JPS56131083A - Welded joint method for stainless steel tube - Google Patents
Welded joint method for stainless steel tubeInfo
- Publication number
- JPS56131083A JPS56131083A JP15866780A JP15866780A JPS56131083A JP S56131083 A JPS56131083 A JP S56131083A JP 15866780 A JP15866780 A JP 15866780A JP 15866780 A JP15866780 A JP 15866780A JP S56131083 A JPS56131083 A JP S56131083A
- Authority
- JP
- Japan
- Prior art keywords
- tube
- stainless steel
- build
- welding
- steel tube
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To manufacture a stainless steel tube joint which can prevent a stress corrosion cracking without requiring a post treatment, by previously performing build-up welding with a anticorrosion metal on the internal circumferential surface of the edge of the coupling part of a stainless steel tube, and then by performing butt welding at the tube end. CONSTITUTION:Over the entire internal circumferential surface of stainless steel tube 1 extending from the tube end by length (l), built-up part 2 made of anticorrosion metal of thickness (q) is provided by welding. After the build-up welding, shot peening or roll work is carried out at build-up part 2 and its circumference. As a result, layer 3 given the residual stress of compression is formed on the surface. The edges of this tube 1 and tube 1A of the same structure are formed and butted for coupling at weld zone 4 of low-carbon stainless steel, thereby obtaining a tube joint. Of this tube joint, the metallurgically sensitized part generated in the formation of weld zone 4 is covered with build-up parts 2 and 2A, so that stress corrosion cracking is prevented.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15866780A JPS56131083A (en) | 1980-11-10 | 1980-11-10 | Welded joint method for stainless steel tube |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15866780A JPS56131083A (en) | 1980-11-10 | 1980-11-10 | Welded joint method for stainless steel tube |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8341675A Division JPS527344A (en) | 1975-07-09 | 1975-07-09 | Method of weld jointing stainless steel pipe |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS56131083A true JPS56131083A (en) | 1981-10-14 |
Family
ID=15676714
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15866780A Pending JPS56131083A (en) | 1980-11-10 | 1980-11-10 | Welded joint method for stainless steel tube |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56131083A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58218391A (en) * | 1982-06-15 | 1983-12-19 | Kawasaki Steel Corp | Circumferential welding method of joint of steel pipes |
EP2422919A1 (en) * | 2008-12-18 | 2012-02-29 | Kobelco Research Institute, Inc. | Austenite-based weld material, and preventive maintenance method for stress corrosion cracking and preventive maintenance method for grain boundary corrosion using same |
EP2868882A4 (en) * | 2012-05-31 | 2016-05-18 | Ud Trucks Corp | Method for improving durability of exhaust-gas pipe, and exhaust-gas purification device |
CN111069703A (en) * | 2019-12-10 | 2020-04-28 | 中国科学院金属研究所 | Method for prolonging fatigue life of welded joint |
-
1980
- 1980-11-10 JP JP15866780A patent/JPS56131083A/en active Pending
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58218391A (en) * | 1982-06-15 | 1983-12-19 | Kawasaki Steel Corp | Circumferential welding method of joint of steel pipes |
JPH0256990B2 (en) * | 1982-06-15 | 1990-12-03 | Kawasaki Steel Co | |
EP2422919A1 (en) * | 2008-12-18 | 2012-02-29 | Kobelco Research Institute, Inc. | Austenite-based weld material, and preventive maintenance method for stress corrosion cracking and preventive maintenance method for grain boundary corrosion using same |
EP2422919A4 (en) * | 2008-12-18 | 2013-06-19 | Kobelco Res Inst Inc | Austenite-based weld material, and preventive maintenance method for stress corrosion cracking and preventive maintenance method for grain boundary corrosion using same |
EP2868882A4 (en) * | 2012-05-31 | 2016-05-18 | Ud Trucks Corp | Method for improving durability of exhaust-gas pipe, and exhaust-gas purification device |
US9657362B2 (en) | 2012-05-31 | 2017-05-23 | Ud Trucks Corporation | Method for improving durability of exhaust pipe |
CN111069703A (en) * | 2019-12-10 | 2020-04-28 | 中国科学院金属研究所 | Method for prolonging fatigue life of welded joint |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5499747A (en) | Reinforcing method for welded joint or stainless steel pipe and construction of welded join of stainless steel pipe | |
JPS56131083A (en) | Welded joint method for stainless steel tube | |
JPS53141140A (en) | Process for forming weld joint of pipeline or vessel | |
GB1393736A (en) | Joining tubes to plates involving friction welding | |
JPS57160582A (en) | Welding method by energy beam | |
JPS5573477A (en) | Tig or mig automatic welding method of stainless steel pipe | |
JPS5758982A (en) | Narrow groove submerged arc welding method | |
JPS56111588A (en) | Rust preventing method for laminated boundary face near pipe end of laminated autofrettage double pipes | |
JPS564392A (en) | Connecting method of piping | |
JPS5758984A (en) | Welding method | |
JPS551981A (en) | Weld joint method of stainless steel pipes | |
SU1464617A2 (en) | Method of applying coating onto pipe inner surface | |
JPS56163092A (en) | Welding method for stainless clad steel plate | |
JPS53140245A (en) | Improving method for fatiuge strength of fillet welded joint | |
ATE30073T1 (en) | COPPER-ALUMINUM PIPE CONNECTIONS. | |
SU1000196A1 (en) | Method of resistance flash butt welding | |
RU1830123C (en) | Method of manufacture of metal pipe line with protective enamel coating | |
JPS574395A (en) | Welding method | |
JPS569092A (en) | Welded joint | |
JPS57168798A (en) | Pipe welding method | |
JPS53116264A (en) | Tack welding method for seam of steel pipe | |
JPS54152639A (en) | Repair welding method for steel pipe | |
JPS5447839A (en) | Prepartion of welded joint | |
JPS5650797A (en) | Increasing method for weld-part fatigue strength of high-tension steel | |
JPS5469539A (en) | Joining method for tube and tube plate in heat exchanger or the like |