WO2015111751A1 - 採光フィルム、採光具および採光フィルムの製造方法 - Google Patents

採光フィルム、採光具および採光フィルムの製造方法 Download PDF

Info

Publication number
WO2015111751A1
WO2015111751A1 PCT/JP2015/052115 JP2015052115W WO2015111751A1 WO 2015111751 A1 WO2015111751 A1 WO 2015111751A1 JP 2015052115 W JP2015052115 W JP 2015052115W WO 2015111751 A1 WO2015111751 A1 WO 2015111751A1
Authority
WO
WIPO (PCT)
Prior art keywords
filling
filled
daylighting film
base portion
daylighting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
PCT/JP2015/052115
Other languages
English (en)
French (fr)
Japanese (ja)
Inventor
康弘 大木
聖 三塚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dai Nippon Printing Co Ltd
Original Assignee
Dai Nippon Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dai Nippon Printing Co Ltd filed Critical Dai Nippon Printing Co Ltd
Publication of WO2015111751A1 publication Critical patent/WO2015111751A1/ja
Anticipated expiration legal-status Critical
Ceased legal-status Critical Current

Links

Images

Classifications

    • B—PERFORMING OPERATIONS; TRANSPORTING
    • B32—LAYERED PRODUCTS
    • B32B—LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
    • B32B17/00—Layered products essentially comprising sheet glass, or glass, slag, or like fibres
    • B32B17/06—Layered products essentially comprising sheet glass, or glass, slag, or like fibres comprising glass as the main or only constituent of a layer, next to another layer of a specific material
    • B32B17/10—Layered products essentially comprising sheet glass, or glass, slag, or like fibres comprising glass as the main or only constituent of a layer, next to another layer of a specific material of synthetic resin
    • B32B17/10005—Layered products essentially comprising sheet glass, or glass, slag, or like fibres comprising glass as the main or only constituent of a layer, next to another layer of a specific material of synthetic resin laminated safety glass or glazing
    • B32B17/10165—Functional features of the laminated safety glass or glazing
    • B32B17/10541—Functional features of the laminated safety glass or glazing comprising a light source or a light guide
    • E—FIXED CONSTRUCTIONS
    • E06—DOORS, WINDOWS, SHUTTERS, OR ROLLER BLINDS IN GENERAL; LADDERS
    • E06B—FIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES OR LIKE ENCLOSURES IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES
    • E06B9/00—Screening or protective devices for wall or similar openings, with or without operating or securing mechanisms; Closures of similar construction
    • E06B9/24—Screens or other constructions affording protection against light, especially against sunshine; Similar screens for privacy or appearance; Slat blinds
    • G—PHYSICS
    • G02—OPTICS
    • G02B—OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
    • G02B5/00—Optical elements other than lenses
    • G02B5/02—Diffusing elements; Afocal elements
    • G02B5/0205—Diffusing elements; Afocal elements characterised by the diffusing properties
    • G02B5/021—Diffusing elements; Afocal elements characterised by the diffusing properties the diffusion taking place at the element's surface, e.g. by means of surface roughening or microprismatic structures
    • G02B5/0231—Diffusing elements; Afocal elements characterised by the diffusing properties the diffusion taking place at the element's surface, e.g. by means of surface roughening or microprismatic structures the surface having microprismatic or micropyramidal shape
    • E—FIXED CONSTRUCTIONS
    • E06—DOORS, WINDOWS, SHUTTERS, OR ROLLER BLINDS IN GENERAL; LADDERS
    • E06B—FIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES OR LIKE ENCLOSURES IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES
    • E06B9/00—Screening or protective devices for wall or similar openings, with or without operating or securing mechanisms; Closures of similar construction
    • E06B9/24—Screens or other constructions affording protection against light, especially against sunshine; Similar screens for privacy or appearance; Slat blinds
    • E06B2009/2417—Light path control; means to control reflection

Definitions

  • the present invention relates to a daylighting film, a daylighting tool, and a method for manufacturing a daylighting film.
  • Light control sheet that improves daylighting efficiency by deflecting outside light incident on the window toward the indoor ceiling as part of efforts to reduce carbon dioxide emissions and reduce power consumption by reducing the intensity of indoor lighting has been proposed.
  • a light control sheet having a structure in which transmissive portions and light-shielding portions are alternately arranged is pasted on, for example, a window glass.
  • a technique for reducing the uptake of sunlight and increasing the uptake of sunlight in winter is disclosed.
  • a base portion having a plurality of grooves and a plurality of filling portions filled in these grooves are provided.
  • the external light incident on the daylighting film is guided toward the indoor ceiling or wall using the difference in refractive index between the base portion and the filling portion.
  • a curable resin that is hardened by an electron beam or heat is often used.
  • the curable resin often shrinks when cured in the groove, and a cavity is formed around the opening of the groove due to a process problem during filling. If this cavity is left as it is, incident light is reflected at the interface between the cavity and the filling portion due to the difference in refractive index between the air in the cavity and the filling portion in the groove. There is a possibility that the ratio of incident light may be reduced. In addition, the refractive angle of incident light changes due to the difference in refractive index between the cavity and the filling portion, and the light may travel in an unintended direction.
  • the present invention has been made to solve the above-described problems, and an object thereof is to provide a daylighting film, a daylighting tool, and a daylighting film manufacturing method capable of improving daylighting efficiency.
  • a base portion having a plurality of grooves that are spaced apart along one surface; A plurality of filling portions filled in the plurality of grooves with a filling material having a refractive index different from that of the base portion; There is provided a daylighting film including a cavity filling portion in which one or more recesses formed by the end surface shape on the one surface side of the plurality of filling portions are filled with a predetermined filling material.
  • the predetermined filling material filled in the cavity filling portion may have the same refractive index as the plurality of filling portions.
  • the predetermined filling material filled in the cavity filling portion may be a material filled in the plurality of filling portions.
  • the predetermined filling material filled in the cavity filling portion may be a material for forming the base portion.
  • the refractive index difference between the base portion and the plurality of filling portions may be 0.1 or more.
  • the cavity filling portion may be filled in the one or more recesses so as to have a height equal to or higher than an opening surface of the one or more recesses.
  • a lighting tool may be provided that includes a transparent base material disposed on the surface of the adhesive layer opposite to the cavity filling portion via the adhesive layer.
  • a plurality of filling portions are formed by filling a filling material having a refractive index different from that of a base portion having a plurality of grooves spaced apart along one surface into the plurality of grooves. Applying a predetermined filling material around and within one or more recesses formed by the end face shape on the one surface side of Scraping off the excess predetermined filling material on the one surface side of the base portion; The step of curing the predetermined filling material filled in the one or more recesses may be performed at least once until the recesses are filled and the filling material is filled in the recesses. .
  • the present invention it is possible to improve the daylighting efficiency even if the concave portions are formed in the plurality of filling portions that are arranged separately in the base portion.
  • FIG. 4 is a view showing a cross-sectional structure different from those shown in FIGS.
  • FIGS. The figure which shows the cross-section of the laminated glass by one Embodiment.
  • the process flowchart which shows an example of the manufacturing process of this embodiment.
  • FIG. 1 is a diagram showing a cross-sectional structure of a daylighting film according to an embodiment.
  • the daylighting film 1 of FIG. 1 is used by being laminated on, for example, a window or a daylighting tool, or incorporated in a window or daylighting tool.
  • a daylighting film 1 has a base portion 3 having a plurality of grooves 2 that are spaced apart along one surface 1 a and a refractive index different from that of the base portion 3.
  • a plurality of filling portions 4 filled with a filling material in the plurality of grooves 2 are provided.
  • the base portion 3 has a higher refractive index than the plurality of filling portions 4. Thereby, the light incident on the base portion 3 from the outside is reflected at the interface with the filling portion 4 and is bounced upward obliquely.
  • the difference in refractive index between the base portion 3 and the plurality of filling portions 4 is 0.1 or more.
  • the refractive index of the base portion 3 is set to about 1.6
  • the refractive index of the filling portion 4 is set to about 1.4.
  • At least one concave portion 4a is formed on one surface 1a side of the plurality of filling portions 4 according to the end face shape of each filling portion 4.
  • the recess 4 a is a recess formed on the one surface 1 a side of the filling portion 4.
  • the concave portion 4a is formed by being scraped too much at the time of filling, and is inevitably formed by curing shrinkage when the filling material filled in each filling portion 4 is cured.
  • the recessed part 4a is not necessarily formed in all the filling parts 4, and may be formed only in the one part filling part 4 by manufacturing dispersion
  • the daylighting film 1 further includes a cavity filling portion 5 filled with a predetermined filling material in the recess 4a.
  • the cavity filling portion 5 is filled in the recess 4a so as to have a height equal to or higher than the height of the opening surface of the recess 4a.
  • the recess 4a is filled with the cavity filling portion 5 so that the recesses due to the recess 4a are completely eliminated from the one surface 1a of the base portion 3.
  • the reason why the recesses 4a are formed in the filling parts 4 is that the filling material shrinks when cured, This is because the filling material may not be properly filled in the recess 4a due to manufacturing reasons.
  • the top of the cavity filling portion 5 is formed so as to be flush with the one surface 1a of the base portion 3 or protrude from the one surface 1a.
  • a fluid curable resin is applied to the one surface 1a side of the base portion 3 and then cured.
  • a cured resin layer may be formed on almost the entire area of one surface 1a of the base portion 3. Even in the case of FIG. 2, a part of the cured resin layer is filled in the recess 4 a to form the above-described cavity filling portion 5.
  • the filling portion 1 and 2 are formed of the same material as the filling portion 4. Thereby, a refractive index difference does not occur at the interface between the cavity filling portion 5 and the filling portion 4, and incident light from the outside is not reflected at this interface, and the ratio of light taken into the daylighting film 1 may be reduced. Disappear. In addition, light can be prevented from being refracted at this interface, and the risk of light traveling in an unintended direction can be avoided. Therefore, the lighting efficiency can be improved by making the cavity filling part 5 the same material as the filling part 4.
  • the cavity filling portion 5 is not necessarily formed of the same material as the filling portion 4.
  • the cavity filling portion 5 may be formed of the same material as the base portion 3.
  • An interface due to a difference in refractive index occurs between the filling portion 5 and the filling portion 4.
  • the refractive index difference between air and the base portion 3 or the filling portion 4 is as large as about 0.5, whereas the refractive index difference between the base portion 3 and the filling portion 4 is about 0.1 to 0.2. Since it is relatively small, there is less possibility that incident light is reflected at this interface, and the efficiency of taking light into the daylighting film 1 is improved as compared with the case where the recess 4a is not filled.
  • the cavity filling portion 5 is formed by filling the concave portion 4a with the same material as the base portion 3, a fluid curable resin is applied to one surface 1a side of the base portion 3 and then cured. Therefore, the cured resin layer may be formed not only in the recess 4a but also in almost the entire area of the one surface 1a of the base 3 as shown in FIG. Even in this case, a part of the cured resin layer is filled in the recess 4a, and the cavity filling portion 5 described above is formed.
  • FIG. 5 is a diagram illustrating an example of a cross-sectional structure of the laminated glass 10.
  • adhesive layers 6 are disposed on both surfaces of the daylighting film 1, and a transparent substrate 7 such as glass is adhered from both surfaces via the adhesive layers 6.
  • a transparent substrate 7 such as glass is adhered from both surfaces via the adhesive layers 6.
  • FIG. 1 and FIG. 3 even if the cavity filling portion 5 protrudes in one surface 1 a of the base portion 3 of the daylighting film 1, it is flattened by the adhesive layer 6.
  • the film 1 is firmly bonded to the entire surface through the adhesive layer 6.
  • the daylighting film 1 according to the present embodiment is not only used for the laminated glass 10. For example, it may be bonded to only one side of the transparent substrate 7 such as glass via an adhesive. Moreover, the lighting film 1 by this embodiment may be adhere
  • the constituent material and manufacturing process of the daylighting film 1 according to the present embodiment will be described.
  • the material of the base portion 3 for example, a material obtained by mixing and homogenizing a photocurable prepolymer, a reactive dilution monomer, a mold release agent, and a photopolymerization initiator is used.
  • a base material (not shown) is bonded to the base portion 3, for example, a PET (polyethylene terephthalate) film is used as the base material.
  • a curable resin such as a thermosetting resin or an electron beam curable resin may be used instead of the ultraviolet curable resin.
  • a mold roll is used to form the groove 2 as shown in FIG.
  • the surface of the mold roll is cut with a cutting tool in accordance with the shape of the groove 2 to form a plurality of convex portions corresponding to the shape of each groove 2.
  • the composition of the base portion 3 is filled between the mold roll and the nip roll formed with the convex portions and pressurized with both rolls.
  • the composition of the base portion 3 is cured by irradiating ultraviolet rays with a high-pressure mercury lamp.
  • the base part 3 is formed. Thereafter, the base portion 3 is released from the mold roller by the peeling roller, and an intermediate member including the base portion 3 is produced.
  • an ultraviolet curable resin such as a photocurable prepolymer, a reactive dilution monomer, a light scattering material, and a photopolymerization initiator are mixed and uniform. Is used.
  • a thermosetting resin or an electron beam curable resin may be used instead of the ultraviolet curable resin.
  • the base part 3 and the filling part 4 have different refractive indexes.
  • Both the base part 3 and the filling part 4 are made of a curable resin such as a thermosetting resin, an ultraviolet curable resin and an electron beam curable resin, but the curable resin material and the types of additives contained therein By changing etc., the base part 3 and the filling part 4 can have a refractive index difference.
  • the filler used as the material of the filling unit 4 is supplied onto the intermediate member, the filler is filled into the groove 2, and the excess filler is scraped off. Then, the filling part 4 is formed by irradiating with an ultraviolet ray from a high pressure mercury lamp and curing. As described above, the filling portion 4 is formed with the concave portion 4a by scraping and curing the filling material. Therefore, in this embodiment, the process of forming the cavity filling portion 5 in the recess 4a is performed in the manufacturing process shown in FIG.
  • a predetermined filling material is applied around the recess 4a (step S1).
  • the predetermined filling material is preferably the same material as the filling portion 4 as shown in FIGS. 1 and 2, but may be the same material as the base portion 3 as shown in FIGS. 3 and 4.
  • the predetermined filling material may be a material different from the material of the filling portion 4 and the base portion 3 as long as the refractive index difference with the filling portion 4 is about 0.1.
  • step S2 a squeegee process is performed so that the predetermined filling material is filled in the concave portion 4a, and excess filling material on the one surface 1a side of the base portion 3 is scraped off.
  • step S3 the predetermined filling material filled in the recess 4a is cured by heat, ultraviolet light, electron beam or the like.
  • the concave portion 4a is not completely eliminated only by performing the processing of steps S1 to S3 once. Therefore, the processes in steps S1 to S3 are repeated at least twice to form the cavity filling portion 5 in the recess 4a (step S4). Thereafter, the adhesive layer 6 is formed as necessary.
  • the composition of the adhesive layer 6 is, for example, one or more of a thermoplastic resin such as polyvinyl acetal resin, ethylene vinyl acetate copolymer resin, ethylene acrylic copolymer resin, polyurethane resin and polyvinyl alcohol resin, It may be used by mixing with additives such as an antioxidant and an ultraviolet shielding agent, or may be formed by mixing an acrylic resin adhesive, a crosslinking agent, and a diluent.
  • the composition of the adhesive layer 6 is made into a sheet or film and placed between the daylighting film 1 and the transparent substrate, and after applying pressure to extrude air, it is heated and integrated with the daylighting film 1. If it is liquid, it is applied to the release film and dried, and then attached to the daylighting film 1.
  • the cavity filling portion 5 is formed by filling the recess 4 a generated when the filling portion 4 is formed by filling the groove 2 of the base portion 3 with the predetermined filling material. Therefore, the refractive index difference at the interface between the cavity filling part 5 and the filling part 4 can be reduced, and the proportion of light reflected at the interface can be reduced as compared with the case without the cavity filling part 5. For this reason, the efficiency of taking light into the daylighting film 1 can be improved.
  • the material of the cavity filling portion 5 is the same as that of the filling portion 4, the interface between the cavity filling portion 5 and the filling portion 4 is substantially eliminated, and there is no ideal recess 4 a between the base portions 3.
  • the filling part 4 can be formed and the daylighting effect of the daylighting film 1 can be further improved.

Landscapes

  • Physics & Mathematics (AREA)
  • Engineering & Computer Science (AREA)
  • Structural Engineering (AREA)
  • General Physics & Mathematics (AREA)
  • Optics & Photonics (AREA)
  • Architecture (AREA)
  • Civil Engineering (AREA)
  • Optical Elements Other Than Lenses (AREA)
PCT/JP2015/052115 2014-01-27 2015-01-27 採光フィルム、採光具および採光フィルムの製造方法 Ceased WO2015111751A1 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2014012716A JP5910644B2 (ja) 2014-01-27 2014-01-27 採光フィルムおよび採光フィルムの製造方法
JP2014-012716 2014-01-27

Publications (1)

Publication Number Publication Date
WO2015111751A1 true WO2015111751A1 (ja) 2015-07-30

Family

ID=53681547

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2015/052115 Ceased WO2015111751A1 (ja) 2014-01-27 2015-01-27 採光フィルム、採光具および採光フィルムの製造方法

Country Status (2)

Country Link
JP (1) JP5910644B2 (enExample)
WO (1) WO2015111751A1 (enExample)

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2010259406A (ja) * 2009-05-11 2010-11-18 Dainippon Printing Co Ltd 光制御シート及び建物
WO2011004772A1 (ja) * 2009-07-06 2011-01-13 大日本印刷株式会社 光学シートの製造方法、光学シート、及び映像表示装置
JP2012112995A (ja) * 2010-11-19 2012-06-14 Dainippon Printing Co Ltd 光学シート、及び映像表示装置
JP2013218261A (ja) * 2012-03-14 2013-10-24 Dainippon Printing Co Ltd 熱線制御フィルム

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009069416A (ja) * 2007-09-12 2009-04-02 Dainippon Printing Co Ltd 光学シート、表示装置及び光学シートの製造方法
JP2009080198A (ja) * 2007-09-25 2009-04-16 Dainippon Printing Co Ltd 光学シート、及び該光学シートを備える表示装置

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2010259406A (ja) * 2009-05-11 2010-11-18 Dainippon Printing Co Ltd 光制御シート及び建物
WO2011004772A1 (ja) * 2009-07-06 2011-01-13 大日本印刷株式会社 光学シートの製造方法、光学シート、及び映像表示装置
JP2012112995A (ja) * 2010-11-19 2012-06-14 Dainippon Printing Co Ltd 光学シート、及び映像表示装置
JP2013218261A (ja) * 2012-03-14 2013-10-24 Dainippon Printing Co Ltd 熱線制御フィルム

Also Published As

Publication number Publication date
JP2015141246A (ja) 2015-08-03
JP5910644B2 (ja) 2016-04-27

Similar Documents

Publication Publication Date Title
CN109804278B (zh) 用于光学器件的边缘密封剂围限和光晕减轻
KR102540565B1 (ko) 이방성 광학 필름을 이용한 도광 적층체 및 그것을 이용한 면상 광원 장치
TWI718106B (zh) 日光照明結構及其製造方法、百葉窗板組件的板條
JP2007334279A (ja) 光線方向制御素子の製造方法、光線方向制御素子,光線方向制御素子を用いた光源及び表示装置
CN104035255B (zh) 阵列基板、显示面板及制作方法
JP2011034060A (ja) 光学シートの製造方法、光学シート、及び映像表示装置
TWI805750B (zh) 光控濾光片
JP2008309829A (ja) 光拡散シートの製造方法
JP5625961B2 (ja) 透過型曲面スクリーンの製造方法、及び表示装置の製造方法
JP6057199B2 (ja) 採光フィルム、採光具および採光フィルムの製造方法
JP5910644B2 (ja) 採光フィルムおよび採光フィルムの製造方法
JP2016066098A (ja) 採光フィルムおよび採光フィルムの製造方法
KR101363473B1 (ko) 무반사 나노구조층을 구비하는 고분자 렌즈 및 이의 제조 방법
JP2010163301A (ja) ガラス基板補修方法
JP2018004956A (ja) 光学ユニット及び光学ユニットの製造方法
WO2016190430A1 (ja) 光制御部材およびそれを用いた光制御機能付き合わせガラス
CN102879855A (zh) 导光板及其制造方法
JP2016051023A (ja) 光制御シート
JP2012027442A (ja) 光学シートの製造方法、この製造方法により製造された光学シートを備える表示装置用光学フィルタおよび表示装置
JP2009208023A (ja) パターンシートの製造方法
TWI572487B (zh) 層疊式光學楔形片之製造方法
KR102915469B1 (ko) 마스킹 효과를 통한 uv 경화 공법
JP6361953B2 (ja) ウィンドウフィルムおよび窓
JP2015151744A (ja) 採光フィルム、採光具および採光フィルムの取付方法
CN115808822B (zh) 一种dpl复合膜片及其制备方法

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 15741086

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 15741086

Country of ref document: EP

Kind code of ref document: A1