SU554252A1 - Шихта дл изготовлени огнеупоров - Google Patents

Шихта дл изготовлени огнеупоров

Info

Publication number
SU554252A1
SU554252A1 SU2301673A SU2301673A SU554252A1 SU 554252 A1 SU554252 A1 SU 554252A1 SU 2301673 A SU2301673 A SU 2301673A SU 2301673 A SU2301673 A SU 2301673A SU 554252 A1 SU554252 A1 SU 554252A1
Authority
SU
USSR - Soviet Union
Prior art keywords
mixture
refractories
manufacture
temperature
single crystals
Prior art date
Application number
SU2301673A
Other languages
English (en)
Inventor
Юрий Федорович Костыря
Николай Семенович Климкович
Сталина Николаевна Умеренкова
Виталий Николаевич Терещенко
Сергей Глебович Тресвятский
Виктор Николаевич Павликов
Original Assignee
Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт filed Critical Днепропетровский Ордена Трудового Красного Знамени Металлургический Институт
Priority to SU2301673A priority Critical patent/SU554252A1/ru
Application granted granted Critical
Publication of SU554252A1 publication Critical patent/SU554252A1/ru

Description

иые компоненты смешивают в необходимых количествах. Из полученной смеси прессуют заготовки при удельном давлении не менее 1300 кг/см2. Временной св зкой может быть сульфитно-спиртова  барда плотностью 1,24- 1,27 г/см. Обжиг изделий проводитс  при температуре не более 1730°С.
Физико-керамические свойства полученных изделий:
Открыта  пористость, %10,1
Предел прочности при сжатии,
кг/см2580
Температура начала деформации под нагрузкой 2 кг/см, °С 1740 Термостойкость при 1300°С с воздупшым охлаждением, количество теплосмен15
Мехаиическа  прочность на
сжатие при 1500°С, кг/см 320
Введение в клинкерную массу игольчатых кристаллов двуокиси циркони  способствует повьппению термической стойкости изделий и их npoiHOCTHbix характеристик при высоких температурах. Монокристаллам свойственно сохран ть прочность при высоких температурах . Вследствие образовани  ориентированной структуры огнеупора монокристаллы несут основную механическую нагрузку, что обеспечивает целостность материала при резких изменени х температуры и механических воздействий .
Повыо)ение термической стойкости объ сн етс  эффектом рассеивани  монокристаллами кинетической энергии распростран ющихс  микротрен1,ин, что способствует их локализации .

Claims (2)

1.Авторское свидетельство СССР №389060, кл. С 04В 35/20, 1971.
2.Авторское свидетельство СССР N° 149702, кл. С 04В 35/04, 1954.
SU2301673A 1975-12-16 1975-12-16 Шихта дл изготовлени огнеупоров SU554252A1 (ru)