WO2005112513A1 - Dispositif électroluminescent, éclairage et affichage - Google Patents

Dispositif électroluminescent, éclairage et affichage Download PDF

Info

Publication number
WO2005112513A1
WO2005112513A1 PCT/JP2005/008878 JP2005008878W WO2005112513A1 WO 2005112513 A1 WO2005112513 A1 WO 2005112513A1 JP 2005008878 W JP2005008878 W JP 2005008878W WO 2005112513 A1 WO2005112513 A1 WO 2005112513A1
Authority
WO
WIPO (PCT)
Prior art keywords
refractive index
transparent substrate
layer
light
electrode layer
Prior art date
Application number
PCT/JP2005/008878
Other languages
English (en)
Japanese (ja)
Inventor
Yasumi Yamada
Motofumi Kashiwagi
Original Assignee
Zeon Corporation
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from JP2004147076A external-priority patent/JP2005327686A/ja
Priority claimed from JP2004147077A external-priority patent/JP2005327687A/ja
Application filed by Zeon Corporation filed Critical Zeon Corporation
Publication of WO2005112513A1 publication Critical patent/WO2005112513A1/fr

Abstract

Augmentation de l’intensité d’émission et diminution de la consommation d’énergie d’un dispositif électroluminescent sont demandés intensément et différents efforts ont été faits pour extraire de façon efficace la lumière émise de la couche émettant la lumière, mais une amélioration supplémentaire de l’efficacité de l’extraction de la lumière est encore requise. Un éclairage ou affichage nouveau ou à haute performance peut être obtenu en développant un tel dispositif. Est divulgué un dispositif électroluminescent comprenant une couche d’indice de réfraction moyen, une première couche d’électrode, une couche d’émission de lumière et une deuxième couche d’électrode formées séquentiellement dans cet ordre sur un substrat transparent. Ce dispositif électroluminescent satisfait la relation : nS < nM < nE, où nS est l’indice de réfraction du substrat transparent, nM l’indice de réfraction de la couche d’indice de réfraction moyen et nE l’indice de réfraction de la couche de première électrode. Sont également divulgués un éclairage et un affichage de haute performance employant un tel dispositif électroluminescent.
PCT/JP2005/008878 2004-05-17 2005-05-16 Dispositif électroluminescent, éclairage et affichage WO2005112513A1 (fr)

Applications Claiming Priority (4)

Application Number Priority Date Filing Date Title
JP2004-147077 2004-05-17
JP2004147076A JP2005327686A (ja) 2004-05-17 2004-05-17 エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置
JP2004-147076 2004-05-17
JP2004147077A JP2005327687A (ja) 2004-05-17 2004-05-17 エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置

Publications (1)

Publication Number Publication Date
WO2005112513A1 true WO2005112513A1 (fr) 2005-11-24

Family

ID=35394545

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2005/008878 WO2005112513A1 (fr) 2004-05-17 2005-05-16 Dispositif électroluminescent, éclairage et affichage

Country Status (1)

Country Link
WO (1) WO2005112513A1 (fr)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2008023586A1 (fr) * 2006-08-23 2008-02-28 Zeon Corporation élément d'électroluminescence, appareil d'éclairage et appareil d'affichage à cristaux liquides
JP2008117742A (ja) * 2006-11-07 2008-05-22 Micro System:Kk 円筒型有機el照明器
WO2009107226A1 (fr) * 2008-02-29 2009-09-03 有限会社マイクロシステム Illuminateur el organique cylindrique
JP2010176928A (ja) * 2009-01-27 2010-08-12 Panasonic Electric Works Co Ltd 有機el発光装置
WO2011162080A1 (fr) * 2010-06-25 2011-12-29 パナソニック電工株式会社 Elément à électroluminescence organique
JPWO2016151820A1 (ja) * 2015-03-25 2017-11-30 パイオニア株式会社 発光装置
JP2019071305A (ja) * 2019-02-18 2019-05-09 パイオニア株式会社 発光装置
JP2021015813A (ja) * 2020-11-18 2021-02-12 パイオニア株式会社 発光装置

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002122702A (ja) * 2000-10-17 2002-04-26 Matsushita Electric Ind Co Ltd 光学フィルム、及び表示素子
JP2003077680A (ja) * 2001-09-06 2003-03-14 Konica Corp 有機エレクトロルミネッセンス素子及び表示装置
JP2004079301A (ja) * 2002-08-14 2004-03-11 Fuji Photo Film Co Ltd 発光素子およびその製造方法
JP2004119211A (ja) * 2002-09-26 2004-04-15 Toyota Industries Corp El素子用透明基板及びel装置並びに液晶表示装置

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002122702A (ja) * 2000-10-17 2002-04-26 Matsushita Electric Ind Co Ltd 光学フィルム、及び表示素子
JP2003077680A (ja) * 2001-09-06 2003-03-14 Konica Corp 有機エレクトロルミネッセンス素子及び表示装置
JP2004079301A (ja) * 2002-08-14 2004-03-11 Fuji Photo Film Co Ltd 発光素子およびその製造方法
JP2004119211A (ja) * 2002-09-26 2004-04-15 Toyota Industries Corp El素子用透明基板及びel装置並びに液晶表示装置

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2008023586A1 (fr) * 2006-08-23 2008-02-28 Zeon Corporation élément d'électroluminescence, appareil d'éclairage et appareil d'affichage à cristaux liquides
JP2008117742A (ja) * 2006-11-07 2008-05-22 Micro System:Kk 円筒型有機el照明器
WO2009107226A1 (fr) * 2008-02-29 2009-09-03 有限会社マイクロシステム Illuminateur el organique cylindrique
JP2010176928A (ja) * 2009-01-27 2010-08-12 Panasonic Electric Works Co Ltd 有機el発光装置
WO2011162080A1 (fr) * 2010-06-25 2011-12-29 パナソニック電工株式会社 Elément à électroluminescence organique
JPWO2016151820A1 (ja) * 2015-03-25 2017-11-30 パイオニア株式会社 発光装置
JP2019071305A (ja) * 2019-02-18 2019-05-09 パイオニア株式会社 発光装置
JP2021015813A (ja) * 2020-11-18 2021-02-12 パイオニア株式会社 発光装置

Similar Documents

Publication Publication Date Title
KR101236574B1 (ko) 전계 발광 소자, 조명 장치, 및 표시 장치
WO2005112513A1 (fr) Dispositif électroluminescent, éclairage et affichage
KR20140088335A (ko) 유기발광 표시장치 및 그의 제조방법
US20090097273A1 (en) Light guide plate and light-emitting apparatus
EP3109902B1 (fr) Matrice noire, dispositif d&#39;affichage à écran plat et son procédé de fabrication
TWI543424B (zh) 利用梯度折射率膜於oled中控制光線之擷取及分佈
WO2021002247A1 (fr) Élément de diffusion, stratifié, ensemble d&#39;éléments de diffusion, rétroéclairage à del et dispositif d&#39;affichage
US8987767B2 (en) Light emitting device having improved light extraction efficiency
CN1499905A (zh) 显示体、显示面板及显示装置
JP2005327687A (ja) エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置
JP2005327689A (ja) エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置
JP4393788B2 (ja) エレクトロルミネッセンス素子、面光源および表示装置
JP7491346B2 (ja) 拡散部材、積層体、拡散部材のセット、ledバックライトおよび表示装置
JP2005327688A (ja) エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置
WO2005112515A1 (fr) Élément électroluminescent, éclairage et affichage
JP2005327686A (ja) エレクトロルミネッセンス素子、並びにこれを用いた照明装置および表示装置
US20060012291A1 (en) Organic light-emitting source
JP2011054443A (ja) 拡散材、導光体ユニット、および面光源装置
JP5515799B2 (ja) 面光源装置用積層体及び面光源装置
CN214956952U (zh) 一种具有反射镀层的柔性oled背板膜及柔性oled
JP5870651B2 (ja) レンズシート及びそれを具備した有機el素子

Legal Events

Date Code Title Description
AK Designated states

Kind code of ref document: A1

Designated state(s): AE AG AL AM AT AU AZ BA BB BG BR BW BY BZ CA CH CN CO CR CU CZ DE DK DM DZ EC EE EG ES FI GB GD GE GH GM HR HU ID IL IN IS KE KG KM KP KR KZ LC LK LR LS LT LU LV MA MD MG MK MN MW MX MZ NA NG NI NO NZ OM PG PH PL PT RO RU SC SD SE SG SK SL SM SY TJ TM TN TR TT TZ UA UG US UZ VC VN YU ZA ZM ZW

AL Designated countries for regional patents

Kind code of ref document: A1

Designated state(s): GM KE LS MW MZ NA SD SL SZ TZ UG ZM ZW AM AZ BY KG KZ MD RU TJ TM AT BE BG CH CY CZ DE DK EE ES FI FR GB GR HU IE IS IT LT LU MC NL PL PT RO SE SI SK TR BF BJ CF CG CI CM GA GN GQ GW ML MR NE SN TD TG

121 Ep: the epo has been informed by wipo that ep was designated in this application
NENP Non-entry into the national phase

Ref country code: DE

WWW Wipo information: withdrawn in national office

Country of ref document: DE

122 Ep: pct application non-entry in european phase