JPS61177353A - 耐摩耗性繊維強化金属型複合摺動部材 - Google Patents
耐摩耗性繊維強化金属型複合摺動部材Info
- Publication number
- JPS61177353A JPS61177353A JP1835285A JP1835285A JPS61177353A JP S61177353 A JPS61177353 A JP S61177353A JP 1835285 A JP1835285 A JP 1835285A JP 1835285 A JP1835285 A JP 1835285A JP S61177353 A JPS61177353 A JP S61177353A
- Authority
- JP
- Japan
- Prior art keywords
- wear
- alumina
- fibers
- composite material
- fiber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture Of Alloys Or Alloy Compounds (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1835285A JPS61177353A (ja) | 1985-01-31 | 1985-01-31 | 耐摩耗性繊維強化金属型複合摺動部材 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1835285A JPS61177353A (ja) | 1985-01-31 | 1985-01-31 | 耐摩耗性繊維強化金属型複合摺動部材 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS61177353A true JPS61177353A (ja) | 1986-08-09 |
| JPH0570688B2 JPH0570688B2 (en:Method) | 1993-10-05 |
Family
ID=11969282
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1835285A Granted JPS61177353A (ja) | 1985-01-31 | 1985-01-31 | 耐摩耗性繊維強化金属型複合摺動部材 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS61177353A (en:Method) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7170220B2 (en) | 2004-10-15 | 2007-01-30 | Dai Nippon Printing Co., Ltd. | Shadow mask with slots having a front side opening with an inclined from side edge |
| US7301267B2 (en) | 2004-10-18 | 2007-11-27 | Dai Nippon Printing Co., Ltd. | Shadow mask having a slot structure that permits electron beams to enter at increased angles |
| CN111575542A (zh) * | 2020-05-03 | 2020-08-25 | 上海工程技术大学 | 非晶增强铝合金复合材料及其制备方法 |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5893841A (ja) * | 1981-11-30 | 1983-06-03 | Toyota Motor Corp | 繊維強化金属型複合材料 |
-
1985
- 1985-01-31 JP JP1835285A patent/JPS61177353A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5893841A (ja) * | 1981-11-30 | 1983-06-03 | Toyota Motor Corp | 繊維強化金属型複合材料 |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US7170220B2 (en) | 2004-10-15 | 2007-01-30 | Dai Nippon Printing Co., Ltd. | Shadow mask with slots having a front side opening with an inclined from side edge |
| US7301267B2 (en) | 2004-10-18 | 2007-11-27 | Dai Nippon Printing Co., Ltd. | Shadow mask having a slot structure that permits electron beams to enter at increased angles |
| CN111575542A (zh) * | 2020-05-03 | 2020-08-25 | 上海工程技术大学 | 非晶增强铝合金复合材料及其制备方法 |
| CN111575542B (zh) * | 2020-05-03 | 2021-04-06 | 上海工程技术大学 | 非晶增强铝合金复合材料及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0570688B2 (en:Method) | 1993-10-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Matti et al. | Dry sliding wear behavior of mica, fly ash and red mud particles reinforced Al7075 alloy hybrid metal matrix composites | |
| JPS5893841A (ja) | 繊維強化金属型複合材料 | |
| JP3017764B2 (ja) | 耐摩耗複合ロール及びその製造法 | |
| CN113061796B (zh) | 一种铝合金表面铁基陶瓷复合材料、涂层及其制备方法 | |
| US20070218320A1 (en) | Metal matrix composites of aluminium, magnesium and titanium using silicon hexaboride, calcium hexaboride, silicon tetraboride, and calcium tetraboride | |
| CN111020360A (zh) | 一种非浸润型陶瓷颗粒增强钢铁基复合材料及其制备方法 | |
| JPS61177353A (ja) | 耐摩耗性繊維強化金属型複合摺動部材 | |
| US7160503B2 (en) | Metal matrix composites of aluminum, magnesium and titanium using silicon hexaboride, calcium hexaboride, silicon tetraboride, and calcium tetraboride | |
| JPS6263635A (ja) | Al−Sn−Pb系軸受合金 | |
| JPS62124244A (ja) | 繊維強化アルミニウム合金製ブレ−キロ−タおよびその製造法 | |
| JPH0635626B2 (ja) | アルミナ繊維・アルミナ−シリカ繊維強化金属複合材料 | |
| Sample et al. | High pressure squeeze casting of unidirectional graphite fiber reinforced aluminum matrix composites | |
| JPH08120367A (ja) | 耐摩耗性アルミニウム合金系複合材料 | |
| JPH01230738A (ja) | アルミニウム合金系複合材料の製造方法 | |
| Raju et al. | Fabrication and analysis of aluminium based metal matrix composites reinforced with aluminium oxide | |
| JPH04350136A (ja) | 繊維強化金属用繊維質成形体 | |
| GKarthikeyan | Evaluation of hardness of aluminium metal matrix composites at elevated temperature | |
| Tiwari et al. | Investigation of Mechanical and Tribological Properties of Aluminum Composite Reinforced by Boron Carbide, Silicon Carbide and Carbon Nanotubes | |
| JPH05106666A (ja) | アルミニウム合金製ブレーキドラム | |
| JPH04332A (ja) | スクロールコンプレッサ渦巻状部品材料 | |
| Li et al. | The Synergy Reinforcement Effect of Sm0. 85Zn0. 15MnO3 and ZrMgMo3O12 on Sm0. 85Zn0. 15MnO3-ZrMgMo3O12/Al-20Si Composites. Materials 2024, 17, 2494 | |
| Uguz et al. | Effect of Si-Content and Microstructure on the Wear Behaviour of Al-Si Alloys | |
| JPS63190127A (ja) | 摩擦摩耗特性及び強度に優れた金属基複合材料 | |
| JPS61194133A (ja) | 部材の組合せ | |
| JPH02209445A (ja) | グラファイト分散自己潤滑性合金 |