SU123179A1 - The way to improve the wear resistance of piston cast iron rings - Google Patents

The way to improve the wear resistance of piston cast iron rings

Info

Publication number
SU123179A1
SU123179A1 SU62104A SU624104A SU123179A1 SU 123179 A1 SU123179 A1 SU 123179A1 SU 62104 A SU62104 A SU 62104A SU 624104 A SU624104 A SU 624104A SU 123179 A1 SU123179 A1 SU 123179A1
Authority
SU
USSR - Soviet Union
Prior art keywords
wear resistance
improve
way
cast iron
iron rings
Prior art date
Application number
SU62104A
Other languages
Russian (ru)
Inventor
С.А. Иванов
М.М. Снитковский
Original Assignee
С.А. Иванов
М.М. Снитковский
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by С.А. Иванов, М.М. Снитковский filed Critical С.А. Иванов
Priority to SU62104A priority Critical patent/SU123179A1/en
Application granted granted Critical
Publication of SU123179A1 publication Critical patent/SU123179A1/en

Description

Предлагаемый способ повышени  срока службы поршневых колец и цилиндровых втулок позвол ет значительно повысить их износостойкость . Способ заключаетс  в гор чем обжатии поршневых колец в штампе.The proposed method of increasing the service life of piston rings and cylinder sleeves makes it possible to significantly increase their wear resistance. The method consists in hot-pressing the piston rings in the die.

На чертеже показана схема обжати  поршневого кольца / на прессе пуансоном 2 в матрице 3.The drawing shows the scheme of compression of the piston ring / press punch 2 in the matrix 3.

Литую заготовку кольца после первой обточки нагревают в печи до 900-950°, обжимают s штампе и охлаждают до 300-400°. Дл  уменьшени  времени обжати  штамп охлаждают проточной водой. После обжати  заготовку кольца подвергают отпуску при 600° и окончательно обрабатывают.After the first turning, the cast ring billet is heated in the furnace to 900–950 °, compressed with the die and cooled to 300–400 °. To reduce the compression time, the stamp is cooled with running water. After crimping, the billet of the ring is subjected to tempering at 600 ° and finally processed.

Предмет изобретени Subject invention

Способ повышени  износостойкости поршневых чугунных колец, отличаюш ийс  тем, что, с целью повышени  износостойкости, заготовки колец перед окончательной механической обработкой подвергаютс  нагреву до 900-950° и обжимаютс  в матрице с охлаждением до 300-400°, после чего вынимаютс  из матрицы и подвергаютс  отпуску лри 600°.The method of increasing the wear resistance of piston cast iron rings, is distinguished by the fact that, in order to increase the wear resistance, the billet rings are heated to 900-950 ° before final machining and compressed in a matrix with cooling to 300-400 °, after which they are removed from the matrix and subjected 600 ° temp.

SU62104A 1959-04-03 1959-04-03 The way to improve the wear resistance of piston cast iron rings SU123179A1 (en)