JPS6456855A - Austenitic stainless steel for boiler for soda recovery - Google Patents
Austenitic stainless steel for boiler for soda recoveryInfo
- Publication number
- JPS6456855A JPS6456855A JP21391487A JP21391487A JPS6456855A JP S6456855 A JPS6456855 A JP S6456855A JP 21391487 A JP21391487 A JP 21391487A JP 21391487 A JP21391487 A JP 21391487A JP S6456855 A JPS6456855 A JP S6456855A
- Authority
- JP
- Japan
- Prior art keywords
- boiler
- stainless steel
- austenitic stainless
- stock
- soda recovery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21391487A JPS6456855A (en) | 1987-08-27 | 1987-08-27 | Austenitic stainless steel for boiler for soda recovery |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21391487A JPS6456855A (en) | 1987-08-27 | 1987-08-27 | Austenitic stainless steel for boiler for soda recovery |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6456855A true JPS6456855A (en) | 1989-03-03 |
| JPH0431020B2 JPH0431020B2 (enExample) | 1992-05-25 |
Family
ID=16647124
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP21391487A Granted JPS6456855A (en) | 1987-08-27 | 1987-08-27 | Austenitic stainless steel for boiler for soda recovery |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6456855A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03153847A (ja) * | 1989-11-13 | 1991-07-01 | Nippon Steel Corp | クリープ破断特性のすぐれたNi―Crオーステナイト系ステンレス鋼 |
| EP0937783A1 (en) * | 1998-02-18 | 1999-08-25 | Sandvik Aktiebolag | New use of a high strength stainless steel |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62199753A (ja) * | 1986-02-25 | 1987-09-03 | Nippon Steel Corp | 高温環境下での時効後靭性および耐高温粒界腐食性に優れたオ−ステナイトステンレス鋼 |
-
1987
- 1987-08-27 JP JP21391487A patent/JPS6456855A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62199753A (ja) * | 1986-02-25 | 1987-09-03 | Nippon Steel Corp | 高温環境下での時効後靭性および耐高温粒界腐食性に優れたオ−ステナイトステンレス鋼 |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH03153847A (ja) * | 1989-11-13 | 1991-07-01 | Nippon Steel Corp | クリープ破断特性のすぐれたNi―Crオーステナイト系ステンレス鋼 |
| EP0937783A1 (en) * | 1998-02-18 | 1999-08-25 | Sandvik Aktiebolag | New use of a high strength stainless steel |
| US6174386B1 (en) | 1998-02-18 | 2001-01-16 | Sandvik Ab | NaOH evaporator comprising at least one component formed by a high strength stainless steel |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0431020B2 (enExample) | 1992-05-25 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR950000912A (ko) | 기계 가공성이 개선된 마르텐시틱 스테인레스강 | |
| NO149850B (no) | Varmebearbeidbart austenittisk rustfritt staal. | |
| HU906124D0 (en) | A ferrochromium alloy | |
| JPS5591960A (en) | High silicon-nickel-chromium steel with resistance to concentrated | |
| US4390367A (en) | High-alloyed steel being resistive to corrosion by natural gas | |
| NO177604B (no) | Austenittisk rustfritt stål | |
| JPS5681658A (en) | Austenitic alloy pipe with superior hot steam oxidation resistance | |
| JPS572869A (en) | Austenite stainless steel for hot corrosive environment | |
| JPS6456855A (en) | Austenitic stainless steel for boiler for soda recovery | |
| KR900008053A (ko) | 오오스테나이트계 크롬-니켈 합금 | |
| US4102677A (en) | Austenitic stainless steel | |
| JPS5672156A (en) | Low-alloy heat-resistant steel for high temperature use | |
| EP0780483B1 (en) | High-strength austenitic heat-resisting steel having improved weldability | |
| JPS6468450A (en) | Austenitic stainless steel for seawater corrosion resistance | |
| Keown et al. | Niobium in stainless steels | |
| EP0205693B1 (en) | Special steels and their method of preparation | |
| KR880003024A (ko) | 내식성 구조용강 | |
| GB2123031A (en) | High-nickel austenitic alloys for sour well service | |
| GB905238A (en) | Improvements in or relating to austenitic stainless steels | |
| ES508364A0 (es) | Perfeccionamientos en un proceso para fabricar un acero inoxidable ferritico. | |
| JPS5662949A (en) | Steel products for steam turbine moving blade or the like | |
| JPS565949A (en) | High tensile steel with superior sulfide corrosion crack resistance and superior corrosion resistance | |
| JPH0430463B2 (enExample) | ||
| JPS57143467A (en) | Low c-low si-cr-mo steel used in wet vapor | |
| Floreen | Chromium substitution in stainless steels. |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| EXPY | Cancellation because of completion of term | ||
| FPAY | Renewal fee payment (prs date is renewal date of database) |
Year of fee payment: 16 Free format text: PAYMENT UNTIL: 20080525 |