JPWO2023282194A5 - - Google Patents

Download PDF

Info

Publication number
JPWO2023282194A5
JPWO2023282194A5 JP2022568990A JP2022568990A JPWO2023282194A5 JP WO2023282194 A5 JPWO2023282194 A5 JP WO2023282194A5 JP 2022568990 A JP2022568990 A JP 2022568990A JP 2022568990 A JP2022568990 A JP 2022568990A JP WO2023282194 A5 JPWO2023282194 A5 JP WO2023282194A5
Authority
JP
Japan
Prior art keywords
less
group
mass
steel sheet
hot
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2022568990A
Other languages
English (en)
Other versions
JP7235188B1 (ja
JPWO2023282194A1 (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from PCT/JP2022/026417 external-priority patent/WO2023282194A1/ja
Publication of JPWO2023282194A1 publication Critical patent/JPWO2023282194A1/ja
Application granted granted Critical
Publication of JP7235188B1 publication Critical patent/JP7235188B1/ja
Publication of JPWO2023282194A5 publication Critical patent/JPWO2023282194A5/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (3)

  1. 無方向性電磁鋼板であって、
    質量%で、
    C:0.01%以下、
    Si:2.0%以上5.0%以下、
    Mn:0.05%以上5.00%以下、
    P:0.1%以下、
    S:0.01%以下、
    Al:3.0%以下および
    N:0.0050%以下
    を含み、Si+Alが4.5%以上であり、残部がFeおよび不可避不純物である成分組成を有し、
    鋼板中の結晶粒について、平均結晶粒径Xが60μm以上200μm以下であり、結晶粒径分布の標準偏差Sが次式(1):
    /X<0.75 …(1)
    を満たし、かつ、結晶粒径分布の歪度γが1.50以下であることを特徴とする、無方向性電磁鋼板。
  2. 前記成分組成は、下記A群、B群、C群、D群およびE群のうちの少なくとも一群をさらに含有する請求項1に記載の無方向性電磁鋼板。
    A群:質量%で、
    Co:0.0005%以上0.0050%以下
    B群:質量%で、
    Cr:0.05%以上5.00%以下
    C群:質量%で、
    Ca:0.001%以上0.100%以下、
    Mg:0.001%以上0.100%以下および
    REM:0.001%以上0.100%以下
    のいずれか1種または2種以上
    D群:質量%で、
    Sn:0.001%以上0.200%以下および
    Sb:0.001%以上0.200%以下
    のいずれか1種または2種
    E群:質量%で、
    Cu:0%以上0.5%以下、
    Ni:0%以上0.5%以下、
    Ti:0%以上0.005%以下、
    Nb:0%以上0.005%以下、
    V:0%以上0.010%以下、
    Ta:0%以上0.002%以下、
    B:0%以上0.002%以下、
    Ga:0%以上0.005%以下、
    Pb:0%以上0.002%以下、
    Zn:0%以上0.005%以下、
    Mo:0%以上0.05%以下、
    W:0%以上0.05%以下、
    Ge:0%以上0.05%以下および
    As:0%以上0.05%以下
    のいずれか1種または2種以上
  3. 請求項1または2に記載の無方向性電磁鋼板を製造する方法であって、
    請求項1または2に記載の成分組成を有する鋼素材に、熱間圧延を施して熱延板を得る熱間圧延工程と、
    前記熱延板に酸洗を施す酸洗工程と、
    前記酸洗が施された前記熱延板に、最終パス入側温度Tが50℃以上、最終パスの圧下率rが15%以上、および最終パスのひずみ速度εが100s-1以上1000s-1以下の条件にて冷間圧延を施して冷延板を得る冷間圧延工程と、
    前記冷延板を、500℃から700℃の平均昇温速度Vが10℃/s以上の条件にて、875℃以上1050℃以下の焼鈍温度Tまで加熱したのち、冷却して、無方向性電磁鋼板である冷延焼鈍板を得る焼鈍工程と、
    を備える、無方向性電磁鋼板の製造方法。
JP2022568990A 2021-07-08 2022-06-30 無方向性電磁鋼板およびその製造方法 Active JP7235188B1 (ja)