JPS594989A - 配管溶接部の残留応力改善方法 - Google Patents
配管溶接部の残留応力改善方法Info
- Publication number
- JPS594989A JPS594989A JP11201482A JP11201482A JPS594989A JP S594989 A JPS594989 A JP S594989A JP 11201482 A JP11201482 A JP 11201482A JP 11201482 A JP11201482 A JP 11201482A JP S594989 A JPS594989 A JP S594989A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- tube
- residual stress
- stress
- welded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23K—SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23K31/00—Processes relevant to this subclass, specially adapted for particular articles or purposes, but not covered by only one of the preceding main groups
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11201482A JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP11201482A JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS594989A true JPS594989A (ja) | 1984-01-11 |
| JPS6219276B2 JPS6219276B2 (cg-RX-API-DMAC7.html) | 1987-04-27 |
Family
ID=14575807
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP11201482A Granted JPS594989A (ja) | 1982-06-29 | 1982-06-29 | 配管溶接部の残留応力改善方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS594989A (cg-RX-API-DMAC7.html) |
-
1982
- 1982-06-29 JP JP11201482A patent/JPS594989A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6219276B2 (cg-RX-API-DMAC7.html) | 1987-04-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7866166B2 (en) | Method for improving residual stress in pipe and apparatus | |
| JPS5950730B2 (ja) | オ−ステナイト系ステンレス鋼管などの残留応力の改善方法 | |
| JPH0724577A (ja) | クラッド管の突合せ溶接方法 | |
| JPS594989A (ja) | 配管溶接部の残留応力改善方法 | |
| US4608101A (en) | Method for heat treating pipe with double-pipe section | |
| JP2008132511A (ja) | 劣化部の再生方法、劣化部の再生装置 | |
| US4588869A (en) | Method for relieving residual stresses by controlling weld heat input | |
| JPS6018293A (ja) | オ−ステナイト系ステンレス鋼の多層盛溶接方法 | |
| JPS61170516A (ja) | 金属管の残留応力改善方法 | |
| JPS60135526A (ja) | 二重管溶接部の熱処理方法 | |
| JPH038568A (ja) | 金属管の応力腐食割れ改善方法 | |
| JPS5852428A (ja) | 軸の応力改善熱処理法 | |
| JP2500165B2 (ja) | 燃料被覆管の製造方法 | |
| JPS62207825A (ja) | 二重円筒状配管の熱処理法 | |
| JPH06182578A (ja) | 配管の溶接方法及び装置 | |
| US2221209A (en) | Method of making jacketed rods and the like | |
| JPS61144590A (ja) | バイメタル部品 | |
| JPS6234630A (ja) | ライニング管およびその製造方法 | |
| JPH03146620A (ja) | 金属管の残留応力改善方法 | |
| JPH04127993A (ja) | 容器貫通管取り付け溶接部の応力改善方法 | |
| JPS6031088A (ja) | 核燃料複合被覆管 | |
| JPS6024234A (ja) | 管端接合構造 | |
| JPS63143221A (ja) | 二重金属管等の残留応力改善方法 | |
| JPS6310081A (ja) | ステンレス鋼の応力腐食割れ防止溶接法 | |
| JPH05169255A (ja) | 管と管の溶接法 |