JPS59184456A - 密閉形鉛蓄電池の化成方法 - Google Patents
密閉形鉛蓄電池の化成方法Info
- Publication number
- JPS59184456A JPS59184456A JP58058150A JP5815083A JPS59184456A JP S59184456 A JPS59184456 A JP S59184456A JP 58058150 A JP58058150 A JP 58058150A JP 5815083 A JP5815083 A JP 5815083A JP S59184456 A JPS59184456 A JP S59184456A
- Authority
- JP
- Japan
- Prior art keywords
- electrolyte
- forming
- amount
- electrode plate
- chemical
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/14—Electrodes for lead-acid accumulators
- H01M4/16—Processes of manufacture
- H01M4/22—Forming of electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P70/00—Climate change mitigation technologies in the production process for final industrial or consumer products
- Y02P70/50—Manufacturing or production processes characterised by the final manufactured product
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58058150A JPS59184456A (ja) | 1983-04-01 | 1983-04-01 | 密閉形鉛蓄電池の化成方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58058150A JPS59184456A (ja) | 1983-04-01 | 1983-04-01 | 密閉形鉛蓄電池の化成方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59184456A true JPS59184456A (ja) | 1984-10-19 |
| JPH0472352B2 JPH0472352B2 (enrdf_load_stackoverflow) | 1992-11-18 |
Family
ID=13075956
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58058150A Granted JPS59184456A (ja) | 1983-04-01 | 1983-04-01 | 密閉形鉛蓄電池の化成方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59184456A (enrdf_load_stackoverflow) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2002216839A (ja) * | 2001-01-17 | 2002-08-02 | Furukawa Battery Co Ltd:The | 鉛蓄電池の電槽化成方法 |
-
1983
- 1983-04-01 JP JP58058150A patent/JPS59184456A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2002216839A (ja) * | 2001-01-17 | 2002-08-02 | Furukawa Battery Co Ltd:The | 鉛蓄電池の電槽化成方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0472352B2 (enrdf_load_stackoverflow) | 1992-11-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Hullmeine et al. | Effect of previous charge/discharge history on the capacity of the PbO2/PbSO4 electrode: the hysteresis or memory effect | |
| JP4224729B2 (ja) | 密閉形鉛蓄電池およびその製造方法 | |
| JPS59184456A (ja) | 密閉形鉛蓄電池の化成方法 | |
| JP4081698B2 (ja) | 鉛蓄電池の充電方法 | |
| JPS60143570A (ja) | 鉛蓄電池 | |
| JPS59184457A (ja) | 密閉形鉛蓄電池の化成方法 | |
| JPH0815075B2 (ja) | 密閉形鉛蓄電池の化成方法 | |
| JPH01302661A (ja) | 鉛蓄電池およびその製造法 | |
| JPS62145664A (ja) | 密閉型鉛蓄電池の製造法 | |
| JPH01149376A (ja) | 密閉型鉛蓄電池 | |
| JPH0193066A (ja) | 密閉形鉛蓄電池の製造法 | |
| JPH0443570A (ja) | 密閉形鉛蓄電池の製造方法 | |
| JPS59157966A (ja) | 密閉形鉛蓄電池 | |
| JPS6065458A (ja) | 鉛蓄電池用電極の製造法 | |
| JPH01117270A (ja) | 鉛蓄電池陽極板の製造方法 | |
| JPH10134810A (ja) | 鉛蓄電池の製造方法 | |
| JPS6321761A (ja) | 密閉形鉛蓄電池 | |
| JPS63211574A (ja) | 密閉形鉛蓄電池 | |
| JP2004199913A (ja) | 制御弁式鉛蓄電池の製造方法 | |
| JPS63187572A (ja) | 密閉式鉛蓄電池 | |
| JPH03163755A (ja) | クラッド式密閉形鉛電池 | |
| JPS61151972A (ja) | ペ−スト式鉛蓄電池 | |
| JPS58209063A (ja) | 鉛蓄電池用極板の製造法 | |
| JP2004111291A (ja) | 制御弁式鉛蓄電池の電槽化成後の処理方法 | |
| JPS59186254A (ja) | 鉛蓄電池の製造方法 |