JPS6455366A - Heat treatment for heat-transfer pipe - Google Patents

Heat treatment for heat-transfer pipe

Info

Publication number
JPS6455366A
JPS6455366A JP21156587A JP21156587A JPS6455366A JP S6455366 A JPS6455366 A JP S6455366A JP 21156587 A JP21156587 A JP 21156587A JP 21156587 A JP21156587 A JP 21156587A JP S6455366 A JPS6455366 A JP S6455366A
Authority
JP
Japan
Prior art keywords
corrosion resistance
heat
heat treatment
pipe
transfer pipe
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP21156587A
Other languages
Japanese (ja)
Other versions
JPH0524985B2 (en
Inventor
Kazuo Yamanaka
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP21156587A priority Critical patent/JPS6455366A/en
Publication of JPS6455366A publication Critical patent/JPS6455366A/en
Publication of JPH0524985B2 publication Critical patent/JPH0524985B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE:To improve the corrosion resistance, particularly uniform corrosion resistance, of a pipe without the addition of new stages, by carrying out a part of the grain boundary-strengthening heat treatment process of a heat- transfer pipe made of Ni-base alloy under specific conditions and then forming an oxide film composed principally of chromium oxide on the surface of the above heat-transfer pipe. CONSTITUTION:As a part of the above heat treatment process in which the above pipe containing, by weight, 20-35% Cr and 40-70% Ni is heated and held under a vacuum as high as >=about 10<-5>Torr, heat treatment is carried out by lowering the degree of vacuum to 10<-2>-10<-4>Torr under the conditions within the area enclosed with straight lines connecting the points A, B, C, D, E, F and A in figure, by which an oxide film composed principally of chromium oxide is formed on the surface of the above pipe. By this method, the corrosion resistance, particularly uniform corrosion resistance, of the above pipe used under a high-temp. and high-pressure water environment can be improved to a greater extent.
JP21156587A 1987-08-26 1987-08-26 Heat treatment for heat-transfer pipe Granted JPS6455366A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP21156587A JPS6455366A (en) 1987-08-26 1987-08-26 Heat treatment for heat-transfer pipe

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP21156587A JPS6455366A (en) 1987-08-26 1987-08-26 Heat treatment for heat-transfer pipe

Publications (2)

Publication Number Publication Date
JPS6455366A true JPS6455366A (en) 1989-03-02
JPH0524985B2 JPH0524985B2 (en) 1993-04-09

Family

ID=16607892

Family Applications (1)

Application Number Title Priority Date Filing Date
JP21156587A Granted JPS6455366A (en) 1987-08-26 1987-08-26 Heat treatment for heat-transfer pipe

Country Status (1)

Country Link
JP (1) JPS6455366A (en)

Cited By (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6482528B2 (en) 2000-08-11 2002-11-19 Sumitomo Metal Industries, Inc. Nickel-base alloy product and method of producing the same
JP2004183051A (en) * 2002-12-04 2004-07-02 Hitachi Ltd Valve stem, production method therefor, and steam valve obtained by using the same
US7037390B2 (en) 2002-02-13 2006-05-02 Sumitomo Metal Industries, Ltd. Method of heat treatment for Ni-base alloy tube
WO2007119706A1 (en) 2006-04-12 2007-10-25 Sumitomo Metal Industries, Ltd. METHOD FOR PRODUCING Cr-CONTAINING NICKEL-BASED ALLOY PIPE AND Cr-CONTAINING NICKEL-BASED ALLOY PIPE
JP2010270400A (en) * 2010-07-21 2010-12-02 Sumitomo Metal Ind Ltd Steam generator tubing for nuclear power plant
WO2012026344A1 (en) 2010-08-26 2012-03-01 住友金属工業株式会社 Cr-containing austenite alloy pipe and production method for same
US8241439B2 (en) 2008-05-16 2012-08-14 Sumitomo Metal Industries, Ltd. Ni-Cr alloy material
WO2013146034A1 (en) 2012-03-28 2013-10-03 新日鐵住金株式会社 Cr-CONTAINING AUSTENITIC ALLOY AND METHOD FOR PRODUCING SAME
WO2013150947A1 (en) 2012-04-04 2013-10-10 新日鐵住金株式会社 Cr-containing austenitic alloy
WO2013191202A1 (en) 2012-06-20 2013-12-27 新日鐵住金株式会社 Austenitic alloy tube
WO2016052551A1 (en) * 2014-09-29 2016-04-07 新日鐵住金株式会社 Ni-BASED ALLOY PIPE

Cited By (24)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6482528B2 (en) 2000-08-11 2002-11-19 Sumitomo Metal Industries, Inc. Nickel-base alloy product and method of producing the same
US7037390B2 (en) 2002-02-13 2006-05-02 Sumitomo Metal Industries, Ltd. Method of heat treatment for Ni-base alloy tube
JP2004183051A (en) * 2002-12-04 2004-07-02 Hitachi Ltd Valve stem, production method therefor, and steam valve obtained by using the same
WO2007119706A1 (en) 2006-04-12 2007-10-25 Sumitomo Metal Industries, Ltd. METHOD FOR PRODUCING Cr-CONTAINING NICKEL-BASED ALLOY PIPE AND Cr-CONTAINING NICKEL-BASED ALLOY PIPE
JP2007284704A (en) * 2006-04-12 2007-11-01 Sumitomo Metal Ind Ltd METHOD FOR MANUFACTURING Cr-CONTAINING NICKEL-BASED ALLOY PIPE AND Cr-CONTAINING NICKEL-BASED ALLOY PIPE
US8241439B2 (en) 2008-05-16 2012-08-14 Sumitomo Metal Industries, Ltd. Ni-Cr alloy material
JP2010270400A (en) * 2010-07-21 2010-12-02 Sumitomo Metal Ind Ltd Steam generator tubing for nuclear power plant
WO2012026344A1 (en) 2010-08-26 2012-03-01 住友金属工業株式会社 Cr-containing austenite alloy pipe and production method for same
KR20150036820A (en) 2010-08-26 2015-04-07 신닛테츠스미킨 카부시키카이샤 Cr-containing austenite alloy pipe and production method for same
US9255319B2 (en) 2010-08-26 2016-02-09 Nippon Steel & Sumitomo Metal Corporation Cr-containing austenitic alloy tube and method for producing the same
KR20160013254A (en) 2010-08-26 2016-02-03 신닛테츠스미킨 카부시키카이샤 Cr-containing austenite alloy pipe and production method for same
WO2013146034A1 (en) 2012-03-28 2013-10-03 新日鐵住金株式会社 Cr-CONTAINING AUSTENITIC ALLOY AND METHOD FOR PRODUCING SAME
US9695486B2 (en) 2012-03-28 2017-07-04 Nippon Steel & Sumitomo Metal Corporation Cr-containing austenitic alloy and method for producing the same
KR20170003709A (en) 2012-04-04 2017-01-09 신닛테츠스미킨 카부시키카이샤 Cr-containing austenitic alloy
JP5561431B2 (en) * 2012-04-04 2014-07-30 新日鐵住金株式会社 Chromium-containing austenitic alloy
US9493860B2 (en) 2012-04-04 2016-11-15 Nippon Steel & Sumitomo Metal Corporation Chromium-containing austenitic alloy
WO2013150947A1 (en) 2012-04-04 2013-10-10 新日鐵住金株式会社 Cr-containing austenitic alloy
KR20150012288A (en) 2012-06-20 2015-02-03 신닛테츠스미킨 카부시키카이샤 Austenitic alloy tube
WO2013191202A1 (en) 2012-06-20 2013-12-27 新日鐵住金株式会社 Austenitic alloy tube
US9859026B2 (en) 2012-06-20 2018-01-02 Nippon Steel & Sumitomo Metal Corporation Austenitic alloy tube
WO2016052551A1 (en) * 2014-09-29 2016-04-07 新日鐵住金株式会社 Ni-BASED ALLOY PIPE
JPWO2016052551A1 (en) * 2014-09-29 2017-07-06 新日鐵住金株式会社 Ni-base alloy tube
CN107075618A (en) * 2014-09-29 2017-08-18 新日铁住金株式会社 Ni base alloy pipes
US10106871B2 (en) 2014-09-29 2018-10-23 Nippon Steel & Sumitomo Metal Corporation Ni-based alloy tube

Also Published As

Publication number Publication date
JPH0524985B2 (en) 1993-04-09

Similar Documents

Publication Publication Date Title
JPS6455366A (en) Heat treatment for heat-transfer pipe
JPS52152814A (en) Thermo-mechanical treatment of seamless steel pipe
JPS54145335A (en) Surface reforming of metal molding
EP0349044A3 (en) Process for the production of a protective film on a magnesium-based substrate, application to the protection of magnesium alloys, substrates thus obtained
EP0107297A3 (en) An anti-corrosion treatment process
JPS54138814A (en) Thermo-mechanical treatment method for austenitic stainless steel pipe to give hot steam oxidation resistance
JPS6428349A (en) Manufacture of aluminum-plated steel sheet and steel foil using stainless steel as base material
JPS6473059A (en) Method for working nickel-base alloy
SE8007053L (en) STABILIZATION OF COALS IN AUSTENITIC ROD ALLOYS
JPS5528351A (en) Treating method for ceramic spray coating
JPS5531118A (en) Surface-treating method for metal
JPS55138096A (en) Surface treated steel plate, for resistance welding having layer containing ni
JPS56105470A (en) Production of steel material having excellent resistance against steam oxidation
JPS5641363A (en) Tinplate
Babei et al. Effect of friction-strengthening treatment on the low-cycle corrosion fatigue of steel 65 G with rigid loading
JPS5597460A (en) Manufacture of aluminum clad stainless steel
JPS5322809A (en) Heat treating method of piping
JPS57120660A (en) Manufacture of nickel superalloy
JPS5534643A (en) Manufacture of very thin steel sheet coated with iron- tin alloy
JPS5511137A (en) Corrosion resistant structural aluminum alloy material
Diko The Aluminide Layers on the Titanium Alloy Prepared by Ion Cladding Process and Diffusion Annealing
JPS5487637A (en) Pressure pipe made of zirconium alloy
JPS5531130A (en) Heat treating method for ni alloy used in warm water
JPS5516701A (en) Method of manufacturing pneumatic cylinder
JPS5585665A (en) Coating method for iron or cast iron product with nickel and chromium

Legal Events

Date Code Title Description
EXPY Cancellation because of completion of term
FPAY Renewal fee payment (prs date is renewal date of database)

Free format text: PAYMENT UNTIL: 20080409

Year of fee payment: 15