TW413621B - Method of producing zipper having chain teeth with metallic multi-color on its surface - Google Patents
Method of producing zipper having chain teeth with metallic multi-color on its surface Download PDFInfo
- Publication number
- TW413621B TW413621B TW87115935A TW87115935A TW413621B TW 413621 B TW413621 B TW 413621B TW 87115935 A TW87115935 A TW 87115935A TW 87115935 A TW87115935 A TW 87115935A TW 413621 B TW413621 B TW 413621B
- Authority
- TW
- Taiwan
- Prior art keywords
- colorful
- metal
- layer
- zipper
- transparent resin
- Prior art date
Description
413621 ’ Λ 7 37 -- 一 五、發明説明(/ ) 本發明係關於拉鏈鏈齒表面具金屬樣多彩之製造方 法,尤指於已鍍有金屬表面之尼龍系拉鏈鏈齒表面再製設 多彩金屬者。 按,於拉鏈鏈齒表面處理多彩習用技術,僅見於專利 前案之公告第245630號’但該專利前案之技術内容由其 說明書之敘述,可明確看出其僅能針對八BS拉鏈鏈齒表 面,以西德進口之雷射轉印紙熱轉印於鏈齒表面上,而得 所謂「具七彩折射效果之拉鍵鏈齒」,但該案亦於其說明 書之背景内明確指出,其無法對傳統之尼龍系或塑鋼系之 拉鏈鏈齒製出同樣效果,即,該案之熱轉印手段,無法使 七彩折射效果之雷射轉印紙之金屬膜黏著在尼龍系或塑鋼 系之拉鏈鏈齒表面上。 事實上’傳統之尼龍系或塑鋼系之拉鏈鏈齒之無法有 多彩之金屬色澤,主要困難在於這類塑膠難以電鍍,即使 採用真空蒸鍍之方式’至多產生單一之金屬光澤,如再試 著蒸著其他金屬,反而產生剝落之現象,故而業界有人轉 而使用熱轉印之方式,且雖終有前述公告第245630號之 專利前案產生,可惜的是,使用最多的尼龍系之拉鏈鏈齒 仍無法以該熱轉印之方式獲得多彩之金屬色澤。 吾人詳閱公告第245630號之專利前案,可知其係直 接將雷射轉印紙熱轉印於鏈齒表面上’故,該案解決問題 之手段是找出適用熱轉印的塑膠材質,而非研發適當的程 序或方法,然而,該案所採之塑膠材質ABS強度比較差, 所製成之拉鏈往往使用不久即已壞掉,相對的在過去也較 / --------{—裳-- (請先閱禎背而之注意事項再填,κ-本K j
-IT 經濟部中央標竿局员工消費合作社印掣 本紙狀度適用中_家標华(CNS) Λ4現格 (2丨0Χ 297公尨) «3621 A7 B7 五、發明説明(3« ) M濟部中央標準局負工消费合作社印家 少使用於拉鏈鏈齒上,該案使用ABS純粹只在取得 感,耐用度無法與尼龍系拉鏈鏈齒相比; ° 本發明人_於上述缝上之絲,乃延續先前已 之試驗經驗,著手於尼龍系拉鏈鏈齒之表面予金屬樣多彩 化〇 . 初始,本發明人採取直接每尼龍系拉鏈鏈齒之表面鍍 上多彩’但效果不佳1 *但喊的·想,觸視覺也不 好,接著在4述岫案公告後,試著以其他熱轉印媒及溫壓 條件使用於尼龍系拉鏈鏈齒,仍得失敗之結果。 本發明人乃再嘗試其他方式,經多次實驗與修正後, 終有本發明之誕生。 本發明之目的亦即在提供一種拉鏈鏈齒表面具金屬樣 多彩之製造方法,係可於已鍍有金屬表面之尼龍系拉鏈鏈 齒表面再製設多彩金屬者β 而’本發明之實用價值或產業上之利用價值,自在於 可獲得強度較佳而表面鍍上多彩之尼龍系拉鏈鏈齒。 至於本發明之實例’則請參閱第—圖之流程圖」,製造 流程如下: 1. 尼龍系拉鏈鏈齒水洗去鹿; 2. 烘乾; 3. 鏈齒表面噴附一層樹脂; 4. 乾燥; 5·鍍一層金屬薄膜: 6.再啃附上一層樹脂; 本歸尺A適则,_家轉(OMS )⑽秘⑺GX297公们 0— (却先閲讀背面之注寫本頁) ¾ 訂· .—線------- I. I · 413621 經濟部中央捸準局男工消費合作社印製 A7 B7 五、發明説明(3 ) 7. 另於一透明樹脂基材上鍍上多彩金屬薄膜層; 8. 將前一流程之多彩金屬薄膜層以攝氏120至180 度,適當壓力輥壓轉印於鏈齒表面; 9. 再喷附上一層樹脂,作為表面保護σ 經以上之流程,如附件一附貼於紙上之樣品,係拉鏈 鏈齒表面上具一層金屬薄膜,金屬薄膜上具一層透明樹 脂,該透明樹脂上具一層多彩金屬薄膜層,該多彩金屬薄 膜層上具一層透明樹脂者,而可得一厚度約在〇> 〇〇1至 之夕彩金厲薄膜層於尼龍系拉鍵鍵齒表面,從而使該尼龍 系拉鏈鏈齒可具有金屬樣之多彩色澤之折射β 前述本發明 < 實例所指之',鍍"乃指真空蒸(電)鍍為 主。 前述流程5之金屬薄膜以鋁最為普遍,但仍可為其他 金屬。 … 前述流程6之樹脂為透明樹脂,流程9之樹脂亦為透 明樹脂。 前述流程7可直接以已另行完成(包括自製與採購)之 多彩金屬薄膜層取代,而逕予進行第8流程。 此外,本發明實例之流程7可為直接將多彩金屬薄膜 層鑛在流程6之透明樹脂上;同時流輕8則將拉鍵鍵齒及 其上之多彩金屬薄膜層,一起以熱壓輥輪於攝氏丨2〇至18〇 度’適當壓力下輥壓而固黏於鏈齒表面;最後,再實施原 來之流程9 ’表面喷附上-廣透明樹脂’作為表面保護。'、 經由前述方法獲致之尼龍系拉鏈鏈齒,表面具有牢固 本紙iR尺度適用中國國家榡隼(CNS ) Λ4规格_( 2丨ΟX ~~ —~~---- ---------f-------1T--^-----洛 (哳先閱讀背面之注意事^.v^寫本頁)( A7 B7 五、發明説明(彳) 之多彩金屬薄膜層僅0. 001至lyiim,既具有多種金屬樣色 澤之光彩,更重要的是不需要仰賴進口之雷射轉印紙,也 不需要被迫使用強度差之ABS,對拉鏈產業業界而言,其 利用價值實已明顯突出。 (請先閱讀背面之注意事Γ.填寫本頁) .裝.
• In *-° 線 經濟部中央標準局貝工消費合作社印製 本紙张尺度逋用中S國家標準(CNS ) Λ4规格(210X297公釐)
Claims (1)
- 413621 A6 B8 C8 D8 A 標 奉 為 Ά 工 消 費 合 作 社 印 袋 、申請專利範圍 (1) 1. 一種拉鏈鏈齒表面具金屬樣多彩之製造方法,其流 程如下: (1) .尼龍系拉鏈鏈齒水洗去脂; (2) .烘乾: (3) .鏈齒表面嗜附一唐樹脂; (4) .乾燥; _ (5) .鍍一層金屬薄膜; (6) .再喷附上一層透明樹脂; (7) .另於一透明樹脂基材上鍍上多彩金屬薄臈層; (8乂將前一流程之多彩金屬薄膜層以攝氏12〇至ι8〇 度,適當壓力輥壓轉印於鏈齒表面; (9).再噴附上一層透明樹脂,作為表面保護。 2. 如申請專利範圍第1項所述之拉鏈键齒表面具金屬 樣多彩之製造方法,其中流程(5)及流程(7)係指真空蒸鍍 者。 3. 如申凊專利範圍苐1項所述之拉鏈鍵齒表面具金屬 樣多彩之製造方法,其中流程(5)之金屬薄臈係鋁者。 4. 如申请專利範圍第1項所述之拉鏈鏈齒表面具金屬 樣多彩之®造方法,其中流程⑺可直接由—已製妥之多 彩金屬薄臈層轉印材料所取代。 5. 如申清專彳彳範ϋ第I項所述之拉鏈鏈齒表面具金眉 樣多彩之製造方法,其巾流程⑺可為直接將多彩金層薄 膜層錢在_⑹之透_撕上;晴流程⑻翁拉鍵鍵 齒及其上之多彩金㈣朗’―起以鍾輥輪於攝氏⑽ .(I 裳 -TJ線 (請先閲讀背面之注f項再填寫本頁} 訂3621丨範圍(2 至18〇縻,、, β ’適當壓力下輥壓而固黏於鏈齒表面者。 樣多彩之=凊專利範圍第1項所述之拉鏈鏈齒表面具金屬 屬薄^製造方法之製成品,係拉鏈鏈齒表面上具一層金 層多彩’金屬薄膜上具一層透明樹脂,該透明樹脂上具一 者。7金屬缚膜層’該多彩金屬薄膜層上具一層透明樹脂 L如申請專利範圍第6項所述之拉鏈鏈齒表面具金屬 遂|彩之製造方法之製成品’其中多彩金屬薄膜層係厚度 者。 (CNS ) Α4规格(210X297公釐)