JPS61120897A - 固体潤滑膜および作製方法 - Google Patents

固体潤滑膜および作製方法

Info

Publication number
JPS61120897A
JPS61120897A JP24222484A JP24222484A JPS61120897A JP S61120897 A JPS61120897 A JP S61120897A JP 24222484 A JP24222484 A JP 24222484A JP 24222484 A JP24222484 A JP 24222484A JP S61120897 A JPS61120897 A JP S61120897A
Authority
JP
Japan
Prior art keywords
film
boron
solid lubricant
atomic beam
sputter
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP24222484A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0129400B2 (enExample
Inventor
Hiroki Kuwano
博喜 桑野
Fusao Shimokawa
房男 下川
Kazutoshi Nagai
一敏 長井
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NTT Inc
Original Assignee
Nippon Telegraph and Telephone Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Telegraph and Telephone Corp filed Critical Nippon Telegraph and Telephone Corp
Priority to JP24222484A priority Critical patent/JPS61120897A/ja
Publication of JPS61120897A publication Critical patent/JPS61120897A/ja
Publication of JPH0129400B2 publication Critical patent/JPH0129400B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Lubricants (AREA)
  • Physical Vapour Deposition (AREA)
JP24222484A 1984-11-19 1984-11-19 固体潤滑膜および作製方法 Granted JPS61120897A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP24222484A JPS61120897A (ja) 1984-11-19 1984-11-19 固体潤滑膜および作製方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP24222484A JPS61120897A (ja) 1984-11-19 1984-11-19 固体潤滑膜および作製方法

Publications (2)

Publication Number Publication Date
JPS61120897A true JPS61120897A (ja) 1986-06-07
JPH0129400B2 JPH0129400B2 (enExample) 1989-06-09

Family

ID=17086076

Family Applications (1)

Application Number Title Priority Date Filing Date
JP24222484A Granted JPS61120897A (ja) 1984-11-19 1984-11-19 固体潤滑膜および作製方法

Country Status (1)

Country Link
JP (1) JPS61120897A (enExample)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63195259A (ja) * 1987-02-06 1988-08-12 Sumitomo Electric Ind Ltd 二硫化モリブデン薄膜の形成方法
JPH01119683A (ja) * 1987-10-30 1989-05-11 Nissan Motor Co Ltd 固体潤滑被膜処理方法
JPH04266994A (ja) * 1991-02-21 1992-09-22 Nissan Motor Co Ltd 真空用潤滑部材
CN111876732A (zh) * 2020-06-17 2020-11-03 西安交通大学 一种硼氮化钼/硫化钼纳米复合涂层及其制备方法

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63195259A (ja) * 1987-02-06 1988-08-12 Sumitomo Electric Ind Ltd 二硫化モリブデン薄膜の形成方法
JPH01119683A (ja) * 1987-10-30 1989-05-11 Nissan Motor Co Ltd 固体潤滑被膜処理方法
JPH04266994A (ja) * 1991-02-21 1992-09-22 Nissan Motor Co Ltd 真空用潤滑部材
CN111876732A (zh) * 2020-06-17 2020-11-03 西安交通大学 一种硼氮化钼/硫化钼纳米复合涂层及其制备方法
CN111876732B (zh) * 2020-06-17 2023-06-06 西安交通大学 一种硼氮化钼/硫化钼纳米复合涂层及其制备方法

Also Published As

Publication number Publication date
JPH0129400B2 (enExample) 1989-06-09

Similar Documents

Publication Publication Date Title
US4364969A (en) Method of coating titanium and its alloys
US5181235A (en) Rotary-anode type x-ray tube
US20170169984A1 (en) Antiwetting coating for liquid metal
CN109504945A (zh) 一种空间环境用长效抗菌固体润滑膜层及其制备方法
US4834856A (en) Method and apparatus for sputtering a superconductor onto a substrate
KR20030035859A (ko) 저널 베어링용 은-함유 구리합금
US4917953A (en) Method of forming solid lubricaitng film on ceramic material and product produced by the same
JPH0129400B2 (enExample)
KR100762198B1 (ko) 고경도,고윤활성 피복재 및 그 피복방법
CN115058688B (zh) 一种复合润滑薄膜及其制备方法和应用
JPH0662978B2 (ja) 固体潤滑膜の作製方法
JP2875892B2 (ja) 立方晶窒化ほう素膜の形成方法
US4476000A (en) Method of making a magnetic film target for sputtering
US5013274A (en) Process for restoring locally damaged parts, particularly anticathodes
JPH046265A (ja) 鉄系合金基体への固体潤滑被膜の形成方法および固体潤滑被膜をもつ摺動部材
EP0352308B1 (en) Method of sputtering
RU2079571C1 (ru) Способ снижения трения и износа поверхностей изделий
US20070207338A1 (en) X-ray target and method for manufacturing same
JPS60197933A (ja) 磁気デイスク
JPH1121663A (ja) 耐摩耗性部材およびその製造方法
Kloss et al. Tribological properties of soft metallic coatings deposited by conventional and thermionically assisted triode ion plating
Bhattacharya et al. Co-implantation of Mo+ and S+ in Al2O3 and ZrO2 and their tribological properties
JP2518424B2 (ja) 磁気ヘッドおよびその製造方法
JP2000129420A (ja) 高温摺動部材用硬質膜
GB2065719A (en) Improvements in or relating to titanium and its alloys

Legal Events

Date Code Title Description
EXPY Cancellation because of completion of term