SU554251A1 - Шихта дл изготовлени огнеупоров - Google Patents

Шихта дл изготовлени огнеупоров

Info

Publication number
SU554251A1
SU554251A1 SU2301624A SU2301624A SU554251A1 SU 554251 A1 SU554251 A1 SU 554251A1 SU 2301624 A SU2301624 A SU 2301624A SU 2301624 A SU2301624 A SU 2301624A SU 554251 A1 SU554251 A1 SU 554251A1
Authority
SU
USSR - Soviet Union
Prior art keywords
refractories
mixture
manufacture
products
temperature
Prior art date
Application number
SU2301624A
Other languages
English (en)
Inventor
Юрий Федорович Костыря
Николай Семенович Климкович
Сталина Николаевна Умеренкова
Сергей Глебович Тресвятский
Виктор Николаевич Павликов
Original Assignee
Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт filed Critical Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт
Priority to SU2301624A priority Critical patent/SU554251A1/ru
Application granted granted Critical
Publication of SU554251A1 publication Critical patent/SU554251A1/ru

Description

(54) ШИХТА ДЛЯ ИЗГОТОВЛЕНИЯ ОГНЕУПОРОВ
60°С/мин. Игольчатые кристаллы двуокиси циркони  содержат 99,9% ZrOg. Средние размеры игольчатых монокристаллов двуокиси циркони  составл ют по длине 150-350 мкм, по толщине 0,5-5 мкм.
Издели  из предлагаемой шихты получают по обычной керамической технологии. Исходные компоненты смешивают в необходимом количестве. Из полученной смеси прессуют заготовки при удельном давлении не менее 1300 кг/см. Временной св зкой служит сульфитно-спиртова  бражка плотностью 1,25- 1,27 г/см. Обжиг изделий производитс  при температуре не более 1720°С.
Полученные изделн  имеют следуюш,ие физико-механические свойства:
Открыта  пористость, %17,9
Предел прочности цри сжатии,
КГ/СМ2680
Температура начала деформации под нагрузкой 2 кг/см, °С 1690 Термостойкость при 1300°С с воздушным охлаждением, количество теплосмен20
Механическа  прочность на
сжатие при 1500°С, кг/см 280
Издели  из предлагаемой шихты могут также найти применение в установках внепечной обработки стали, непрерывной и бесстопорной разливки стали.
Технико-экономическа  эффективность применени  огнеупоров из предлагаемой шихты достигаетс  повышением стойкости огнеупоров в сравнении с известными на 30-40% в результате повышени  термической стойкости и прочностных свойств при высоких температурах .

Claims (2)

1.Авторское свидетельство СССР № 292926, кл. С 04В 35/06, 1968.
2.Авторское свидетельство СССР № 421668, С 04В, 35/04, 1972.
SU2301624A 1975-12-16 1975-12-16 Шихта дл изготовлени огнеупоров SU554251A1 (ru)