JPS5650112A - Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays - Google Patents

Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays

Info

Publication number
JPS5650112A
JPS5650112A JP12400579A JP12400579A JPS5650112A JP S5650112 A JPS5650112 A JP S5650112A JP 12400579 A JP12400579 A JP 12400579A JP 12400579 A JP12400579 A JP 12400579A JP S5650112 A JPS5650112 A JP S5650112A
Authority
JP
Japan
Prior art keywords
molar ratio
mullite
sodium silicate
starting material
clays
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP12400579A
Other languages
English (en)
Japanese (ja)
Other versions
JPS6247810B2 (cg-RX-API-DMAC7.html
Inventor
Takamura Suzuki
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP12400579A priority Critical patent/JPS5650112A/ja
Publication of JPS5650112A publication Critical patent/JPS5650112A/ja
Publication of JPS6247810B2 publication Critical patent/JPS6247810B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Silicates, Zeolites, And Molecular Sieves (AREA)
JP12400579A 1979-09-28 1979-09-28 Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays Granted JPS5650112A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP12400579A JPS5650112A (en) 1979-09-28 1979-09-28 Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP12400579A JPS5650112A (en) 1979-09-28 1979-09-28 Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays

Publications (2)

Publication Number Publication Date
JPS5650112A true JPS5650112A (en) 1981-05-07
JPS6247810B2 JPS6247810B2 (cg-RX-API-DMAC7.html) 1987-10-09

Family

ID=14874668

Family Applications (1)

Application Number Title Priority Date Filing Date
JP12400579A Granted JPS5650112A (en) 1979-09-28 1979-09-28 Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays

Country Status (1)

Country Link
JP (1) JPS5650112A (cg-RX-API-DMAC7.html)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5939253U (ja) * 1982-09-07 1984-03-13 本田技研工業株式会社 新車に対する燃料油供給装置
CN110342555A (zh) * 2019-08-22 2019-10-18 湖南绿脉环保科技有限公司 一种含高岭石的矿物生产氧化铝的方法

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4844161A (cg-RX-API-DMAC7.html) * 1971-10-11 1973-06-25

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4844161A (cg-RX-API-DMAC7.html) * 1971-10-11 1973-06-25

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5939253U (ja) * 1982-09-07 1984-03-13 本田技研工業株式会社 新車に対する燃料油供給装置
CN110342555A (zh) * 2019-08-22 2019-10-18 湖南绿脉环保科技有限公司 一种含高岭石的矿物生产氧化铝的方法

Also Published As

Publication number Publication date
JPS6247810B2 (cg-RX-API-DMAC7.html) 1987-10-09

Similar Documents

Publication Publication Date Title
AU572467B2 (en) Process for manufacturing crystalline alumina
KR890003623A (ko) 미세결정질 베마이트 및 요업체류의 제조
GB1416730A (en) Method of cementing a ceramic liner in a metal tube
KR860000218A (ko) 다결정 알파 알루미나체(體)의 제조방법
DE3781409D1 (de) Verfahren zur spritzverarbeitung von feuerfesten stoffen.
KR890014160A (ko) 촉진된 실리카 촉매의 제조방법
KR840007860A (ko) 내알루미늄 내화조성물
GB1446103A (en) Hydraulically setting refractory compositions
JPS5650112A (en) Obtaining method for high molar ratio sodium silicate together with mullite or higher alumina material from clay or high alumina starting material containing clays
US4575439A (en) Method of producing a refractory brick
GB964978A (en) Alumina preparation and product
GB1199013A (en) Refractory Ramming Mix Composition and process of Forming Refractory Surface
GB1360183A (en) Method for manufacturing refractory products
FR2059789A5 (en) Binder for refractory concrete
DE59900972D1 (de) Grossformatiger Schamottestein, insbesondere Zinnbadbodenstein, und Verfahren zu seiner Herstellung
GB1254097A (en) Porcelain
ATE49585T1 (de) Feuerfeste thixotrope vibrations-masse zur vibrationszustellung von metallurgischen gefaessen.
GB1449484A (en) Refractory compositions
JPS5777023A (en) Manufacture of crystalline aluminosilicate
JPS56149319A (en) Manufacture of low-soda alumina
SU1724643A1 (ru) Масса дл изготовлени огнеприпаса
Lombardo The effect of ball clays on tile body formulations
GB1356247A (en) Silica-gels
GB1503454A (en) Method of in situ fabrication of a refractory monolith
GB1314619A (en) Concretes and reinforced concretes with a low expansion coefficient