JPS61253323A - フエライト系ステンレス冷延鋼帯の光輝焼鈍方法 - Google Patents
フエライト系ステンレス冷延鋼帯の光輝焼鈍方法Info
- Publication number
- JPS61253323A JPS61253323A JP9243485A JP9243485A JPS61253323A JP S61253323 A JPS61253323 A JP S61253323A JP 9243485 A JP9243485 A JP 9243485A JP 9243485 A JP9243485 A JP 9243485A JP S61253323 A JPS61253323 A JP S61253323A
- Authority
- JP
- Japan
- Prior art keywords
- steel strip
- stainless steel
- ferritic stainless
- bright annealing
- cold rolled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9243485A JPS61253323A (ja) | 1985-04-30 | 1985-04-30 | フエライト系ステンレス冷延鋼帯の光輝焼鈍方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9243485A JPS61253323A (ja) | 1985-04-30 | 1985-04-30 | フエライト系ステンレス冷延鋼帯の光輝焼鈍方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61253323A true JPS61253323A (ja) | 1986-11-11 |
| JPH02414B2 JPH02414B2 (enExample) | 1990-01-08 |
Family
ID=14054327
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP9243485A Granted JPS61253323A (ja) | 1985-04-30 | 1985-04-30 | フエライト系ステンレス冷延鋼帯の光輝焼鈍方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61253323A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01234595A (ja) * | 1988-03-16 | 1989-09-19 | Kawasaki Steel Corp | 耐銹性に優れた光輝焼鈍フェライト系ステンレス鋼帯の製造方法 |
| KR100436881B1 (ko) * | 1998-09-09 | 2004-09-08 | 주식회사 포스코 | 내식성이향상된오스테나이트계스테인레스강판의제조방법 |
| JP2007119856A (ja) * | 2005-10-28 | 2007-05-17 | Nisshin Steel Co Ltd | 親水性ステンレス鋼板及びその製造方法 |
-
1985
- 1985-04-30 JP JP9243485A patent/JPS61253323A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01234595A (ja) * | 1988-03-16 | 1989-09-19 | Kawasaki Steel Corp | 耐銹性に優れた光輝焼鈍フェライト系ステンレス鋼帯の製造方法 |
| KR100436881B1 (ko) * | 1998-09-09 | 2004-09-08 | 주식회사 포스코 | 내식성이향상된오스테나이트계스테인레스강판의제조방법 |
| JP2007119856A (ja) * | 2005-10-28 | 2007-05-17 | Nisshin Steel Co Ltd | 親水性ステンレス鋼板及びその製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH02414B2 (enExample) | 1990-01-08 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN109112283A (zh) | 低温高磁感取向硅钢的制备方法 | |
| JPS5558333A (en) | Production of non-aging cold rolled steel plate of superior deep-drawability through continuous heat treatment | |
| KR101696103B1 (ko) | 오스테나이트계 스테인리스강의 열처리 및 산세 방법 | |
| EP0523809A1 (en) | Method for hot-dip coating chromium-bearing steel | |
| JPS6043431A (ja) | 連続焼鈍による耐フル−チイング性のすぐれた軟質表面処理用鋼板の製造法 | |
| JP3915235B2 (ja) | 表面に模様のないオーステナイト系ステンレス鋼板の製造方法 | |
| CA1142068A (en) | Process for producing high strength cold rolled steel sheet having excellent paintability, weldability and workability | |
| JPH02414B2 (enExample) | ||
| US3335036A (en) | Deep drawing steel sheet and method for producing the same | |
| JPS6149706A (ja) | オ−ステナイト系ステンレス鋼薄板の製造方法 | |
| JPS60251227A (ja) | 低熱膨張Fe−Ni系鋼板の製造方法 | |
| JP3112195B2 (ja) | 耐酸化性に優れた研磨仕上げフェライト系ステンレス鋼板の製造方法 | |
| JPS5681629A (en) | Continuous annealing method of cold-rolled steel plate | |
| KR100276293B1 (ko) | 오스테나이트계 스텐레스 냉연강판의 광휘소둔방법 | |
| JPS6119688B2 (enExample) | ||
| RU1780884C (ru) | Способ изготовлени холоднокатаной нагартованной ленты дл производства биметаллических ленточных пил | |
| KR100466442B1 (ko) | 크롬계 스테인레스강 선재의 소둔방법 | |
| JP3572800B2 (ja) | オーステナイト系ステンレス熱延鋼板および冷延鋼板の製造方法 | |
| JP3120301B2 (ja) | ステンレス薄鋼板の製造方法 | |
| JP3451882B2 (ja) | 肌あれを生じないステンレス鋼の焼鈍方法 | |
| JPH09184012A (ja) | 表面光沢性および耐食性に優れるオーステナイト系ステンレス鋼板の製造方法 | |
| JPH02240216A (ja) | 一方向性電磁鋼板の良質一次絶縁皮膜形成方法 | |
| JPH0320407A (ja) | 高強度冷間圧延鋼板の粒界酸化防止方法 | |
| JPS6230823A (ja) | 耐スケ−ル性に優れた低Cr系ステンレス冷延鋼帯の焼鈍方法 | |
| JPS583924A (ja) | 冷延鋼板の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| S531 | Written request for registration of change of domicile |
Free format text: JAPANESE INTERMEDIATE CODE: R313531 |
|
| S533 | Written request for registration of change of name |
Free format text: JAPANESE INTERMEDIATE CODE: R313533 |
|
| R350 | Written notification of registration of transfer |
Free format text: JAPANESE INTERMEDIATE CODE: R350 |
|
| LAPS | Cancellation because of no payment of annual fees |