JPS57167885A - Shot blasting method for hull's shell plating - Google Patents
Shot blasting method for hull's shell platingInfo
- Publication number
- JPS57167885A JPS57167885A JP56051593A JP5159381A JPS57167885A JP S57167885 A JPS57167885 A JP S57167885A JP 56051593 A JP56051593 A JP 56051593A JP 5159381 A JP5159381 A JP 5159381A JP S57167885 A JPS57167885 A JP S57167885A
- Authority
- JP
- Japan
- Prior art keywords
- hull
- shot blasting
- approximately
- resistance
- shell plating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To save expenses required for hull's shot blasting and contrive reduction of resistance to the hull by means of applying shot blasting only on the shell plating at lower level than the load water line for the range as far as the hull's shell plating asperity covers almost one fourth of the ship's length from the bow end which greatly contributes to the hull's resistance. CONSTITUTION:Shot blasting is applied only on the shell plating at lower level than the load water line for the range 2 as far as it is approximately one fourth of the ship's length from the bow end which is part of the hull recognized as that the hull's shell plating asperity greatly contributes to the increased in the hull's resistance, and the shot blasting is not applied for other hull's parts. Thus, necessary expenses for applying the shot blasting can be widely reduced to approximately one fourth, and approximately 43% of the increase in the hull's resistance can be lessened. Further, as to the range not alone at the bow part but also as far as it is approximately one fourth from the stern, if the shot blasting is applied, the increase in the hull's resistance can be reduced as much as approximately 70%.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP56051593A JPS57167885A (en) | 1981-04-06 | 1981-04-06 | Shot blasting method for hull's shell plating |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP56051593A JPS57167885A (en) | 1981-04-06 | 1981-04-06 | Shot blasting method for hull's shell plating |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS57167885A true JPS57167885A (en) | 1982-10-15 |
Family
ID=12891204
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP56051593A Pending JPS57167885A (en) | 1981-04-06 | 1981-04-06 | Shot blasting method for hull's shell plating |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS57167885A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2555119A1 (en) * | 1983-11-17 | 1985-05-24 | Nippon Oils & Fats Co Ltd | Method of treating the surface of the hull of a commissioned ship |
WO1991001247A1 (en) * | 1989-07-25 | 1991-02-07 | Hans Willi Velke | Fluid dynamic surfaces |
-
1981
- 1981-04-06 JP JP56051593A patent/JPS57167885A/en active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2555119A1 (en) * | 1983-11-17 | 1985-05-24 | Nippon Oils & Fats Co Ltd | Method of treating the surface of the hull of a commissioned ship |
WO1991001247A1 (en) * | 1989-07-25 | 1991-02-07 | Hans Willi Velke | Fluid dynamic surfaces |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
RU95105892A (en) | Ship's hull | |
JPS57167885A (en) | Shot blasting method for hull's shell plating | |
GB1311935A (en) | Floating hulls | |
JPS57167893A (en) | Cleaning method for hull's shell plating | |
GB893153A (en) | Ship's hull formation | |
ES472020A1 (en) | Ships' hulls | |
GB1141954A (en) | Improvements in or relating to the bows of ships | |
JPS5253387A (en) | Ship | |
JPS5568497A (en) | Method of removing marine living thing adhered on ship body and apparatus thereof | |
JPS5758584A (en) | Shape of bow of chunky ship | |
GB1309753A (en) | Transverse propulsion units for ships | |
JPS6412993A (en) | Bow wave reducer for ship | |
ES8502040A1 (en) | Barge carrying vessel. | |
GB1056033A (en) | Improved form of bow for ships | |
JPS5643090A (en) | Dirt preventive method of ship body | |
JPS57982A (en) | Bows shape of craft made of fiber-reinforced plastic | |
JPS5247297A (en) | Controlling method of longitudinal strength of ship body during cargo handling operation of the ship | |
JPS5559081A (en) | Ship | |
GB826155A (en) | Improvements in and relating to the hull form of tug boats and towing vessels | |
JPS5470587A (en) | Floating matter recovery boat | |
GB878345A (en) | Stern bulb or blister for single-screw ships | |
JPS57107990A (en) | Unloading method in liquid cargo ship | |
JPS5747283A (en) | Fishing boat for laver | |
JPS5639983A (en) | Submerged ship | |
JPS56131481A (en) | Configuration of small vessel |