JPS5576570A - Manufacturing method for alkali battery plate - Google Patents

Manufacturing method for alkali battery plate

Info

Publication number
JPS5576570A
JPS5576570A JP15063978A JP15063978A JPS5576570A JP S5576570 A JPS5576570 A JP S5576570A JP 15063978 A JP15063978 A JP 15063978A JP 15063978 A JP15063978 A JP 15063978A JP S5576570 A JPS5576570 A JP S5576570A
Authority
JP
Japan
Prior art keywords
plates
washed
plate
water
subjected
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP15063978A
Other languages
Japanese (ja)
Inventor
Kiyoshi Fujita
Yoshiyuki Shioi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Furukawa Battery Co Ltd
Original Assignee
Furukawa Battery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Furukawa Battery Co Ltd filed Critical Furukawa Battery Co Ltd
Priority to JP15063978A priority Critical patent/JPS5576570A/en
Publication of JPS5576570A publication Critical patent/JPS5576570A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To raise workability and productivity as well as save the consumption of water by the procedure in which plate is subjected to a forming treatment, neutralized, washed with water, and then dried.
CONSTITUTION: Plate groups, formed by filling a fixed amount of an electrode active substance in porous base plates of sintered Ni plate, etc., are subjected to a forming treatment, then taken out of an alkali aqueous solution while being washed with running water, and then dipped in a 5∼10% boric acid aqueous solution tank to neutralize alkali adhered to the plates with the boric acid. Then, the plates are washed with running water to remove borate formed, and lastly dried to obtain complete plates.
COPYRIGHT: (C)1980,JPO&Japio
JP15063978A 1978-12-06 1978-12-06 Manufacturing method for alkali battery plate Pending JPS5576570A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP15063978A JPS5576570A (en) 1978-12-06 1978-12-06 Manufacturing method for alkali battery plate

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP15063978A JPS5576570A (en) 1978-12-06 1978-12-06 Manufacturing method for alkali battery plate

Publications (1)

Publication Number Publication Date
JPS5576570A true JPS5576570A (en) 1980-06-09

Family

ID=15501237

Family Applications (1)

Application Number Title Priority Date Filing Date
JP15063978A Pending JPS5576570A (en) 1978-12-06 1978-12-06 Manufacturing method for alkali battery plate

Country Status (1)

Country Link
JP (1) JPS5576570A (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5998459A (en) * 1982-11-29 1984-06-06 Shin Kobe Electric Mach Co Ltd Manufacture of sintered nickel electrode
EP0160845A2 (en) * 1984-05-07 1985-11-13 VARTA Batterie Aktiengesellschaft Process for manufacturing a gas-tight accumulator
EP0160846A2 (en) * 1984-05-07 1985-11-13 VARTA Batterie Aktiengesellschaft Process for manufacturing a precharged and dry-storable nickel-cadmium accumulator in a non-sealed construction
EP0203294A2 (en) * 1985-05-28 1986-12-03 VARTA Batterie Aktiengesellschaft Process for manufacturing negative cadmium electrodes for gas-tight alkaline accumulator cells

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5998459A (en) * 1982-11-29 1984-06-06 Shin Kobe Electric Mach Co Ltd Manufacture of sintered nickel electrode
EP0160845A2 (en) * 1984-05-07 1985-11-13 VARTA Batterie Aktiengesellschaft Process for manufacturing a gas-tight accumulator
EP0160846A2 (en) * 1984-05-07 1985-11-13 VARTA Batterie Aktiengesellschaft Process for manufacturing a precharged and dry-storable nickel-cadmium accumulator in a non-sealed construction
EP0203294A2 (en) * 1985-05-28 1986-12-03 VARTA Batterie Aktiengesellschaft Process for manufacturing negative cadmium electrodes for gas-tight alkaline accumulator cells

Similar Documents

Publication Publication Date Title
ATE3653T1 (en) ELECTROLYSIS PROCESS FOR THE PRODUCTION OF HYDROGEN IN AN ALKALINE MEDIUM.
JPS5576570A (en) Manufacturing method for alkali battery plate
JPS55105966A (en) Manufacturing method of diaphragm for cell having high dimensional stability
GB864592A (en) Process for the treatment of formed negative electrodes of lead accumulators
IT7925016A0 (en) PROCEDURE FOR PRODUCING HYDROGEN AND SULFURIC ACID BY ELECTROCHEMICAL DECOMPOSITION OF AN ELECTROLYTE, AS WELL AS AN ELECTRODE TO IMPLEMENT THE ELECTROCHEMICAL DECOMPOSITION.
JPS5244285A (en) Method of treating microbial cells containing glucose isomerase
SE7609309L (en) PROCEDURE FOR THE PRODUCTION OF PLANT PRESSURE PLATBERS OF ALUMINUM BY ELECTROCHEMICAL RECOVERY OF THE SURFACE
JPS55152191A (en) Formed cation exchange membrane
JPS5512672A (en) Button type air cell
JPS5727929A (en) Manufacture of electrolytic manganese dioxide
JPS5535420A (en) Manufacturing method of cell
JPS55113263A (en) Manufacturing method of alkali cell
JPS5521859A (en) Preparation of electrode
JPS5581466A (en) Positive electrode plate for alkaline storage battery
JPS5545802A (en) Fibers comprising immobilized enzymes and their preparation
JPS5219725A (en) Process for preparing an azo dye containing sulfonic acid group
JPS56136460A (en) Production of lead storage battery plate
JPS5629684A (en) Production of hydrogen
JPS5569962A (en) Manufacturing method for plate cell
ES449814A1 (en) Method for the production of lead storage battery electrodes
JPS56167269A (en) Formation of lead acid battery
JPS5553874A (en) Method of manufacturing cadmium negative electrode for alkaline battery
JPS5217889A (en) Enzyme electrode
JPS54162682A (en) Duel electrode for anode process in single cell
JPS56126260A (en) Formation of positive nickel plate