JPS6283425A - 表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法 - Google Patents
表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法Info
- Publication number
- JPS6283425A JPS6283425A JP22378185A JP22378185A JPS6283425A JP S6283425 A JPS6283425 A JP S6283425A JP 22378185 A JP22378185 A JP 22378185A JP 22378185 A JP22378185 A JP 22378185A JP S6283425 A JPS6283425 A JP S6283425A
- Authority
- JP
- Japan
- Prior art keywords
- steel sheet
- iron loss
- steel plate
- extremely low
- oriented electrical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/12—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of articles with special electromagnetic properties
- C21D8/1294—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of articles with special electromagnetic properties involving a localized treatment
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Materials Engineering (AREA)
- Thermal Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Electromagnetism (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Electroplating Methods And Accessories (AREA)
- Manufacturing Of Steel Electrode Plates (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22378185A JPS6283425A (ja) | 1985-10-09 | 1985-10-09 | 表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP22378185A JPS6283425A (ja) | 1985-10-09 | 1985-10-09 | 表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6283425A true JPS6283425A (ja) | 1987-04-16 |
| JPS6319574B2 JPS6319574B2 (enExample) | 1988-04-23 |
Family
ID=16803606
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP22378185A Granted JPS6283425A (ja) | 1985-10-09 | 1985-10-09 | 表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6283425A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH07258863A (ja) * | 1994-03-24 | 1995-10-09 | Sumitomo Metal Ind Ltd | 磁気特性の優れた電磁鋼板の製造方法 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60103124A (ja) * | 1983-11-09 | 1985-06-07 | Kawasaki Steel Corp | 歪取り焼鈍によって特性が劣化しない低鉄損の方向性けい素鋼板の製造方法 |
-
1985
- 1985-10-09 JP JP22378185A patent/JPS6283425A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS60103124A (ja) * | 1983-11-09 | 1985-06-07 | Kawasaki Steel Corp | 歪取り焼鈍によって特性が劣化しない低鉄損の方向性けい素鋼板の製造方法 |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH07258863A (ja) * | 1994-03-24 | 1995-10-09 | Sumitomo Metal Ind Ltd | 磁気特性の優れた電磁鋼板の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6319574B2 (enExample) | 1988-04-23 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP6915689B2 (ja) | 方向性電磁鋼板及びその製造方法 | |
| US4846939A (en) | Method for producing a grain-oriented electrical steel sheet having an ultra low watt loss | |
| JPS61235514A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS61284529A (ja) | 鉄損の極めて低い方向性電磁鋼板の製造方法 | |
| JPS6376819A (ja) | 低鉄損方向性電磁鋼板およびその製造方法 | |
| JPS6283425A (ja) | 表面性状が良好で鉄損の極めて低い方向性電磁鋼板の製造方法 | |
| JPS61133321A (ja) | 超低鉄損方向性電磁鋼板の製造方法 | |
| JPS6332849B2 (enExample) | ||
| JPS637333A (ja) | グラス皮膜特性のすぐれた低鉄損方向性電磁鋼板の製造方法 | |
| JPS6319568B2 (enExample) | ||
| JPS61201732A (ja) | 熱安定性、超低鉄損一方向性珪素鋼板の製造方法 | |
| JP3148093B2 (ja) | 鉄損の低い鏡面方向性電磁鋼板の製造方法 | |
| JPS6319573B2 (enExample) | ||
| JPH01309922A (ja) | 鉄損の低い一方向性電磁鋼板の製造方法 | |
| JPS6319572B2 (enExample) | ||
| JPS61186420A (ja) | 鉄損の極めて低い方向性電磁鋼板の製造方法 | |
| JPS6330968B2 (enExample) | ||
| JPH0730409B2 (ja) | 低鉄損一方向性珪素鋼板の製造方法 | |
| JPS61130421A (ja) | 超低鉄損方向性電磁鋼板の製造方法 | |
| JPS6319569B2 (enExample) | ||
| JPS62290844A (ja) | 超低鉄損一方向性けい素鋼板 | |
| JPS58144429A (ja) | 鉄損劣化のない一方向性珪素鋼板の製造方法 | |
| JPH0730410B2 (ja) | 低鉄損一方向性珪素鋼板の製造方法 | |
| JPS6396218A (ja) | 超低鉄損一方向性珪素鋼板の製造方法 | |
| JPS62124221A (ja) | 超低鉄損方向性電磁鋼板の製造方法 |