JPS62142722A - 溶接性に優れた高張力鋼の製造方法 - Google Patents
溶接性に優れた高張力鋼の製造方法Info
- Publication number
- JPS62142722A JPS62142722A JP28272885A JP28272885A JPS62142722A JP S62142722 A JPS62142722 A JP S62142722A JP 28272885 A JP28272885 A JP 28272885A JP 28272885 A JP28272885 A JP 28272885A JP S62142722 A JPS62142722 A JP S62142722A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- toughness
- strength
- welding
- weldability
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28272885A JPS62142722A (ja) | 1985-12-18 | 1985-12-18 | 溶接性に優れた高張力鋼の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP28272885A JPS62142722A (ja) | 1985-12-18 | 1985-12-18 | 溶接性に優れた高張力鋼の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62142722A true JPS62142722A (ja) | 1987-06-26 |
| JPH0570681B2 JPH0570681B2 (enExample) | 1993-10-05 |
Family
ID=17656269
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP28272885A Granted JPS62142722A (ja) | 1985-12-18 | 1985-12-18 | 溶接性に優れた高張力鋼の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62142722A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH07150300A (ja) * | 1993-10-22 | 1995-06-13 | Woojin Co Ltd | Fe−Mn系振動減衰合金鋼とその製造方法 |
| KR100325705B1 (ko) * | 1997-12-27 | 2002-06-26 | 이구택 | 고장력강의제조방법 |
| CN114717487A (zh) * | 2021-08-25 | 2022-07-08 | 哈尔滨工程大学 | 一种2700MPa级高塑韧性高耐蚀马氏体时效不锈钢及其制备方法 |
-
1985
- 1985-12-18 JP JP28272885A patent/JPS62142722A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH07150300A (ja) * | 1993-10-22 | 1995-06-13 | Woojin Co Ltd | Fe−Mn系振動減衰合金鋼とその製造方法 |
| KR100325705B1 (ko) * | 1997-12-27 | 2002-06-26 | 이구택 | 고장력강의제조방법 |
| CN114717487A (zh) * | 2021-08-25 | 2022-07-08 | 哈尔滨工程大学 | 一种2700MPa级高塑韧性高耐蚀马氏体时效不锈钢及其制备方法 |
| CN114717487B (zh) * | 2021-08-25 | 2023-03-31 | 哈尔滨工程大学 | 一种2700MPa级高塑韧性高耐蚀马氏体时效不锈钢及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0570681B2 (enExample) | 1993-10-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR0157540B1 (ko) | 용접부의 피로강도와 용접성이 뛰어난 고장력강 및 그 제조방법 | |
| JPH01230713A (ja) | 耐応力腐食割れ性の優れた高強度高靭性鋼の製造法 | |
| CN1989266B (zh) | 声各向异性小的焊接性优异的高强度钢板及其制造方法 | |
| JP7410438B2 (ja) | 鋼板 | |
| JP4751341B2 (ja) | 溶接熱影響部のctodが優れた鋼およびその製造方法 | |
| JPS5896853A (ja) | 耐食性および機械加工性に優れた極低温用高Mn鋼 | |
| JPS6033310A (ja) | 耐水素誘起割れ性及び耐硫化物応力腐食割れ性の優れた鋼板の製造方法 | |
| JPH0636993B2 (ja) | 耐食性および靭性に優れたステンレスクラッド鋼板の製造方法 | |
| JP2681591B2 (ja) | 耐食性と低温靱性に優れた複合鋼板の製造法 | |
| JPS62142726A (ja) | 溶接性の良好な耐摩耗用鋼板の製造法 | |
| JPS62142722A (ja) | 溶接性に優れた高張力鋼の製造方法 | |
| JP2020019995A (ja) | 厚鋼板およびその製造方法ならびに溶接構造物 | |
| JP2004323966A (ja) | 耐震性と溶接性に優れた鋼板およびその製造方法 | |
| JPS60181229A (ja) | 低降伏比高張力厚鋼板の製造法 | |
| JPS61104054A (ja) | ラインパイプ用高強度高靭性溶接クラツド鋼管 | |
| JP2004162076A (ja) | 溶接性および耐震性に優れた鋼板およびその製造方法 | |
| JPH0570682B2 (enExample) | ||
| JP2500019B2 (ja) | 溶接性の優れた570N/mm2級以上の低降伏比高張力鋼板 | |
| JP7281314B2 (ja) | クラッド鋼用母材、クラッド鋼およびクラッド鋼の製造方法 | |
| JPH06100933A (ja) | 溶接性に優れた構造物用高張力鋼の製造方法 | |
| JP3390234B2 (ja) | 大入熱溶接特性に優れた鋼材 | |
| JP3526702B2 (ja) | 溶接継手の疲労強度に優れた高張力溶接構造用鋼板及びその製造方法 | |
| JP3303672B2 (ja) | 耐溶融亜鉛めっき割れ性に優れた高張力鋼及びその製造方法 | |
| JPH04187713A (ja) | 溶接性に優れた高張力鋼構造物の製造方法 | |
| JPH04221015A (ja) | 高い降伏強度を有する鋼板の製造方法 |