JPS6223930A - 高強度平歯車の製造方法 - Google Patents

高強度平歯車の製造方法

Info

Publication number
JPS6223930A
JPS6223930A JP16338385A JP16338385A JPS6223930A JP S6223930 A JPS6223930 A JP S6223930A JP 16338385 A JP16338385 A JP 16338385A JP 16338385 A JP16338385 A JP 16338385A JP S6223930 A JPS6223930 A JP S6223930A
Authority
JP
Japan
Prior art keywords
spur gear
forging
strength
upsetting
warm
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP16338385A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0535203B2 (enrdf_load_stackoverflow
Inventor
Wataru Takahashi
渉 高橋
Takashi Fukuda
隆 福田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP16338385A priority Critical patent/JPS6223930A/ja
Publication of JPS6223930A publication Critical patent/JPS6223930A/ja
Publication of JPH0535203B2 publication Critical patent/JPH0535203B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Preventing Corrosion Or Incrustation Of Metals (AREA)
  • Forging (AREA)
  • Solid-Phase Diffusion Into Metallic Material Surfaces (AREA)
  • Heat Treatment Of Steel (AREA)
  • Heat Treatment Of Articles (AREA)
JP16338385A 1985-07-23 1985-07-23 高強度平歯車の製造方法 Granted JPS6223930A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP16338385A JPS6223930A (ja) 1985-07-23 1985-07-23 高強度平歯車の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP16338385A JPS6223930A (ja) 1985-07-23 1985-07-23 高強度平歯車の製造方法

Publications (2)

Publication Number Publication Date
JPS6223930A true JPS6223930A (ja) 1987-01-31
JPH0535203B2 JPH0535203B2 (enrdf_load_stackoverflow) 1993-05-26

Family

ID=15772841

Family Applications (1)

Application Number Title Priority Date Filing Date
JP16338385A Granted JPS6223930A (ja) 1985-07-23 1985-07-23 高強度平歯車の製造方法

Country Status (1)

Country Link
JP (1) JPS6223930A (enrdf_load_stackoverflow)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6418545A (en) * 1987-07-14 1989-01-23 Honda Motor Co Ltd Method for forging gear
JPH01201423A (ja) * 1988-02-05 1989-08-14 Toyota Central Res & Dev Lab Inc 肌焼鋼強靭部品の製造方法
WO2008126939A1 (ja) 2007-04-11 2008-10-23 Nippon Steel Corporation 鍛造用鋼
CN104668433A (zh) * 2015-02-03 2015-06-03 江苏金源锻造股份有限公司 一种大齿轮的锻造工艺
CN104972037A (zh) * 2015-06-24 2015-10-14 陈文建 一种改善锻件表面质量的锻造工艺
CN104972036A (zh) * 2015-06-24 2015-10-14 陈文建 一种工件锻造工艺
CN107470528A (zh) * 2017-08-04 2017-12-15 钢铁研究总院 一种核电用SA508Gr.4N钢大锻件中心部位细化的锻造方法
CN107699671A (zh) * 2017-08-05 2018-02-16 周君 一种雪橇合金滑板用型钢

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6418545A (en) * 1987-07-14 1989-01-23 Honda Motor Co Ltd Method for forging gear
JPH01201423A (ja) * 1988-02-05 1989-08-14 Toyota Central Res & Dev Lab Inc 肌焼鋼強靭部品の製造方法
WO2008126939A1 (ja) 2007-04-11 2008-10-23 Nippon Steel Corporation 鍛造用鋼
EP2762593A1 (en) 2007-04-11 2014-08-06 Nippon Steel & Sumitomo Metal Corporation Forging steel
US9657379B2 (en) 2007-04-11 2017-05-23 Nippon Steel & Sumitomo Metal Corporation Forging steel
CN104668433A (zh) * 2015-02-03 2015-06-03 江苏金源锻造股份有限公司 一种大齿轮的锻造工艺
CN104972037A (zh) * 2015-06-24 2015-10-14 陈文建 一种改善锻件表面质量的锻造工艺
CN104972036A (zh) * 2015-06-24 2015-10-14 陈文建 一种工件锻造工艺
CN107470528A (zh) * 2017-08-04 2017-12-15 钢铁研究总院 一种核电用SA508Gr.4N钢大锻件中心部位细化的锻造方法
CN107699671A (zh) * 2017-08-05 2018-02-16 周君 一种雪橇合金滑板用型钢

Also Published As

Publication number Publication date
JPH0535203B2 (enrdf_load_stackoverflow) 1993-05-26

Similar Documents

Publication Publication Date Title
US6059898A (en) Induction hardening of heat treated gear teeth
JPH08311607A (ja) 歯元曲げ強度に優れた低歪浸炭歯車およびその製造方法
JP5729213B2 (ja) 熱間プレス部材の製造方法
JPS6043431B2 (ja) 軽荷重用窒化機械部品の製造法
JPH0325253B2 (enrdf_load_stackoverflow)
JPS6223930A (ja) 高強度平歯車の製造方法
JP4266341B2 (ja) 冷間鍛造性及び肌焼処理時の耐粗粒化特性に優れた球状化焼鈍省略肌焼用鋼及びその製造方法
CN105369259A (zh) 一种螺母板的加工方法
JP3550886B2 (ja) 被削性および疲労強度に優れた高周波焼入用の歯車用鋼材の製造方法
JPS5967365A (ja) 機械部品の製造方法
JP2000063935A (ja) 窒化部品の製造方法
JPH10226817A (ja) 軟窒化用鋼材の製造方法及びその鋼材を用いた軟窒化部品
JPS59126718A (ja) 冷間加工性に優れた鋼材の製造方法
JP3623313B2 (ja) 浸炭歯車部品
JP2614653B2 (ja) 熱処理歪の少ない浸炭部品の製造方法
JPH07138613A (ja) 熱処理鉄系焼結合金部品の製造方法
JP3109146B2 (ja) 低歪高強度部材の製造方法
JPH0754041A (ja) 冷間鍛造用鋼の製造方法
JP3077433B2 (ja) 浸炭歯車の加工−熱処理法
JPH0663080B2 (ja) 細粒組織を有する浸炭部品の製造方法
JPH02294450A (ja) プラスチック成型用金型鋼およびその製造方法
JPH03111551A (ja) 歯車の製造方法
KR100501680B1 (ko) 기어용 보론 합금강의 열처리 방법
JPS60262941A (ja) 温間鍛造用鋼
JPH0463261A (ja) 耐用性金型の製造方法