JPS63186857A - 耐食アルミニウム合金製プレス製品の製造方法 - Google Patents
耐食アルミニウム合金製プレス製品の製造方法Info
- Publication number
- JPS63186857A JPS63186857A JP1662687A JP1662687A JPS63186857A JP S63186857 A JPS63186857 A JP S63186857A JP 1662687 A JP1662687 A JP 1662687A JP 1662687 A JP1662687 A JP 1662687A JP S63186857 A JPS63186857 A JP S63186857A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- aluminum alloy
- annealing
- corrosion
- corrosion resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1662687A JPS63186857A (ja) | 1987-01-27 | 1987-01-27 | 耐食アルミニウム合金製プレス製品の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1662687A JPS63186857A (ja) | 1987-01-27 | 1987-01-27 | 耐食アルミニウム合金製プレス製品の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63186857A true JPS63186857A (ja) | 1988-08-02 |
| JPH029102B2 JPH029102B2 (enExample) | 1990-02-28 |
Family
ID=11921560
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1662687A Granted JPS63186857A (ja) | 1987-01-27 | 1987-01-27 | 耐食アルミニウム合金製プレス製品の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63186857A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05287469A (ja) * | 1992-04-07 | 1993-11-02 | Sky Alum Co Ltd | 耐型かじり性、耐きず性、耐食性に優れたアルミニウム合金板の製法 |
| WO2006057452A1 (en) * | 2004-11-25 | 2006-06-01 | Showa Denko K.K. | Aluminum hot forged article, and method for producing the same |
| CN112342356A (zh) * | 2020-10-19 | 2021-02-09 | 西南铝业(集团)有限责任公司 | 一种2000系包铝合金退火铜扩散的生产工艺 |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4834103A (enExample) * | 1971-09-07 | 1973-05-16 | ||
| JPS5323548A (en) * | 1976-08-17 | 1978-03-04 | Toshiba Corp | Signal generator |
-
1987
- 1987-01-27 JP JP1662687A patent/JPS63186857A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4834103A (enExample) * | 1971-09-07 | 1973-05-16 | ||
| JPS5323548A (en) * | 1976-08-17 | 1978-03-04 | Toshiba Corp | Signal generator |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05287469A (ja) * | 1992-04-07 | 1993-11-02 | Sky Alum Co Ltd | 耐型かじり性、耐きず性、耐食性に優れたアルミニウム合金板の製法 |
| WO2006057452A1 (en) * | 2004-11-25 | 2006-06-01 | Showa Denko K.K. | Aluminum hot forged article, and method for producing the same |
| CN112342356A (zh) * | 2020-10-19 | 2021-02-09 | 西南铝业(集团)有限责任公司 | 一种2000系包铝合金退火铜扩散的生产工艺 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH029102B2 (enExample) | 1990-02-28 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR102428588B1 (ko) | 알루미늄계 도금 강판, 알루미늄계 도금 강판의 제조 방법 및 자동차용 부품의 제조 방법 | |
| KR102301116B1 (ko) | 부식에 대한 보호를 제공하는 금속성 코팅이 제공된 강 부품의 제조 방법, 및 강 부품 | |
| US20100294400A1 (en) | Method for producing a steel component by hot forming and steel component produced by hot forming | |
| CN111527233A (zh) | 热压成型用镀覆钢板、利用其的成型部件及其制造方法 | |
| EP2584059A1 (en) | Hot-dip al-coated steel sheet with excellent thermal blackening resistance and process for production of same | |
| CN100543170C (zh) | 具有良好耐蚀性的高强度淬火成形体及其生产方法 | |
| CN109112360A (zh) | 一种锌铝基镀层钢板及其制造方法、热成型方法和部件 | |
| CN111020296B (zh) | 宽热成形加热工艺窗口的Ni-Al-Si合金体系涂覆钢板及其制备和热冲压成形工艺 | |
| CN110965002B (zh) | 宽热成形加热工艺窗口的Mg-Al-Si合金体系涂覆钢板及其制备和热冲压成形工艺 | |
| US4861390A (en) | Method of manufacturing formable as-rolled thin steel sheets | |
| CN108842122B (zh) | 一种热浸镀镀层钢板及其制造方法 | |
| CN111041370A (zh) | 宽热成形加热工艺窗口的Cr-Al-Si合金体系涂覆钢板及其制备和热冲压成形工艺 | |
| EP4079928A2 (en) | Aluminum alloy-plated steel sheet having excellent workability and corrosion resistance and method for manufacturing same | |
| JP2002317258A (ja) | 加工後の耐食性に優れた溶融アルミめっき鋼板とその製造方法 | |
| AU2024394616A1 (en) | Zinc-aluminum-magnesium coated steel plate and manufacturing method therefor | |
| JP2003034854A (ja) | 高温プレス成形性に優れた溶融アルミめっき鋼板 | |
| JPH029102B2 (enExample) | ||
| US20250215519A1 (en) | Hot-stamped component having high cold-bending performance and high strength, and manufacturing method therefor | |
| JP2743228B2 (ja) | 加工性とめっき密着性に優れた溶融アルミめっきCr含有鋼板の製造方法 | |
| US2172422A (en) | Corrosion-resistant ferrous alloys | |
| US5795662A (en) | Zincate-treated article of Al-Mg-Si base alloy and method of manufacturing the same | |
| JPS6428349A (ja) | 不錆鋼を素地とするアルミニウムめつき被覆鋼板及び鋼箔の製造法 | |
| JP3002445B1 (ja) | 接合特性に優れた自動車燃料タンク用溶融Sn系めっき鋼板 | |
| JPH083671A (ja) | 成形性、溶接性、焼付け硬化性及び耐食性に優れるアルミニウム合金合わせ材とその製造方法 | |
| JP2724045B2 (ja) | 溶融亜鉛または亜鉛合金めっきクロム含有鋼板の製造方法 |