SU567755A1 - Способ рафинировани ферросилици - Google Patents

Способ рафинировани ферросилици

Info

Publication number
SU567755A1
SU567755A1 SU7602345756A SU2345756A SU567755A1 SU 567755 A1 SU567755 A1 SU 567755A1 SU 7602345756 A SU7602345756 A SU 7602345756A SU 2345756 A SU2345756 A SU 2345756A SU 567755 A1 SU567755 A1 SU 567755A1
Authority
SU
USSR - Soviet Union
Prior art keywords
metal
slag
impurities
flies
iron
Prior art date
Application number
SU7602345756A
Other languages
English (en)
Inventor
Николай Павлович Меликаев
Юрий Игнатьевич Мухин
Моисей Иосифович Друинский
Анатолий Алексеевич Парфенов
Original Assignee
Melikaev Nikolaj P
Mukhin Yurij
Druinskij Moisej
Parfenov Anatolij A
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Melikaev Nikolaj P, Mukhin Yurij, Druinskij Moisej, Parfenov Anatolij A filed Critical Melikaev Nikolaj P
Priority to SU7602345756A priority Critical patent/SU567755A1/ru
Application granted granted Critical
Publication of SU567755A1 publication Critical patent/SU567755A1/ru

Links

Claims (1)

  1. (54) СПСЮОБ РАФИНИРОВАНИЯ ФЕРРОСИЛИЦИЯ работки шлак перемешивали с металлом дерев нными рейками в течение 6 мин к после этого вьшерживали в ковше 15 ми Анализ металла до и после обработки пр ставлен вес.%: Содержание в метал Металл ЗВОСГГКН /Q.A . 1«ь/ь.ViO«. «-« в нспользован ом пирите содержание железа 36%, следовательно, в металл вн сено 240.хО,Зв-8в кг. Удалено примесей: алюминн  (а.51 Ul.22)3650 - 48 квльа  (1.27-0,32)к3650 магнк (0.31x3650 -. ., 100 При переходе примесей в шлак содер жание Еремни  в металле должно составить 75.4 «3650 . , 7с; д% :Зв50-48.В5-11+86 НО фактичесви составило 78,1%. Следовательно, часть примесей была использована на восстановление коемннй из шлака, образовавшегос  из рафинировочной смеси. Возрастаниесодержани  кремни  в металле подтверждает, что при предложенном способе обработки идет восстановление кремни  из шлака. Использование предлагаемого способа обработки ферросилици  обеспечивает отсутствие улета кремни  в виде фторидов и компенсацию улета кремни  восстановлением его из шлака алюминием, кальцием, магни ем , что значительно улучшает техникиэкономические показатели процесса получени  рационированного ферросилици . Формула изобретени  Способ рафинировани  ферросилиций, включающий обработку жидкого сплава в ковше ;рафинировочной| смесью, 6 тличйюшийс   тем, что, с целью снижени  потерь кремни  сплава, на струю заливаемого в ковШ сплава подают 2-2О% от веса обрабатьюаемого металла рафинировочной смеси пирита и силикатов натри , вз тых в соотношении 1:(0,3-4). ИсточниЕН информации, прин тые во вниМйние при экспертизе: i: Патент ПНР J 70806, кл. С 22 С 35/00, 1869.
SU7602345756A 1976-04-07 1976-04-07 Способ рафинировани ферросилици SU567755A1 (ru)