SU374254A1 - Огнеупорный материал - Google Patents

Огнеупорный материал

Info

Publication number
SU374254A1
SU374254A1 SU1658595A SU1658595A SU374254A1 SU 374254 A1 SU374254 A1 SU 374254A1 SU 1658595 A SU1658595 A SU 1658595A SU 1658595 A SU1658595 A SU 1658595A SU 374254 A1 SU374254 A1 SU 374254A1
Authority
SU
USSR - Soviet Union
Prior art keywords
refractory material
chromium oxide
heat resistance
zirconia
bending
Prior art date
Application number
SU1658595A
Other languages
English (en)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1658595A priority Critical patent/SU374254A1/ru
Application granted granted Critical
Publication of SU374254A1 publication Critical patent/SU374254A1/ru

Description

Изобретение относитс  -к неоргани-чеоким материала м типа «ерамики, .которые могут быть иопользованы в качестве конструкцион:ного материала в вы:сокотем1пе|ратур,ных агрегатах .
Известен огнеупорный -материал на основе акиси хрома.
Цель Предлагаемаго изобретени  - повышение термостойкости огнеупор ного материала .
Это достигаетс  тем, что 1материал содержит окиси Х|рама 80-85 о;бъбмных % и, кроме того, 15-20 объемных % нитевидных монокристаллов двуокиси циркони .
Материал получают следующим образом.
Диюперсный порошок окиси хрома смешивают с нитевидеыми монокристаллами двуокиси циркони  (/ мк, d 0,5- 5 мк).
Полученную смесь подвергают гор чему прессаваиию по следующему режиму:
1300°С
температура
150-200 кг/см давление 15-20 мин. выдерж1ка Затем омесь охлаждают в графитовой
пресс-форме.
Ползченный материал
ооладает следуюЩИ1МИ свойствами:
пористость, %
4,8 П|рач;ность при изгибе, кг/см 1520
термостойкость (количество воздушных циклов 1000-20° С)
150
Предмет изобретени 
15
Огнеупорный материал «а основе окиси хрома, отличающийс  тем, что, с целью повышени  термостойкости, он содержит в 20 объемных %%: окись Х1рома 80-85 и, кроме того, нитевидные кристаллы двуокиси циркони  15-20.
SU1658595A 1971-05-17 1971-05-17 Огнеупорный материал SU374254A1 (ru)