JPS624473B2 - - Google Patents
Info
- Publication number
- JPS624473B2 JPS624473B2 JP58012646A JP1264683A JPS624473B2 JP S624473 B2 JPS624473 B2 JP S624473B2 JP 58012646 A JP58012646 A JP 58012646A JP 1264683 A JP1264683 A JP 1264683A JP S624473 B2 JPS624473 B2 JP S624473B2
- Authority
- JP
- Japan
- Prior art keywords
- stainless steel
- annealing
- plating
- corrosion resistance
- thin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Electroplating Methods And Accessories (AREA)
- Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1264683A JPS59140390A (ja) | 1983-01-31 | 1983-01-31 | ステンレス薄板の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1264683A JPS59140390A (ja) | 1983-01-31 | 1983-01-31 | ステンレス薄板の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59140390A JPS59140390A (ja) | 1984-08-11 |
| JPS624473B2 true JPS624473B2 (OSRAM) | 1987-01-30 |
Family
ID=11811124
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1264683A Granted JPS59140390A (ja) | 1983-01-31 | 1983-01-31 | ステンレス薄板の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59140390A (OSRAM) |
Families Citing this family (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| FR2867991B1 (fr) * | 2004-03-25 | 2007-05-04 | Ugine Et Alz France Sa | Bandes en acier inoxydable austenitique d'aspect de surface mat |
| JP5995478B2 (ja) * | 2012-03-23 | 2016-09-21 | 日新製鋼株式会社 | 絶縁性の良好なステンレス鋼材およびその製造法 |
| JP6091145B2 (ja) * | 2012-10-10 | 2017-03-08 | 日新製鋼株式会社 | 表面改質ステンレス鋼板およびその製造方法 |
| JPWO2024195860A1 (OSRAM) * | 2023-03-22 | 2024-09-26 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4959048A (OSRAM) * | 1972-10-12 | 1974-06-07 | ||
| JPS5313335B2 (OSRAM) * | 1973-11-07 | 1978-05-09 |
-
1983
- 1983-01-31 JP JP1264683A patent/JPS59140390A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS59140390A (ja) | 1984-08-11 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| EP0565029B1 (en) | Grain oriented silicon steel sheet having low core loss and method of manufacturing same | |
| US3932236A (en) | Method for producing a super low watt loss grain oriented electrical steel sheet | |
| JPH04202630A (ja) | めっき密着性の良好な高Si含有高張力溶融亜鉛めっき鋼板の製造方法 | |
| CN110026433A (zh) | 一种提高含p高强if钢连退板表面质量的方法 | |
| JP2991928B2 (ja) | 加工性および耐食性に優れたCrーNi拡散処理鋼板とその製造方法 | |
| JPS624473B2 (OSRAM) | ||
| JPS624475B2 (OSRAM) | ||
| JP3277063B2 (ja) | 高張力熱延鋼板の溶融めっき方法 | |
| JPH04202631A (ja) | P含有高張力合金化溶融亜鉛めっき鋼板の製造方法 | |
| JPH02285057A (ja) | 溶融亜鉛めっき用鋼板の連続焼鈍方法 | |
| JPH0331798B2 (OSRAM) | ||
| JP6341382B2 (ja) | 方向性電磁鋼板とその製造方法 | |
| JP2787371B2 (ja) | めっき密着性および外観性に優れたアルミめっき鋼板の製造法 | |
| JPH0735586B2 (ja) | 着色フェライト系ステンレス鋼とその製造方法 | |
| JPS6028909B2 (ja) | 化成処理性に優れた鋼板 | |
| KR100720278B1 (ko) | Nb첨가 고 Cr 페라이트계 안정화 스테인리스강의 고속산세방법 | |
| JP4402886B2 (ja) | ホーロー密着性が著しく優れたホーロー用鋼板及びその製造方法並びにホーロー製品 | |
| JPH0474899A (ja) | 耐食性の優れたフェライト系ステンレス冷延鋼帯の製造方法 | |
| JP2002194494A (ja) | ほうろう用鋼板、その製造方法、ほうろう製品、およびその製造方法 | |
| EP1347070B1 (en) | Steel sheet for porcelain enameling and method for production thereof, and enameled product and method for production thereof | |
| JPS63230898A (ja) | 溶融めつき鋼板の製造法 | |
| JPS6328965B2 (OSRAM) | ||
| JPH11269539A (ja) | 脱スケール性に優れたオーステナイト系ステンレス鋼板の製造方法 | |
| JPH09279359A (ja) | 一方向性珪素鋼板の絶縁皮膜形成方法 | |
| JPS624474B2 (OSRAM) |