JPS6129964B2 - - Google Patents
Info
- Publication number
- JPS6129964B2 JPS6129964B2 JP56065056A JP6505681A JPS6129964B2 JP S6129964 B2 JPS6129964 B2 JP S6129964B2 JP 56065056 A JP56065056 A JP 56065056A JP 6505681 A JP6505681 A JP 6505681A JP S6129964 B2 JPS6129964 B2 JP S6129964B2
- Authority
- JP
- Japan
- Prior art keywords
- polymer
- acrylamide
- temperature
- water content
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6505681A JPS57179204A (en) | 1981-04-28 | 1981-04-28 | Production of partially hydrolyzed acrylamide polymer |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6505681A JPS57179204A (en) | 1981-04-28 | 1981-04-28 | Production of partially hydrolyzed acrylamide polymer |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57179204A JPS57179204A (en) | 1982-11-04 |
JPS6129964B2 true JPS6129964B2 (enrdf_load_stackoverflow) | 1986-07-10 |
Family
ID=13275906
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6505681A Granted JPS57179204A (en) | 1981-04-28 | 1981-04-28 | Production of partially hydrolyzed acrylamide polymer |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57179204A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS59184203A (ja) * | 1983-04-04 | 1984-10-19 | Nitto Chem Ind Co Ltd | 部分加水分解されたアクリルアミド重合体の製造法 |
JP5705622B2 (ja) * | 2011-04-07 | 2015-04-22 | 三井化学株式会社 | 吸水性ポリマーから得られる新規なポリマー並びにその用途 |
Family Cites Families (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4917668B1 (enrdf_load_stackoverflow) * | 1970-12-19 | 1974-05-02 | ||
JPS4917668A (enrdf_load_stackoverflow) * | 1972-06-05 | 1974-02-16 | ||
JPS5615407B2 (enrdf_load_stackoverflow) * | 1973-07-30 | 1981-04-10 | ||
JPS50104292A (enrdf_load_stackoverflow) * | 1974-01-24 | 1975-08-18 | ||
JPS5918668B2 (ja) * | 1974-09-27 | 1984-04-28 | 株式会社横河電機製作所 | 指示電気計器の自動校正装置 |
JPS535295A (en) * | 1976-07-05 | 1978-01-18 | Mitsubishi Chem Ind Ltd | Preparation of partially hydrolyzed acrylamide polymer |
-
1981
- 1981-04-28 JP JP6505681A patent/JPS57179204A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS57179204A (en) | 1982-11-04 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4154910A (en) | Method for producing acrylamide polymers | |
US2960486A (en) | Polymer composition and method | |
US2831841A (en) | Treatment of acrylamide polymers | |
JPH0414684B2 (enrdf_load_stackoverflow) | ||
KR101384322B1 (ko) | 흡수성수지의 제조방법 | |
JPH06122707A (ja) | 吸水性樹脂の製造方法 | |
EP0520007A1 (en) | Process for purifying brominated polystyrene | |
JPS6129964B2 (enrdf_load_stackoverflow) | ||
NO140272B (no) | Fremgangsmaate for hindring av polymer-oppbygging ved fremstilling av vinylkloridpolymerer | |
JPH03115313A (ja) | 吸水性樹脂の製造方法 | |
JPS58219205A (ja) | アクリルアミド重合体の製造法 | |
US4535131A (en) | Process for producing partially hydrolyzed acrylamide polymer | |
US4482682A (en) | Process for preparing water-soluble, partially-hydrolyzed, solid acrylamide polymer | |
SU497781A3 (ru) | Способ получени сульфированных макросетчатых пористых сополимеров | |
JPH0214925B2 (enrdf_load_stackoverflow) | ||
JP4108491B2 (ja) | アクリルアミド系水溶性重合体の製造方法 | |
WO2004113398A1 (fr) | Procede ameliorant la resistance a la chaleur d'un copolymere d'ethylene/alcool vinylique | |
JPH0128762B2 (enrdf_load_stackoverflow) | ||
JP4744170B2 (ja) | 水溶性ビニルアミン重合体の製造方法 | |
RU2084462C1 (ru) | Способ получения порошкообразных акриловых сополимеров | |
JPS6239604A (ja) | アクリルアミド系重合体の製造法 | |
US4085045A (en) | Low molecular weight hydrolyzed polyacrylamide used as a scale inhibitor in water systems | |
JPH09302022A (ja) | 水溶性重合体の製造方法 | |
JPS588681B2 (ja) | 部分加水分解アクリルアミド系重合体の製造法 | |
US4551266A (en) | Treatment of substantially metallic ion free acrylamide and related compounds |