JPS5874553A - 水蒸気養生軽量気泡コンクリ−トの製造法 - Google Patents
水蒸気養生軽量気泡コンクリ−トの製造法Info
- Publication number
- JPS5874553A JPS5874553A JP16958381A JP16958381A JPS5874553A JP S5874553 A JPS5874553 A JP S5874553A JP 16958381 A JP16958381 A JP 16958381A JP 16958381 A JP16958381 A JP 16958381A JP S5874553 A JPS5874553 A JP S5874553A
- Authority
- JP
- Japan
- Prior art keywords
- raw materials
- weight
- calcium carbonate
- steam
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Porous Artificial Stone Or Porous Ceramic Products (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP16958381A JPS5874553A (ja) | 1981-10-23 | 1981-10-23 | 水蒸気養生軽量気泡コンクリ−トの製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP16958381A JPS5874553A (ja) | 1981-10-23 | 1981-10-23 | 水蒸気養生軽量気泡コンクリ−トの製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5874553A true JPS5874553A (ja) | 1983-05-06 |
| JPS6144835B2 JPS6144835B2 (enrdf_load_stackoverflow) | 1986-10-04 |
Family
ID=15889164
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP16958381A Granted JPS5874553A (ja) | 1981-10-23 | 1981-10-23 | 水蒸気養生軽量気泡コンクリ−トの製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5874553A (enrdf_load_stackoverflow) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3633471A1 (de) * | 1985-10-01 | 1987-04-02 | Sumitomo Metal Mining Co | Verfahren zur herstellung von autoklavengehaertetem gasleichtbeton |
| JPS6278173A (ja) * | 1985-10-01 | 1987-04-10 | 住友金属鉱山株式会社 | Alcの製造方法 |
| JPS62162679A (ja) * | 1986-01-14 | 1987-07-18 | 住友金属鉱山株式会社 | 水蒸気養生軽量気泡コンクリ−トの製造法 |
| EP2824086B1 (de) | 2013-07-12 | 2016-11-09 | Xella Baustoffe GmbH | Hydrothermal gehärtetes Poren- oder Schaumbetonmaterial sowie Verfahren zu dessen Herstellung |
-
1981
- 1981-10-23 JP JP16958381A patent/JPS5874553A/ja active Granted
Cited By (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3633471A1 (de) * | 1985-10-01 | 1987-04-02 | Sumitomo Metal Mining Co | Verfahren zur herstellung von autoklavengehaertetem gasleichtbeton |
| JPS6278173A (ja) * | 1985-10-01 | 1987-04-10 | 住友金属鉱山株式会社 | Alcの製造方法 |
| JPS62162679A (ja) * | 1986-01-14 | 1987-07-18 | 住友金属鉱山株式会社 | 水蒸気養生軽量気泡コンクリ−トの製造法 |
| EP2824086B1 (de) | 2013-07-12 | 2016-11-09 | Xella Baustoffe GmbH | Hydrothermal gehärtetes Poren- oder Schaumbetonmaterial sowie Verfahren zu dessen Herstellung |
| EP3100991B1 (de) | 2013-07-12 | 2017-09-13 | Xella Baustoffe GmbH | Verfahren zur herstellung eines hydrothermal gehärteten poren- oder schaumbetonformkörpers |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6144835B2 (enrdf_load_stackoverflow) | 1986-10-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4464353A (en) | Quicklime slaking process | |
| JPH05238792A (ja) | 再生骨材の製造方法および再生骨材 | |
| CN112592145A (zh) | 一种早强磷石膏膨胀砂浆的制备方法 | |
| CN105948639A (zh) | 一种高强低收缩抗裂路面基层材料 | |
| JPH06144944A (ja) | 多孔質珪酸カルシウム水和物の炭酸化処理方法 | |
| JPS5874553A (ja) | 水蒸気養生軽量気泡コンクリ−トの製造法 | |
| US4781760A (en) | Method for improving the properties of cement mortar and concrete | |
| US7537653B2 (en) | Microsilica materials with improved pozzolanic activity | |
| TWI753785B (zh) | 膠結材料製造方法 | |
| JPS63199283A (ja) | 水硬性微粉末を用いた固化材 | |
| JP3020143B2 (ja) | 脱硫剤の製造方法 | |
| JP4561190B2 (ja) | 処理対象土の固化処理方法 | |
| CN112225485A (zh) | 晶核剂、铜尾矿蒸压加气混凝土制品、制备方法、应用 | |
| US1282188A (en) | Oxysalt composition and process of making the same. | |
| JP3007905B2 (ja) | 土壌改良方法 | |
| JP2753194B2 (ja) | 地盤改良材および地盤改良方法 | |
| JP3104036B2 (ja) | 静的破壊剤 | |
| CN115557723B (zh) | 一种硅酸钙盐晶种胶体及其制备方法 | |
| CN110066697A (zh) | 一种粉煤制无水添加高强度冷态型煤的制备方法 | |
| JP3520561B2 (ja) | 珪酸二石灰微粉末の製造方法 | |
| TWI675813B (zh) | 可安定化具膨脹特性資材的資源化方法 | |
| JPS62265160A (ja) | Alcの製造方法 | |
| CA1206980A (en) | Conversion of fluoroanhydrite to plaster | |
| CN117945683A (zh) | 一种利用粉煤灰制备纳米水化硅酸钙晶种早强剂的制备方法及其应用 | |
| CN117361916A (zh) | 一种适用于低碳建材的超细低碳胶凝材料及其制备方法 |