JPS60141389A - 貴金属複合材料 - Google Patents
貴金属複合材料Info
- Publication number
- JPS60141389A JPS60141389A JP24503783A JP24503783A JPS60141389A JP S60141389 A JPS60141389 A JP S60141389A JP 24503783 A JP24503783 A JP 24503783A JP 24503783 A JP24503783 A JP 24503783A JP S60141389 A JPS60141389 A JP S60141389A
- Authority
- JP
- Japan
- Prior art keywords
- materials
- layers
- powder
- alone
- durability
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
本発明は、工業用等に用いて有用外貨金属の複合旧41
」に関する。
」に関する。
PL、 Pt−Rh、 Pt−Ir、 Pt−Ru 、
Pt−Au 。
Pt−Au 。
pt−wは高温における化学的安定性が良い性質を有し
ている為に、化学機械羽村や常温から高温まで広い温度
領域で腐食性物質と接触する部分に多用されている。
ている為に、化学機械羽村や常温から高温まで広い温度
領域で腐食性物質と接触する部分に多用されている。
しかし、」−記の様な利子lば*1j]/J穎直にビン
ポールやブローホールが発生し易く、これ舌の内部欠陥
を無くすこと1l−i極めて困難であり、4た製品’k
:’;:J温で使用していると、結晶粒が粗大し 白
玉や他の物質の重量を受けて徐々に変形するが、このと
きビンポールやブローホール等の内部欠陥にLiol、
力が伝わって、マイクロクランクの発生が」−じ、11
.7間の経jfMと共に遂には割れに寸で発展すること
と々る。
ポールやブローホールが発生し易く、これ舌の内部欠陥
を無くすこと1l−i極めて困難であり、4た製品’k
:’;:J温で使用していると、結晶粒が粗大し 白
玉や他の物質の重量を受けて徐々に変形するが、このと
きビンポールやブローホール等の内部欠陥にLiol、
力が伝わって、マイクロクランクの発生が」−じ、11
.7間の経jfMと共に遂には割れに寸で発展すること
と々る。
そこで本発明は上記の欠点をIQ!(決することを目的
とし、Pt、Pt−Rh、Pt−Ir、Pt−Rtj、
Pt−Au、Pt−Wの単独−または2種以−にの層間
にW粉末を介在させて積層し、複合して一体にすること
を特徴とする4、 以下に本発明の一実施例を図面に従って述へると、Pt
インゴットを熱間鍛造し、圧延を11なって薄い相料と
する。この様にしたs4::1の層間にW粉末を介在さ
せ所望枚数重ね合せて熱間圧危を1工なって希望寸法に
加工し、更に用途に応じ/ζ形状に製作するものである
。
とし、Pt、Pt−Rh、Pt−Ir、Pt−Rtj、
Pt−Au、Pt−Wの単独−または2種以−にの層間
にW粉末を介在させて積層し、複合して一体にすること
を特徴とする4、 以下に本発明の一実施例を図面に従って述へると、Pt
インゴットを熱間鍛造し、圧延を11なって薄い相料と
する。この様にしたs4::1の層間にW粉末を介在さ
せ所望枚数重ね合せて熱間圧危を1工なって希望寸法に
加工し、更に用途に応じ/ζ形状に製作するものである
。
なお、」−記実施例はptを用いだが他にpt−Rh、
Pt−1r、PL−Ru、Pt−Au、Pt−W の単
独1だはptを含めた2種以上の層間にW粉末を介在さ
せてもよい。
Pt−1r、PL−Ru、Pt−Au、Pt−W の単
独1だはptを含めた2種以上の層間にW粉末を介在さ
せてもよい。
以」二による本発明の貴金属羽村は機械的強度が同寸法
の従来品より増太し、特に高温耐久性が著しく向上する
が、これは以下の理由と考えられる。
の従来品より増太し、特に高温耐久性が著しく向上する
が、これは以下の理由と考えられる。
金属は、温度の上昇とともに徐々に膨張が起シ、更に加
熱を続け、融点を越えると急激に容積が増大する。また
溶融した金属は多量のガスを吸収して更に容積の増加傾
向を助長するが、鋳造時は逆に吸蔵ガスを放出しながら
同化収縮する。この冷却過程における収縮や放出ガスに
よって生ずる収縮孔、ピンホールやブローホール等の欠
陥がインゴット内に不規則に散在し、一般的鋳造法でこ
れら内部欠陥を完全に排除することは不可能と云える。
熱を続け、融点を越えると急激に容積が増大する。また
溶融した金属は多量のガスを吸収して更に容積の増加傾
向を助長するが、鋳造時は逆に吸蔵ガスを放出しながら
同化収縮する。この冷却過程における収縮や放出ガスに
よって生ずる収縮孔、ピンホールやブローホール等の欠
陥がインゴット内に不規則に散在し、一般的鋳造法でこ
れら内部欠陥を完全に排除することは不可能と云える。
またこれら内部欠陥は発生機構上局部に集中する傾向が
あるため、そこに応力が加わったり、腐蝕性物質と接触
した場合、割れや腐蝕孔に発展する。
あるため、そこに応力が加わったり、腐蝕性物質と接触
した場合、割れや腐蝕孔に発展する。
本発明は上述の如ぐこれら内部欠陥がイf存するインゴ
ットを熱間鍛造し、圧延を行なって薄くし多数枚重ねて
複合することによって第2図に7]eず如く各層の集中
欠陥を分散せしめその結果として第1図に示す様な割れ
や腐食が後わtの層によって喰い止められることとなる
。加えて本発明による材料を再結晶温度以上で使用した
場合、結晶の成長は4各層間で抑制される為、全体が微
結晶質となり、高温強度が著しく向上するものである。
ットを熱間鍛造し、圧延を行なって薄くし多数枚重ねて
複合することによって第2図に7]eず如く各層の集中
欠陥を分散せしめその結果として第1図に示す様な割れ
や腐食が後わtの層によって喰い止められることとなる
。加えて本発明による材料を再結晶温度以上で使用した
場合、結晶の成長は4各層間で抑制される為、全体が微
結晶質となり、高温強度が著しく向上するものである。
以上の様な理由により本発明による貴金属月別は耐久性
1機械的強度にすぐれた性質を有する旧料となるもので
ある。
1機械的強度にすぐれた性質を有する旧料となるもので
ある。
第1図は金属材料が割れて発展する状i、11Aを示す
拡大説明図、第2図は本発明の状態を示す拡大説明図で
ある。 特許出願人 株式会社徳力本店 代理人弁理士 金 倉 喬 二
拡大説明図、第2図は本発明の状態を示す拡大説明図で
ある。 特許出願人 株式会社徳力本店 代理人弁理士 金 倉 喬 二
Claims (1)
- 【特許請求の範囲】 」 熱間圧延または冷間圧延を行なって薄くしたPt、
Pt−Rh、Pt−Ir、Pt−Ru、Pt−Au 。 pt−wの単独または2種以上の層間にW粉末を介在さ
せたと記材料を複数枚重ね、熱間圧着。 冷間圧着または拡散接合等によって複合加工して所定の
厚みとし、各層間における再結晶の成長を抑制すると共
に各層における内部欠陥同士が合致しない様にしたこと
を![1″徴とする貴金属複合4)料。