KR900015365A - 초전도 물품의 제조방법 - Google Patents
초전도 물품의 제조방법 Download PDFInfo
- Publication number
- KR900015365A KR900015365A KR1019900002813A KR900002813A KR900015365A KR 900015365 A KR900015365 A KR 900015365A KR 1019900002813 A KR1019900002813 A KR 1019900002813A KR 900002813 A KR900002813 A KR 900002813A KR 900015365 A KR900015365 A KR 900015365A
- Authority
- KR
- South Korea
- Prior art keywords
- layer
- superconducting
- mixture
- bacuo
- lnba
- Prior art date
Abstract
내용 없음.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제3도는 초천도물품을 제조하기 위한 본 발명의 방법의 한 실시양태에서의 전반의 스텝을 나타내는 개략 설명도,
제4도는 초전도물품을 제조하기 위한 본 발명의 방법의 한 실시양태에서의 중반의 스텝을 나타내는 개략 설명도,
제5도는 초전도물품을 제조하기 위한 본 발명의 방법을 한 실시양태에서의 후반의 스텝을 나타내는 개략 설명도.
Claims (4)
- LnBa2Cu3Ox및 LnBa2CuOx의 혼합물로 되는 제2층을 모재의 표면상에 형성하고, 여기서 Ln는 임의의 희토류원소이며, 그리고 제1층내에서의 Ln2BaCuOx의 함유비율은 LnBa2Cu3Ox및 LnBaCuOx의 합계량에 관하여 5-80wt.%의 번위내에 있고, 이어 제1층의 표면상에 적어도 CuO 및 BaCuO2의 혼합물로 되는 제2층을 형성하고, 이 제2층은 800-1,000℃의 범위내의 융점을 지니고 있고, 이어 제2층내의 혼합물을 용융시켜 그리고, 제2층용융 상태를 산소함유 분위기에서 1분-4시간 유지하여 제2층내의 혼합물의 융융물을 제1층내의 Ln2BaCuox와 확산반응시켜 그것에 의하여 제1층 및 제2층을 LnBa2Cu3Ox로 되는 초전도물질의 피막으로 변환하고, 그리고 이와같이 하여 생성된 초전도물질의 피막을 상온에까지 냉각하고 이리하여 생성된 초전도물질의 피막을 상온에까지 냉각하고 이리하여 모재와 모재의 표면상에 형성된 초전도물질의 피막으로 되는 초전도물품을 제조하는 스텝으로 되는 것을 특징으로 하는 초전도물품의 제조방법.
- 제1항에 있어서, 모재는 세라믹, 니켈 및 니켈기 합금중의 어느것 한가지로 된 것을 특징으로 하는 초전도물품의 제조방법.
- 제1항 또는 제2항에 있어서, 제2층은 CuO, BaCuO2및 BaO의 혼합물로 되어 있고, 그리고, 제2층에서의 동(Cu)의 바륨(Ba)에 대한 비율은 몰(mole) 비율로 Cu:Ba=1:0.10-0.95인 것을 특징으로 하는 초전도물품의 제조방법.
- 제1항 또는 제2항에 있어서, 제2층은 CuO, BaCuO2B4OSB>9, Y2O3및 YBa2Cu3O7의 혼합물로 되어있고 그리고 제2층에서의 동(Cu)의 바륨(Ba) 및 이트륨(Y)에 대한 비율은, 몰 비율로 Cu:Ba:Y=1: 0.10-0.95:0.001-0.330인 것을 특징으로 하는 초전도물품의 제조방법.※참고사항:최초출원 내용에 의하여 공개하는 것임.