓨즈 요소, 퓨즈 소자, 보호 소자, 단락 소자, 전환 소자
CN201580059056.7A CN107735849B (zh) 2014-11-11 2015-11-04 熔丝单元、熔丝元件、保护元件、短路元件、切换元件

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2014-229360 2014-11-11
JP2014229360A JP6436729B2 (ja) 2014-11-11 2014-11-11 ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子

Publications (1)

Publication Number Publication Date
WO2016076173A1 true WO2016076173A1 (ja) 2016-05-19

Family

ID=55954263

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2015/081030 WO2016076173A1 (ja) 2014-11-11 2015-11-04 ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子

Country Status (5)

Country Link
JP (1) JP6436729B2 (zh)
KR (1) KR101950619B1 (zh)
CN (1) CN107735849B (zh)
TW (1) TWI697022B (zh)
WO (1) WO2016076173A1 (zh)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP6811590B2 (ja) * 2016-11-10 2021-01-13 デクセリアルズ株式会社 保護素子
WO2018100984A1 (ja) * 2016-11-29 2018-06-07 デクセリアルズ株式会社 保護素子
JP7433783B2 (ja) * 2019-06-19 2024-02-20 デクセリアルズ株式会社 ヒューズエレメント、ヒューズ素子及び保護素子
JP2024049240A (ja) * 2022-09-28 2024-04-09 デクセリアルズ株式会社 保護素子及び保護素子の製造方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5539168A (en) * 1978-09-13 1980-03-18 Mitsubishi Electric Corp Fuse and method of fabricating same
JPH03205731A (ja) * 1990-01-01 1991-09-09 Uchihashi Estec Co Ltd 温度ヒユーズエレメントの製造方法
WO2013146889A1 (ja) * 2012-03-29 2013-10-03 デクセリアルズ株式会社 保護素子
JP2014179309A (ja) * 2013-02-12 2014-09-25 Dexerials Corp 短絡素子、およびこれを用いた回路
WO2014157585A1 (ja) * 2013-03-28 2014-10-02 デクセリアルズ株式会社 ヒューズエレメント、及びヒューズ素子

Family Cites Families (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US4320374A (en) * 1979-03-21 1982-03-16 Kearney-National (Canada) Limited Electric fuses employing composite aluminum and cadmium fuse elements
JP4632358B2 (ja) * 2005-06-08 2011-02-16 三菱マテリアル株式会社 チップ型ヒューズ
JP5072796B2 (ja) * 2008-05-23 2012-11-14 ソニーケミカル&インフォメーションデバイス株式会社 保護素子及び二次電池装置
JP5130232B2 (ja) * 2009-01-21 2013-01-30 デクセリアルズ株式会社 保護素子
JP5130233B2 (ja) * 2009-01-21 2013-01-30 デクセリアルズ株式会社 保護素子
JP5306139B2 (ja) 2009-10-08 2013-10-02 北陸電気工業株式会社 チップヒューズ
JP6249600B2 (ja) * 2012-03-29 2017-12-20 デクセリアルズ株式会社 保護素子
JP6081096B2 (ja) * 2012-08-01 2017-02-15 デクセリアルズ株式会社 保護素子及びバッテリパック
WO2014123139A1 (ja) * 2013-02-05 2014-08-14 デクセリアルズ株式会社 短絡素子、およびこれを用いた回路

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5539168A (en) * 1978-09-13 1980-03-18 Mitsubishi Electric Corp Fuse and method of fabricating same
JPH03205731A (ja) * 1990-01-01 1991-09-09 Uchihashi Estec Co Ltd 温度ヒユーズエレメントの製造方法
WO2013146889A1 (ja) * 2012-03-29 2013-10-03 デクセリアルズ株式会社 保護素子
JP2014179309A (ja) * 2013-02-12 2014-09-25 Dexerials Corp 短絡素子、およびこれを用いた回路
WO2014157585A1 (ja) * 2013-03-28 2014-10-02 デクセリアルズ株式会社 ヒューズエレメント、及びヒューズ素子

Also Published As

Publication number Publication date
CN107735849B (zh) 2020-05-05
JP6436729B2 (ja) 2018-12-12
TWI697022B (zh) 2020-06-21
KR101950619B1 (ko) 2019-02-20
KR20170059004A (ko) 2017-05-29
CN107735849A (zh) 2018-02-23
JP2016095899A (ja) 2016-05-26
TW201630022A (zh) 2016-08-16

Similar Documents

Publication Publication Date Title
JP6420053B2 (ja) ヒューズエレメント、及びヒューズ素子
JP6483987B2 (ja) ヒューズエレメント、ヒューズ素子、及び発熱体内蔵ヒューズ素子
KR102523229B1 (ko) 보호 소자 및 실장체
JP6249600B2 (ja) 保護素子
TWI714595B (zh) 熔絲單元、熔絲元件、保護元件、短路元件、切換元件
JP2008311161A (ja) 保護素子
JP6576618B2 (ja) 保護素子
KR102135832B1 (ko) 퓨즈 엘리먼트, 퓨즈 소자, 보호 소자
WO2013146889A1 (ja) 保護素子
WO2016076173A1 (ja) ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子
KR102442404B1 (ko) 퓨즈 소자
JP2010165685A (ja) 保護素子及びバッテリーパック
JP2017022009A (ja) 保護素子、ヒューズ素子
WO2016076172A1 (ja) フラックスシート、フラックス、ヒューズエレメント、ヒューズ素子、保護素子、短絡素子及び切替素子
JP6577118B2 (ja) ヒューズエレメント、ヒューズ素子、保護素子、短絡素子、切替素子
JP2016170892A (ja) ヒューズエレメント及びヒューズ素子
JP6429591B2 (ja) 保護素子
JP2014044955A (ja) 保護素子及びバッテリーパック
JP2012059719A (ja) 保護素子及びバッテリーパック
JP2018018835A (ja) 保護素子、ヒューズ素子

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 15858876

Country of ref document: EP

Kind code of ref document: A1

DPE1 Request for preliminary examination filed after expiration of 19th month from priority date (pct application filed from 20040101)
ENP Entry into the national phase

Ref document number: 20177011371

Country of ref document: KR

Kind code of ref document: A

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 15858876

Country of ref document: EP

Kind code of ref document: A1