SU1464617A2 - Method of applying coating onto pipe inner surface - Google Patents
Method of applying coating onto pipe inner surface Download PDFInfo
- Publication number
- SU1464617A2 SU1464617A2 SU864119712A SU4119712A SU1464617A2 SU 1464617 A2 SU1464617 A2 SU 1464617A2 SU 864119712 A SU864119712 A SU 864119712A SU 4119712 A SU4119712 A SU 4119712A SU 1464617 A2 SU1464617 A2 SU 1464617A2
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- coating
- pipe inner
- coating onto
- applying coating
- onto pipe
- Prior art date
Abstract
Изобретение относитс к защите труб от коррозии. Цель изобретени - повышение качества покрыти за счет улучшени защитных свойств концевых участков свариваем.1х труб. После, очистки, нагрева и нанесени ме.тал- локерамического самофпюсующегос ма- |териала провод т его оплавление, Раз- ;м гченньш сплав уплотн ют обкаткой . на длину термического воздействи сварки.This invention relates to the protection of pipes against corrosion. The purpose of the invention is to improve the quality of the coating due to the improvement of the protective properties of the end sections of welded 1x pipes. After cleaning, heating and applying a me- tallocaric self-fabricating material, it is reflowed, expanded, and the soft alloy is compacted by running. on the length of the thermal effects of welding.
Description
1one
Изобретение касаетс запиты трув от коррозии и вл етс усовершенствованием способа нанесени покрыти на внутреннюю поверхность трубы, описанного в авт.. св. № 1239445,The invention relates to corrosion-resistant pipes and is an improvement of the method of coating the inner surface of a pipe described in the author. No. 1239445,
Цель дополнительного изобретени - i повышение качества покрыти за счет улучшени защитных свойств концевых участков cвapивae G,Ix труб.The purpose of the additional invention is to improve the quality of the coating by improving the protective properties of the end sections of the C, G, Ix tubes.
Внутреннюю поверхность трубы очищают одним из известных способов. После предварительного нагрева на внутреннюю и торцовую поверхности конца трубы нанос т металлокерами- ческий самофлюсующийс матери-ал, например сплав dr- CP, на длину, превышающую зону термического воздействи сварки. Затем провод т термообработку покрыти. оплавлением с последую- The inner surface of the pipe is cleaned with one of the known methods. After preheating, the metal-ceramic self-fluxing material, such as dr-CP alloy, is applied to the inner and end surfaces of the pipe end for a length exceeding the heat-affected zone of welding. Then the coating is heat treated. reflow with subsequent
щим уплотнением разм гченного сплава обкаткой на длину термического воздействи сварки. Под готов ениьте таким образом трубы покрывают затем облицовочным материалом.The secondary seal of the softened alloy runs on the length of the thermal effect of welding. Prepare the pipes in this way and then cover them with facing material.
Claims (1)