JPS61261030A - ガラス繊維強化樹脂成形板の連続製造方法 - Google Patents
ガラス繊維強化樹脂成形板の連続製造方法Info
- Publication number
- JPS61261030A JPS61261030A JP60103187A JP10318785A JPS61261030A JP S61261030 A JPS61261030 A JP S61261030A JP 60103187 A JP60103187 A JP 60103187A JP 10318785 A JP10318785 A JP 10318785A JP S61261030 A JPS61261030 A JP S61261030A
- Authority
- JP
- Japan
- Prior art keywords
- glass fiber
- resin molded
- molded plate
- water
- fiber reinforced
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Reinforced Plastic Materials (AREA)
- Laminated Bodies (AREA)
- Moulding By Coating Moulds (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60103187A JPS61261030A (ja) | 1985-05-15 | 1985-05-15 | ガラス繊維強化樹脂成形板の連続製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP60103187A JPS61261030A (ja) | 1985-05-15 | 1985-05-15 | ガラス繊維強化樹脂成形板の連続製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61261030A true JPS61261030A (ja) | 1986-11-19 |
| JPH0554418B2 JPH0554418B2 (enExample) | 1993-08-12 |
Family
ID=14347513
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60103187A Granted JPS61261030A (ja) | 1985-05-15 | 1985-05-15 | ガラス繊維強化樹脂成形板の連続製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61261030A (enExample) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR101851920B1 (ko) * | 2018-01-17 | 2018-04-27 | 주식회사에이피에스케미칼 | 페놀수지를 사용한 몰드 그레이팅의 제조방법 및 그로부터 제조된 몰드 그레이팅 |
Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS53124577A (en) * | 1977-04-06 | 1978-10-31 | Nippon Shokubai Kagaku Kogyo Co Ltd | Manufacture of glass-fiber reinforced resin board |
| JPS5465773A (en) * | 1977-11-07 | 1979-05-26 | Dainippon Ink & Chem Inc | Molding of reinforced plastic |
| JPS55103928A (en) * | 1979-01-31 | 1980-08-08 | Matsushita Electric Works Ltd | Production of plate of glass fiber-reinforced resin |
-
1985
- 1985-05-15 JP JP60103187A patent/JPS61261030A/ja active Granted
Patent Citations (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS53124577A (en) * | 1977-04-06 | 1978-10-31 | Nippon Shokubai Kagaku Kogyo Co Ltd | Manufacture of glass-fiber reinforced resin board |
| JPS5465773A (en) * | 1977-11-07 | 1979-05-26 | Dainippon Ink & Chem Inc | Molding of reinforced plastic |
| JPS55103928A (en) * | 1979-01-31 | 1980-08-08 | Matsushita Electric Works Ltd | Production of plate of glass fiber-reinforced resin |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR101851920B1 (ko) * | 2018-01-17 | 2018-04-27 | 주식회사에이피에스케미칼 | 페놀수지를 사용한 몰드 그레이팅의 제조방법 및 그로부터 제조된 몰드 그레이팅 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0554418B2 (enExample) | 1993-08-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4012267A (en) | Process for producing pultruded clad composites | |
| SU576027A3 (ru) | Способ изготовлени ориентированных слоистых пластиков | |
| US5032431A (en) | Glass fiber insulation binder | |
| JPS6296556A (ja) | 改良フェノール樹脂成形材料 | |
| CN109642138B (zh) | 粘结体系的硬化 | |
| JPS61261030A (ja) | ガラス繊維強化樹脂成形板の連続製造方法 | |
| JPS62259847A (ja) | 複合材料およびその製造法 | |
| US3215583A (en) | Integral structure | |
| JPH05501282A (ja) | プラスチツク含浸マツト及びその製造方法と使用 | |
| JPS5870760A (ja) | 硝子短繊維用バインダ−並びに硝子短繊維マツトの製造方法 | |
| DE2623738B2 (de) | Verfahren zur Herstellung von Bauteilen | |
| JPS6139901B2 (enExample) | ||
| FI72683C (fi) | Laminatprodukter bildade av fenolharts och innehaollande bor. | |
| CN1073506C (zh) | 刨花板表面覆层方法 | |
| JPH0462044A (ja) | 繊維強化フェノール樹脂発泡体及びその製造方法 | |
| JPS5920184A (ja) | スキ−の外表面を加工する方法 | |
| JPH01197539A (ja) | 構造材 | |
| KR820000686B1 (ko) | 무기섬유 복합보온판 제조방법 | |
| JPS63305146A (ja) | 繊維強化フェノール樹脂発泡体の製造方法 | |
| KR830001292B1 (ko) | 경질표피의 페놀수지품의 성형방법 | |
| US4355145A (en) | Furan resins of improved fire resistance | |
| JPH0438360A (ja) | 無機系パネル及びその製造方法 | |
| JPS58209560A (ja) | 建材用補強合成樹脂成型品 | |
| JPS5888162A (ja) | フイルム被覆繊維補強マグネシアセメントの連続成形方法 | |
| JPS6366939B2 (enExample) |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| EXPY | Cancellation because of completion of term |