JPS604537A - 陰イオン交換膜の製法 - Google Patents
陰イオン交換膜の製法Info
- Publication number
- JPS604537A JPS604537A JP58111864A JP11186483A JPS604537A JP S604537 A JPS604537 A JP S604537A JP 58111864 A JP58111864 A JP 58111864A JP 11186483 A JP11186483 A JP 11186483A JP S604537 A JPS604537 A JP S604537A
- Authority
- JP
- Japan
- Prior art keywords
- anion exchange
- membrane
- group
- quaternary ammonium
- exchange membrane
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Manufacture Of Macromolecular Shaped Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58111864A JPS604537A (ja) | 1983-06-23 | 1983-06-23 | 陰イオン交換膜の製法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58111864A JPS604537A (ja) | 1983-06-23 | 1983-06-23 | 陰イオン交換膜の製法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS604537A true JPS604537A (ja) | 1985-01-11 |
| JPH0319863B2 JPH0319863B2 (enrdf_load_stackoverflow) | 1991-03-18 |
Family
ID=14572075
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58111864A Granted JPS604537A (ja) | 1983-06-23 | 1983-06-23 | 陰イオン交換膜の製法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS604537A (enrdf_load_stackoverflow) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62110704A (ja) * | 1985-11-11 | 1987-05-21 | Toyo Soda Mfg Co Ltd | フツ素系陰イオン交換膜を用いた酸・金属塩混合液からの酸の回収方法 |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP7260241B2 (ja) | 2020-04-13 | 2023-04-18 | アルプスアルパイン株式会社 | 取付物取付状態の管理システム |
-
1983
- 1983-06-23 JP JP58111864A patent/JPS604537A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62110704A (ja) * | 1985-11-11 | 1987-05-21 | Toyo Soda Mfg Co Ltd | フツ素系陰イオン交換膜を用いた酸・金属塩混合液からの酸の回収方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0319863B2 (enrdf_load_stackoverflow) | 1991-03-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Kim et al. | Single-step synthesis of proton conducting poly (vinylidene fluoride)(PVDF) graft copolymer electrolytes | |
| CN100417677C (zh) | 通过电子束交联的溴、氯或碘官能聚合物电解质 | |
| JP4718010B2 (ja) | 架橋イオン伝導性膜 | |
| US6765027B2 (en) | Ion-exchange materials with improved ion conductivity | |
| CN100468852C (zh) | 通过芳香砜交联的聚合物电解质 | |
| US3684747A (en) | Method for increasing the liquid absorptive capacity of linear fluorocarbon sulfonic acid polymer | |
| JP5025971B2 (ja) | 複合イオノマー膜 | |
| CN108586745B (zh) | 一种基于氟化聚苯并咪唑的阴离子交换膜及其制备方法 | |
| JP2007516324A (ja) | 架橋ポリマー | |
| JP2004079252A (ja) | 高耐久性固体高分子電解質及びそれを用いた固体高分子電解質(複合)膜 | |
| CN102272177A (zh) | 新型互穿聚合物网络及其用途 | |
| Park et al. | Proton-conducting nanocomposite membranes based on P (VDF-co-CTFE)-g-PSSA graft copolymer and TiO2–PSSA nanoparticles | |
| JPS604537A (ja) | 陰イオン交換膜の製法 | |
| JP4743680B2 (ja) | リン酸基/フッ素基/スルホン酸基含有固体高分子電解質膜及び用途 | |
| JPS609053B2 (ja) | 陽イオン交換膜の製造方法 | |
| JP3423765B2 (ja) | イオン交換膜の積層方法 | |
| US3840634A (en) | Vinyl heterocyclic copolymers,semipermeable membranes from said copolymers and method for preparing said membranes | |
| JPS61185507A (ja) | 陰イオン交換体の製造方法 | |
| JP3846843B2 (ja) | バナジウム系レドックスフロー電池用隔膜の製造方法 | |
| KR100473351B1 (ko) | 폴리에틸렌/폴리스티렌 양이온교환막의 제조방법 | |
| JP2005112985A (ja) | 疎水性ブロックを有するスルホン化ポリマーおよび固体高分子電解質 | |
| US9184459B2 (en) | Sulfonated polymers useful for forming fuel cell membranes | |
| RU2797133C1 (ru) | Протонпроводящие полимерные мембраны и способ их получения | |
| JP2004087137A (ja) | 燃料電池用固体高分子電解質膜 | |
| JP4080925B2 (ja) | 高分子電解質およびプロトン伝導膜 |